# US 8,277,574 B2 · Method for manufacturing grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,574 B2
- Document ID: US8277574B2
- Status: Granted
- Kind: B2
- Application number: 12/744,583
- Filed: 2008-12-11
- Published: 2010-09-30
- Granted: 2012-10-02
- Earliest claimed: 2007-12-12
- Assignees: Nippon Steel Corporation
- Inventors: Tatsuhiko Sakai; Hideyuki Hamamura; Masao Yabumoto
- Web page: https://patentgrep.com/patent/US8277574B2

## CPC

- H01F 1/16: in the form of sheets (H01F1/147 takes precedence)
- C21D 8/1294: involving a localised treatment
- Y10T 428/1234: Honeycomb, or with grain orientation or elongated elements in defined angular relationship in respective components [e.g., parallel, inter- secting, etc.]
- Y10T 428/2457: Parallel ribs and/or grooves
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

There is provided a method for manufacturing a grain-oriented electromagnetic steel sheet whose iron losses are reduced by laser beam irradiation, capable of improving the iron losses in both the L-direction and the C-direction while easily ensuring high productivity. The method for manufacturing a grain-oriented electromagnetic steel sheet reduces iron losses by scanning and irradiating a grain-oriented electromagnetic steel sheet with a continuous-wave laser beam condensed into a circular or elliptical shape at constant intervals in a direction substantially perpendicular to a rolling direction of the grain-oriented electromagnetic steel sheet, wherein when an average irradiation energy density Ua is defined as Ua=P/(Vc×PL) (mJ/mm2), where P (W) is average power of the laser beam, Vc (m/s) is a beam scanning velocity, and PL (mm) is an irradiation interval in a rolling direction, PL and Ua are in the following ranges: 1.0 mm≦PL≦3.0 mm, 0.8 mJ/mm2≦Ua≦2.0 mJ/mm2.

## Claims

### Claim 1

A method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation, comprising the step of:
repeatedly irradiating a surface of a grain-oriented electromagnetic steel sheet with a condensed continuous-wave laser beam by scanning the grain-oriented electromagnetic steel sheet from a rolling direction toward an inclination direction thereof while scanning portions of the continuous-wave laser beam are being shifted at intervals, wherein
when an average irradiation energy density Ua is defined as Ua=P/Vc/PL (mJ/mm2),
where P (W) is average power of the continuous-wave laser beam,
Vc (mm/s) is a velocity of the scanning, and
PL (mm) is each of the intervals,
the following relationships are satisfied:
1.0 mm≦PL≦3.0 mm
0.8 mJ/mm2≦Ua≦2.0 mJ/mm2.

### Claim 2 (depends on 1)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 1, wherein
when an irradiation power density Ip of the continuous-wave laser beam is defined as Ip=(4/π)×P/(dL×dc) (kW/mm2),
where dc (mm) is a diameter of the continuous-wave laser beam in a direction of the scanning, and
dL (mm) is a diameter of the continuous-wave laser beam in a direction orthogonal to the direction of the scanning,
the following relationships are satisfied:
(88−15×PL) kW/mm2≧Ip≧(6.5−1.5×PL) kW/mm2
1.0 mm≦PL≦4.0 mm.

### Claim 3 (depends on 2)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 2, wherein a shape of the continuous-wave laser beam on a surface of the grain-oriented electromagnetic steel sheet is circular or elliptical.

### Claim 4 (depends on 3)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 3, wherein the direction of the scanning is substantially orthogonal to the rolling direction of the grain-oriented electromagnetic steel sheet.

### Claim 5 (depends on 2)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 2, wherein the direction of the scanning is substantially orthogonal to the rolling direction of the grain-oriented electromagnetic steel sheet.

### Claim 6 (depends on 1)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 1, wherein a shape of the continuous-wave laser beam on a surface of the grain-oriented electromagnetic steel sheet is circular or elliptical.

### Claim 7 (depends on 6)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 6, wherein the direction of the scanning is substantially orthogonal to the rolling direction of the grain-oriented electromagnetic steel sheet.

### Claim 8 (depends on 1)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 1, wherein the direction of the scanning is substantially orthogonal to the rolling direction of the grain-oriented electromagnetic steel sheet.

### Claim 9

A method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation, which reduces iron losses by scanning and irradiating a grain-oriented electromagnetic steel sheet with a continuous-wave laser beam condensed into a circular or elliptical shape at constant intervals in a direction substantially perpendicular to a rolling direction of the grain-oriented electromagnetic steel sheet, wherein
when an average irradiation energy density Ua is defined as Ua=P/Vc/PL (mJ/mm2),
where P (W) is average power of the laser beam,
Vc (mm/s) is a beam scanning velocity, and
PL (mm) is an irradiation interval in a rolling direction,
the following relationships are satisfied:
1.0 mm≦PL≦3.0 mm
0.8 mJ/mm2≦Ua≦2.0 mJ/mm2.

### Claim 10 (depends on 9)

The method for manufacturing a grain-oriented electromagnetic steel sheet whose magnetic domains are controlled by laser beam irradiation according to claim 9, wherein
when an irradiation power density Ip is defined as Ip=(4/π)×P/(dL×dc) (kW/mm2),
where dc (mm) is a light condensing diameter in a beam scanning direction, and
dL (mm) is a light condensing beam diameter in a direction orthogonal to the scanning direction,
the following relationships are satisfied:
(88−15×PL) kW/mm2≧Ip≧(6.5−1.5×PL) kW/mm2
1.0 mm≦PL≦4.0 mm.