# US 8,277,582 B2 · Hydrogen absorbing alloy, hydrogen absorbing alloy electrode, secondary battery, and production method of hydrogen absorbing alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,582 B2
- Document ID: US8277582B2
- Status: Granted
- Kind: B2
- Application number: 13/090,184
- Filed: 2011-04-19
- Published: 2011-08-11
- Granted: 2012-10-02
- Earliest claimed: 2005-08-11
- Assignees: GS Yuasa International Ltd.; National Institute of Advanced Industrial Science and Technology
- Inventors: Manabu Kanemoto; Tadashi Kakeya; Minoru Kuzuhara; Masaharu Watada; Tetsuo Sakai; Tetsuya Ozaki
- Web page: https://patentgrep.com/patent/US8277582B2

## CPC

- H01M 4/383: {Hydrogen absorbing alloys}
- H01M 8/04216: {characterised by the choice for a specific material, e.g. carbon, hydride, absorbent}
- H01M 8/065: by dissolution of metals or alloys; by dehydriding metallic substances
- H01M 10/345: {Gastight metal hydride accumulators}
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a hydrogen absorbing alloy containing a phase of a Pr5Co19 type crystal structure having a composition defined by a general formula A(4−w)B(1+w)C19 (A denotes one or more element(s) selected from rare earth elements including Y (yttrium); B denotes an Mg element; C denotes one or more element(s) selected from a group consisting of Ni, Co, Mn, and Al; and w denotes a numeral in a range from −0.1 to 0.8) and having a composition as a whole defined by a general formula R1xR2yR3z (15.8≦x≦17.8, 3.4≦y≦5.0, 78.8≦z≦79.6, and x+y+z=100; R1 denotes one or more element(s) selected from rare earth elements including Y (yttrium); R2 denotes an Mg element, R3 denotes one or more element(s) selected from a group consisting of Ni, Co, Mn, and Al; the numeral of Mn+Al in the z is 0.5 or higher; and the numeral of Al in the z is 4.1 or lower).

## Claims

### Claim 1

A hydrogen absorbing alloy containing 15 weight % or higher of a phase of a Pr5Co19 crystal structure, wherein the content of Cu is in a range of 1 to 8 mol %.

### Claim 2 (depends on 1)

A hydrogen absorbing alloy production method for producing the hydrogen absorbing alloy according to claim 1, wherein the method comprises steps of cooling a melted alloy at a cooling speed of 1000 K/second or more and further annealing the obtained alloy at a temperature in a range from 860 to 980° C. in an inert gas atmosphere under a pressurized state.

### Claim 3 (depends on 2)

The hydrogen absorbing alloy production method according to claim 2, wherein the temperature range of said annealing is in a range from 920 to 970° C.

### Claim 4 (depends on 1)

The hydrogen absorbing alloy according to claim 1, wherein the alloy as a whole has a composition defined by a general formula R1aR2bR3cCud; wherein R1 denotes one or more element(s) selected from rare earth elements including Y (yttrium); R2 denotes one or more element(s) selected from the group consisting of Mg, Ca, Sr, and Ba; R3 denotes one or more element(s) selected from the group consisting of Ni, Co, Mn, Al, Fe, Cr, Zn, Si, Sn, V, Nb, Ta, Ti, Zr, and Hf; and a, b, c, and d denote numerals satisfying 15≦a≦19, 2≦b≦7, 70≦c≦80, 1≦d≦7, and a+b+c+d=100, respectively.

### Claim 5 (depends on 4)

A hydrogen absorbing alloy production method for producing the hydrogen absorbing alloy according to claim 4, wherein the method comprises steps of cooling a melted alloy at a cooling speed of 1000 K/second or more and further annealing the obtained alloy at a temperature in a range from 860 to 980° C. in an inert gas atmosphere under a pressurized state.

### Claim 6 (depends on 4)

The hydrogen absorbing alloy according to claim 4, wherein said R2 is Mg and said R3 is one or more element(s) selected from the group consisting of Co, Mn, Al, and Ni.

### Claim 7 (depends on 6)

A hydrogen absorbing alloy production method for producing the hydrogen absorbing alloy according to claim 6, wherein the method comprises steps of cooling a melted alloy at a cooling speed of 1000 K/second or more and further annealing the obtained alloy at a temperature in a range from 860 to 980° C. in an inert gas atmosphere under a pressurized state.