# US 8,277,585 B1 · Electric primer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,585 B1
- Document ID: US8277585B1
- Status: Granted
- Kind: B1
- Application number: 12/983,970
- Filed: 2011-01-04
- Granted: 2012-10-02
- Earliest claimed: 2011-01-04
- Assignees: The United States of America as represented by the Secretary of the Army
- Inventors: Rao Yalamanchili; John Hirlinger; Christopher Csernica
- Web page: https://patentgrep.com/patent/US8277585B1

## CPC

- C06B 23/001: {Fillers, gelling and thickening agents (e.g. fibres) , absorbents for nitroglycerine (binders, plasticisers for propellants C06B45/10; crosslinking or curing agents C06B45/10)}
- C06C 7/00: Non-electric detonators; Blasting caps; Primers
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})
- C06C: DETONATING OR PRIMING DEVICES; FUSES (ammunition fuzes F42C); CHEMICAL LIGHTERS; PYROPHORIC COMPOSITIONS

## Abstract

Improved electric primer compositions, structures, and methods that are compatible with existing munitions and in particular an exemplary electric primer composition including carbon nanotubes along with energetic primer mixture(s) and an exemplary primer structure including layers of energetic materials wherein a layer exhibiting the most energetic character is positioned proximate to a primer button. Alternative embodiments include both conductive and non-conductive layers.

## Claims

### Claim 1

A method of preparing an energetic mix for use in a primer comprising the steps of:
Preparing a solution of Gum Arabic;
Preparing a solution of Ammonium Dihydrogen Phosphide (ADP);
Adding a quantity of the Gum Arabic solution and a quantity of the ADP solution to a quantity of Bismuth Trioxide (Bi2O3) such that it is sufficiently wet;
Adding a quantity of nano-aluminum and an additional quantity of Gum Arabic solution to the wet Bi2O3 and mixing sufficiently to produce the energetic mix;
Adding a quantity of carbon nanotubes to the energetic mix and further mixing such that the energetic mix is electrically conductive.

### Claim 2 (depends on 1)

The method of claim 1 wherein the quantity of carbon nanotubes is substantially 2.5% by weight.

### Claim 3 (depends on 1)

The method of claim 1 further comprising the step of:
Adding to the electrically conductive energetic mix a quantity of a booster comprising a secondary explosive material.

### Claim 4 (depends on 3)

The method of claim 3 wherein said secondary explosive material is PETN and is added in a quantity of substantially 5% by weight.