# US 8,277,606 B2 · Method of providing paper-making fibers with durable curl and absorbent products incorporating same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,606 B2
- Document ID: US8277606B2
- Status: Granted
- Kind: B2
- Application number: 11/052,419
- Filed: 2005-02-07
- Published: 2005-07-07
- Granted: 2012-10-02
- Earliest claimed: 2000-03-06
- Assignees: Georgia-Pacific Consumer Products LP
- Inventors: Jeffrey A. Lee
- Web page: https://patentgrep.com/patent/US8277606B2

## CPC

- D21C 9/007: {by mechanical or physical means}
- D21H 11/16: modified by a particular after-treatment
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

A process for producing high bulk cellulosic fiber exhibiting a durable elevated curl index includes: (a) concurrently heat treating and convolving cellulosic fiber pulp at elevated temperature and pressure at high consistency under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development; and (b) recovering the pulp wherein the length weighted curl index of the treated fiber is at least about 20% higher than the length weighted curl index of the fiber prior to the heat treatment and convolving thereof. The curl imparted to the fiber persists upon treatment for 30 minutes in a laboratory disintegrator at 3000 rpm at 1% consistency at a temperature of 125° F. Moreover, the curl may be imparted to the fiber in a disk refiner at very short residence times, on the order of several seconds or less. In general, the process is carried out in the presence of saturated steam at a pressure of from about 5 to about 150 psig.

## Claims

### Claim 1

An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by way of:
(a) preparing a high bulk cellulosic pulp exhibiting a durable elevated curl index through the steps of (i) feeding a cellulosic pulp including Kraft fiber to a refining gap defined between opposed surfaces, at least one of the surfaces being rotatable with respect to its opposed surface; (ii) concurrently heat-treating and convolving the cellulosic pulp including Kraft fiber in the refining gap at elevated temperature and pressure under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development to form the heat-treated and convolved fiber; and
(b) incorporating the fiber so prepared into the absorbent sheet.

### Claim 2

An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber nor to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by a process comprising:
(a) thickening pulp process stream including Kraft fiber to a consistency of from about 20% to about 60%;
(b) concurrently heat-treating and convolving the fiber of said thickened pulp process stream including Kraft fiber under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development to form the treated fiber;
(c) combining the treated pulp process stream with a second pulp process stream to provide a papermaking furnish;
(d) depositing the papermaking furnish on a foraminous support to form a web; and
(e) drying the web to make absorbent sheet.

### Claim 3

An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by a process comprising:
(a) preparing a first cellulosic pulp component of including Kraft fiber exhibiting an elevated durable curl index by way of concurrently heat-treating and convolving cellulosic fiber at elevated temperature and pressure under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development to form the treated fiber;
(b) combining in admixture said first cellulosic pulp component with a second cellulosic pulp component to make a papermaking furnish, the second cellulosic pulp component having a length weighted curl index lower than the length weighted curl index of the first pulp component;
(c) depositing the papermaking furnish on a foraminous support to form a web; and
(d) drying the web to make absorbent sheet.

### Claim 4 (depends on 1)

The absorbent sheet according to claim 1, wherein the length weighted curl index of the treated fiber is at least 50% higher than the length weighted curl index of the fiber prior to treatment and wherein the 50% elevation of the length weighted curl index of the treated fiber is capable of persisting for 30 minutes in a disintegrator at 1% consistency of 125° F.

### Claim 5 (depends on 1)

The absorbent sheet according to claim 1, wherein the sheet incorporates secondary fiber which has been heat-treated and convolved.

### Claim 6 (depends on 5)

The absorbent sheet according to claim 5, wherein the sheet exhibits a through-air flow at 20″ water pressure drop of at least about 50% higher than a like sheet made with like fiber which has not been heat-treated and convolved.

### Claim 7 (depends on 5)

The absorbent sheet according to claim 5, wherein the sheet exhibits a through-air flow at 20″ water pressure drop of at least about 100% higher than a like sheet made with like fiber which has not been heat-treated and convolved.

### Claim 8

An absorbent sheet comprising a heat treated mechanically curled fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F. and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, wherein the fiber is made by a process comprising:
(a) preparing a high bulk cellulosic pulp exhibiting a durable elevated curl index through the steps of (i) feeding a cellulosic pulp including Kraft fiber to a refining gap defined between opposed surfaces, at least one of the surfaces being rotatable with respect to its opposed surface; (ii) concurrently heat-treating and convolving the cellulosic pulp including Kraft fiber in the refining gap at elevated temperature and pressure for about 0.1 seconds up to about 20 seconds under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development to form the fiber; and
(b) incorporating the fiber so prepared into the absorbent sheet.

