# US 8,277,581 B2 · Nickel-iron-zinc alloy nanoparticles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,581 B2
- Document ID: US8277581B2
- Status: Granted
- Kind: B2
- Application number: 12/595,562
- Filed: 2008-04-10
- Published: 2011-07-07
- Granted: 2012-10-02
- Earliest claimed: 2008-04-10
- Assignees: Sumitomo Osaka Cement Co., Ltd.
- Inventors: Masayuki Ishizuka; Nobuhiro Hidaka
- Web page: https://patentgrep.com/patent/US8277581B2

## CPC

- C22C 19/03: based on nickel
- B22F 1/06: Metallic powder characterised by the shape of the particles (nanosized particles B22F1/054)
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 1/054: Nanosized particles
- B22F 2009/041: {by mechanical alloying, e.g. blending, milling}
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- H05K 1/0233: {Filters, inductors or a magnetic substance}
- H05K 1/097: {Inks comprising nanoparticles and specially adapted for being sintered at low temperature (H05K1/095 takes precedence)}
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Nickel-iron-zinc alloy nanoparticles of the present invention are in the form of tabular particles having a thickness of 1 μm or less and an aspect ratio of 2 or more, wherein the (220) plane which is the crystal plane of the face-centered cubic lattice is oriented on the tabular surface of the particles.

## Claims

### Claim 1

Nickel-iron-zinc alloy nanoparticles in the form of tabular particles having a thickness of 1 μm or less and an aspect ratio of 2 or more, wherein the (220) plane which is the crystal plane of the face-centered cubic lattice is oriented on the tabular surface of the particles.

### Claim 2 (depends on 1)

The nickel-iron-zinc alloy nanoparticles according to claim 1, wherein when the peak intensity of the (200) plane is defined as I(200) and the peak intensity of the (220) plane is defined as I(220) in an X-ray diffraction pattern measured on the tabular surface, the nickel-iron-zinc alloy nanoparticles satisfy the relation of I(220)/[I(220)+I(200)]>0.5.

### Claim 3 (depends on 1)

The nickel-iron-zinc alloy nanoparticles according to claim 1, wherein the thickness of the nickel-iron-zinc alloy nanoparticles is 0.5 μm or less.

### Claim 4 (depends on 1)

The nickel-iron-zinc alloy nanoparticles according to claim 1, wherein the thickness of the nickel-iron-zinc alloy nanoparticles is 0.2 μm or less.

### Claim 5 (depends on 1)

The nickel-iron-zinc alloy nanoparticles according to claim 1, wherein the aspect ratio of the particles is 5 or more.

### Claim 6 (depends on 1)

The nickel-iron-zinc alloy nanoparticles according to claim 1, wherein the aspect ratio of the particles is 10 or more.

### Claim 7 (depends on 1)

The nickel-iron-zinc alloy nanoparticles according to claim 1, further containing at least one metal selected from the group consisting of molybdenum, chromium, cobalt, manganese, vanadium, niobium and copper.

### Claim 8

A production method of nickel-iron-zinc alloy nanoparticles in the form of tabular plates having a thickness of 1 μm or less and an aspect ratio of 2 or more, with the (220) plane, which is the crystal plane of the face-centered cubic lattice and is oriented on the tabular surface of the particles, wherein the method is selected from the following (a), (b) and (c):
(a) a method comprising steps of; forming particles by adding a reducing agent to an aqueous solution containing a nickel salt, an iron salt and a zinc salt and simultaneously reducing nickel ions, iron ions and zinc ions contained in the aqueous solution; and forming nanoparticles by subjecting the formed particles to plastic deformation by applying mechanical stress;
(b) a method comprising steps of; forming particles by atomization; and forming nanoparticles by subjecting the formed particles to plastic deformation by applying mechanical stress; and,
(c) a method comprising steps of; forming particles by gas phase synthesis; and forming nanoparticles by subjecting the formed particles to plastic deformation by applying mechanical stress.

### Claim 9 (depends on 8)

The production method of nickel-iron-zinc alloy nanoparticles according to claim 8, wherein when the peak intensity of the (200) plane having a diffraction angle 2θ in the vicinity of 52° is defined as I(200), and the peak intensity of the (220) plane having a diffraction angle 2θ in the vicinity of 76° is defined as I(220) in an X-ray diffraction pattern measured on the tabular surface, the nickel-iron-zinc alloy nanoparticles satisfy the following relation I(220)/[I(220)+I(200)]>0.5.