# US 8,277,633 B2 · Process for producing scorodite and recycling the post-scorodite-synthesis solution

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,633 B2
- Document ID: US8277633B2
- Status: Granted
- Kind: B2
- Application number: 12/155,469
- Filed: 2008-06-04
- Published: 2009-03-26
- Granted: 2012-10-02
- Earliest claimed: 2007-09-25
- Assignees: JX Nippon Mining & Metals Corporation
- Inventors: Yukio Kimura; Shigeo Katsura
- Web page: https://patentgrep.com/patent/US8277633B2

## CPC

- C01G 49/00: Compounds of iron
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)

## Abstract

The present invention is to provide a process for producing a scorodite that can shorten the time required for synthesizing the scorodite, and further can improve the yield of arsenic and iron into the scorodite. Accordingly, a process for producing a crystalline scorodite from an acidic aqueous solution containing pentavalent As and trivalent Fe, wherein the synthesis of the crystalline scorodite is performed after the molar ratio of trivalent Fe to pentavalent As contained in the acidic aqueous solution is adjusted to be equal to or more than 0.9 and equal to or less than 1.1 is provided.

## Claims

### Claim 1

A process for recycling a post-scorodite-synthesis solution, comprising the steps of:
(1) conducting a sulfuric acid leaching by feeding an oxygen-containing gas into an electrolytically precipitated copper in an acidic aqueous solution of sulfuric acid, while stirring the solution at a temperature and for a time sufficient for oxidizing As component contained in the electrolytically precipitated copper to pentavalent, followed by solid-liquid-separation of the solution into a post-leaching residue and a sulfuric acid-leached solution containing the pentavalent As component,
(2) adding ferric sulfate into said sulfuric acid-leached solution so that the molar ratio of trivalent Fe to pentavalent As may be equal to or more than 0.9 and equal to or less than 1.1 to prepare a reaction solution, followed by synthesis of a crystalline scorodite,
(3) after the synthesis of the scorodite, conducting solid-liquid-separation of the reaction solution into a post-scorodite-synthesis solution and a scorodite crystal, and
(4) using the post-scorodite-synthesis solution directly as an electrolyte solution used in electrolytic refining of copper.

### Claim 2 (depends on 1)

The process according to claim 1, further comprising the steps of:
(1)′ adding water to the post-leaching residue in step (1) for dissolving copper sulfate, followed by solid-liquid separation of a copper sulfate solution from the post-leaching residue, and
(3) adding said copper sulfate solution to the post-scorodite-synthesis solution obtained in Step (3) between Step (3) and Step (4).