# US 8,277,559 B2 · Quartz glass crucible for pulling up silicon single crystal and method for manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,559 B2
- Document ID: US8277559B2
- Status: Granted
- Kind: B2
- Application number: 10/555,853
- Filed: 2004-04-26
- Published: 2006-10-26
- Granted: 2012-10-02
- Earliest claimed: 2003-05-01
- Assignees: Heraeus Quarzglas GmbH & Co. KG; Shin-Estu Quartz Products Co., Ltd.
- Inventors: Yasuo Ohama
- Web page: https://patentgrep.com/patent/US8277559B2

## CPC

- C30B 29/06: Silicon
- C03B 19/095: {by centrifuging, e.g. arc discharge in rotating mould (crucibles for crystal pulling in general C30B15/10, C30B35/002)}
- C30B 15/10: Crucibles or containers for supporting the melt
- Y10T 117/10: Apparatus
- Y10T 117/1032: Seed pulling
- Y10T 117/1052: including a sectioned crucible [e.g., double crucible, baffle]
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A quartz glass crucible which has a non-transparent outer layer formed through melting a natural silica powder and a transparent layer formed in the inside of the outer layer, wherein the transparent layer comprises a natural quartz layer having a thickness of 0.4 to 5.0 mm transparent layer comprising a synthetic quarts glass is formed thereon in the inside of the crucible in the range of 0.15 to 0.55 L relative to L, which is the distance from the center of the bottom of the inner surface of the quartz glass crucible to the upper end thereof along the inner surface thereof. The quartz glass crucible can be suitably used for suppressing the occurrence of vibration and reducing the generation of roughened face in the surface of a crucible, and thus for pulling up a silicon single crystal with enhanced stability.

## Claims

### Claim 1

A quartz glass crucible for pulling up a silicon single crystal, comprising:
a quartz glass crucible body having a hollow cylindrical top portion forming an opening into the quartz glass crucible, a bottom portion forming a circular depression with a centrally-located bottom dead center point and a bent portion interconnecting the top portion and the bottom portion to form an inside surface of the quartz glass crucible body, the quartz glass crucible body having an opaque outer layer formed by melting natural silica powder and a transparent layer structure formed on the inside thereof, characterized in that the transparent layer structure includes a transparent layer made of natural quartz glass with a thickness of 0.4 to 5.0 mm covering the entirety of the inside of the opaque outer layer, and a transparent layer made of a synthetic quartz glass having a lower transparent layer portion and an upper transparent layer portion, the lower transparent layer portion formed on and covering a lower portion of the transparent layer made of the natural quartz glass of the inside of the crucible and having:
a thickness extending in a range from 0.15 to 0.55 L selected from a thickness range of 0.2 to 1.5 mm,
the upper transparent layer portion having a thickness of 0.1 mm or less and formed on and covering an upper portion of the transparent layer made of the natural quartz glass of the inside of the crucible in a range from 0.6 to 1.0 L,
wherein L is a distance extending along the inside surface of the quartz glass crucible body, as viewed in cross-section, from the bottom dead center point to the opening into the quartz glass crucible body and
wherein the range of 0.15 to 0.55 L is inclusive of the bottom portion and the bent portion and is exclusive of the top portion.

### Claim 2 (depends on 1)

The quartz glass crucible for pulling up a silicon single crystal according to claim 1, characterized in that an average OH group concentration CA in the transparent layer made of a synthetic quartz glass is from 100 to 300 ppm, an average OH group concentration CB in the transparent layer made of natural quartz glass is from 60 to 150 ppm, an average OH group concentration CC in the opaque outer layer made of natural quartz glass is from 20 to 60 ppm, and they satisfy the relation: CA>CB>CC.

### Claim 3 (depends on 1)

A method for producing a quartz glass crucible for pulling up a silicon single crystal according to claim 1, characterized by making an inner cavity of a quartz glass crucible base body mounted on a rotatable mold a high temperature atmosphere, feeding natural silica powder to the high temperature atmosphere in the inside of an opaque outer layer after or during the formation of the opaque outer layer by partially melting the inner cavity to form the transparent layer made of natural quartz glass on the entire inner surface of the opaque outer layer by melting and vitrifying the natural silica powder, and then feeding a synthetic silica powder and melting and vitrifying the synthetic silica powder to form the transparent layer made of a synthetic quartz glass on the inside of the crucible in the range from at least 0.15 to 0.55 L in terms of a distance L from the center of the bottom of the inner surface of the quartz glass crucible having the transparent layer made of natural quartz glass to the upper end face along the inner surface of the crucible.