### Claim 9 (depends on 8)

The absorbent sheet according to claim 8, wherein the cellulosic pulp is concurrently heat treated and convolved for less than 10 seconds.

### Claim 10 (depends on 8)

The absorbent sheet according to claim 8, wherein the cellulosic pulp is concurrently heat treated and convolved for less than 5 seconds.

### Claim 11

An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 0.4% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by way of:
(a) preparing a high bulk cellulosic pulp exhibiting a durable elevated curl index through the steps of (i) feeding a cellulosic pulp including Kraft fiber to a refining gap defined between opposed surfaces, at least one of the surfaces being rotatable with respect to its opposed surface; (ii) concurrently heat-treating and convolving the cellulosic pulp including Kraft fiber in the refining gap at elevated temperature and pressure under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development to form the treated fiber; and
(b) incorporating the fiber so prepared into the absorbent sheet.

### Claim 12

An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by way of:
(a) preparing a high bulk cellulosic pulp exhibiting a durable elevated curl index through the steps of (i) feeding a cellulosic pulp including Kraft fiber to a refining gap defined between opposed surfaces, at least one of the surfaces being rotatable with respect to its opposed surface; (ii) concurrently heat-treating and convolving the cellulosic pulp including Kraft fiber in the refining gap at elevated temperature and pressure to form the treated fiber; and
(b) incorporating the fiber so prepared into the absorbent sheet.

### Claim 13 (depends on 12)

The absorbent sheet according to claim 12, wherein the cellulosic pulp is concurrently heat treated and convolved at a temperature of from about 230° F. to about 370° F. and a pressure of from about 5 psig to about 150 psig.

### Claim 14 (depends on 13)

The absorbent sheet according to claim 13, wherein the cellulosic pulp is concurrently heat treated and convolved at a pressure of from about 10 psig to about 90 psig.

### Claim 15 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp is carried out at a consistency of from about 20% to about 60%.

### Claim 16 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp is carried out at a consistency of from about 20% to about 50%.

### Claim 17 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp is carried out at a consistency of from about 30% to about 40%.

### Claim 18 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp has a duration of from about 0.01 to about 20 seconds.

### Claim 19 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp has a duration of less than about 10 seconds.

### Claim 20 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp has a duration of less than about 5 seconds.

### Claim 21 (depends on 13)

The absorbent sheet according to claim 13, wherein heat-treating and convolving the cellulosic pulp has a duration of less than about 2 seconds.

### Claim 22 (depends on 13)

The absorbent sheet according to claim 13, wherein mechanical energy input to the cellulosic pulp during heat-treating and convolving is less than about 2 HP day/ton.

### Claim 23 (depends on 13)

The absorbent sheet according to claim 13, wherein mechanical energy input to the cellulosic pulp during heat-treating and convolving is less than about 1 HP day/ton.

### Claim 24 (depends on 13)

The absorbent sheet according to claim 13, wherein mechanical energy input to the cellulosic pulp during heat-treating and convolving is less than about 0.5 HP day/ton.

### Claim 25

An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, said at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and said treated fiber having substantially the same fibrillation and attendant strength as the fiber prior to said treatment, the absorbent sheet made by way of:
(a) preparing a high bulk cellulosic pulp of exhibiting a durable elevated curl index through the steps of (i) feeding a cellulosic pulp including Kraft fiber to a refining gap defined between opposed surfaces, at least one of the surfaces being rotatable with respect to its opposed surface; (ii) concurrently heat-treating and convolving the cellulosic pulp including Kraft fiber in the refining gap at elevated temperature and pressure to form the treated fiber; and
(b) incorporating the treated fiber so prepared into the absorbent sheet.

### Claim 26 (depends on 25)

The absorbent sheet according to claim 25, wherein the cellulosic pulp is concurrently heat treated and convolved at a temperature of from about 230° F. to about 370° F. and a pressure of from about 5 psig to about 150 psig.

### Claim 27 (depends on 25)

The absorbent sheet according to claim 25, wherein the cellulosic pulp is concurrently heat treated and convolved at a pressure of from about 10 psig to about 90 psig.

### Claim 28 (depends on 25)

The absorbent sheet according to claim 25, wherein the cellulosic pulp includes Kraft softwood fiber.

### Claim 29 (depends on 25)

The absorbent sheet according to claim 25, wherein the cellulosic pulp includes secondary fiber.