# US 8,277,578 B2 · Rare earth permanent magnet and its preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,578 B2
- Document ID: US8277578B2
- Status: Granted
- Kind: B2
- Application number: 12/913,276
- Filed: 2010-10-27
- Published: 2011-02-17
- Granted: 2012-10-02
- Earliest claimed: 2007-03-16
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Inventors: Hiroaki Nagata; Tadao Nomura; Takehisa Minowa
- Web page: https://patentgrep.com/patent/US8277578B2

## CPC

- H01F 1/0577: {sintered}
- C22C 33/0278: {with at least one alloying element having a minimum content above 5%}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/10: containing cobalt
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A rare earth permanent magnet is prepared by disposing a powdered metal alloy containing at least 70 vol % of an intermetallic compound phase on a sintered body of R—Fe—B system, and heating the sintered body having the powder disposed on its surface below the sintering temperature of the sintered body in vacuum or in an inert gas for diffusion treatment. The advantages include efficient productivity, excellent magnetic performance, a minimal or zero amount of Tb or Dy used, an increased coercive force, and a minimized decline of remanence.

## Claims

### Claim 1

A rare earth permanent magnet, which is prepared by
disposing an alloy powder on a surface of an original sintered body of the composition Ra-T1b-Bcwherein R is at least one element selected from rare earth elements inclusive of Y and Sc, T1 is at least one element selected from Fe and Co, B is boron, “a,” “b” and “c” indicative of atomic percent are in the range: 12≦a≦20, 4.0≦c7.0, and the balance of b, said alloy powder having the composition M1d- M2ewherein each of M1 and M2is at least one element selected from the group consisting of Al, Si, C, P, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, Ge, Zr, Nb, Mo, Ag, In, Sn, Sb, Hf, Ta, W, Pb, and Bi, M1 is different from M2, “d” and “e” indicative of atomic percent are in the range: 0.1≦e≦99.9 and the balance of d, and containing at least 70% by volume of an intermetallic compound phase, and
heat treating the sintered body having the alloy powder disposed on its surface at a temperature equal to or below the sintering temperature of the original sintered body in vacuum or in an inert gas,
wherein at least one element of M1 and at least one element of M2 in the alloy powder is diffused to grain boundaries in the interior of the sintered body and/or near grain boundaries within sintered body primary phase grains, and not into the interior of primary phase grains, so that the coercive force of the magnet is increased over the magnet properties of the original sintered body.

### Claim 2 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein the at least one element of M1 and the at least one element of M2 in the alloy powder is diffused to grain boundaries in the interior of the sintered body and near grain boundaries within sintered body primary phase grains so that the coercive force of the magnet is increased over the magnet properties of the original sintered body.

### Claim 3 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein a majority of the element composition of the R is Nd and/or Pr.

### Claim 4 (depends on 1)

The rare earth permanent magnet according to claim 1, further comprising machining the original sintered body prior to the disposing step.

### Claim 5 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein the intermetallic compound phase is at least 90% by volume.

### Claim 6 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein the alloy powder has an average particle size of 1 μm to 500 μm.

### Claim 7 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein the alloy powder has an average particle size of 1 μm to 100 μm.

### Claim 8 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein the heat treatment is for 1 minute to 30 hours.

### Claim 9 (depends on 1)

The rare earth permanent magnet according to claim 1, wherein the heat treatment occurs at a temperature of at least 200° C.