### Claim 4

A quartz glass crucible for pulling up a silicon single crystal, said quartz glass crucible having an opaque outer layer made of natural quartz glass and a transparent layer formed on the inside thereof, characterized in that the number of brown rings per unit area (cm2) observed in the range from the initial surface level of a silicon melt to 0.3 M in terms of a length M from the initial surface level of the silicon melt to the surface level of the remaining melt after pulling up a single crystal measured along the inner surface of the quartz glass crucible is 1.8-fold or more greater than the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt.

### Claim 5 (depends on 4)

The quartz glass crucible for pulling up a silicon single crystal according to claim 4, characterized in that the number of brown rings per unit area (cm2) observed in the range from the initial surface level of a melt to 0.3 M is 2.5-fold or more greater than the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt.

### Claim 6 (depends on 4)

The quartz glass crucible for pulling up a silicon single crystal according to claim 4, said quartz glass crucible having an opaque outer layer made of natural quartz glass and a transparent layer formed on the inside thereof, characterized in that a transparent layer made of natural quartz glass or a mixture of natural and synthetic quartz glasses is formed on the inner surface of the crucible in the range from the initial surface level of a silicon melt to 0.3 M in terms of a length M from the initial surface level of the silicon melt to the surface level of the remaining melt after pulling up a single crystal measured along the inner surface of the quartz glass crucible, a transparent layer made of a synthetic quartz glass is formed on the inner surface of the crucible in the range up to 0.3 M above the surface level of the remaining melt, and the number of brown rings per unit area (cm2) observed in the range from the initial surface level of the melt to 0.3 M is 1.8-fold or more greater than the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt.

### Claim 7 (depends on 6)

The quartz glass crucible for pulling up a silicon single crystal according to claim 6, characterized in that the number of brown rings per unit area (cm2) observed in the range from the initial surface level of a melt to 0.3 M is 2.5-fold or more greater than the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt.

### Claim 8 (depends on 4)

The quartz glass crucible for pulling up a silicon single crystal according to claim 4, said quartz glass crucible having an opaque outer layer made of natural quartz glass and a transparent layer formed on the inside thereof, characterized in that the inner surface of the crucible in the range from the initial surface level of a melt to 0.3 M is subjected to an etching treatment or a sandblast process, and the number of brown rings per unit area (cm2) observed in the range after it is used for pulling up a silicon single crystal is 1.8-fold or more greater than the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt which is not subjected to the etching treatment or the sandblast process.

### Claim 9 (depends on 8)

The quartz glass crucible for pulling up a silicon single crystal according to claim 8, characterized in that the number of brown rings per unit area (cm2) observed in the range from the initial surface level of a melt to 0.3 M is 2.5-fold or more greater than the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt.

### Claim 10 (depends on 4)

The quartz glass crucible for pulling up a silicon single crystal according to claim 4, characterized in that the number of brown rings observed in the range up to 0.3 M above the surface level of the remaining melt is 0.02 to 0.9/cm2.

### Claim 11 (depends on 4)

The quartz glass crucible for pulling up a silicon single crystal according to claim 4, characterized in that the number of brown rings per unit area (cm2) observed in the range from the initial surface level of a melt to 0.3 M is 2.0 to 5.0/cm2.

### Claim 12 (depends on 4)

A method for producing a quartz glass crucible for pulling up a silicon single crystal according to claim 4, characterized by making an inner cavity of a quartz glass crucible base body mounted on a rotatable mold a high temperature atmosphere, feeding natural silica powder or a powder mixture of natural and synthetic silicas to the high temperature atmosphere in the inside of an opaque outer layer after or during the formation of the opaque outer layer by partially melting the inner cavity to form a transparent layer made of natural quartz glass or a mixture of natural and synthetic quartz glasses in the range from the initial surface level of a melt to 0.3 M by melting and vitrifying the natural silica powder or the powder mixture of natural and synthetic silicas, and then feeding a synthetic silica powder and melting and vitrifying the synthetic silica powder to form a transparent layer made of a synthetic quartz glass on the inner surface of the crucible in the range up to 0.3 M above the surface level of the remaining melt.