# US 8,277,539 B2 · Leaching process for copper concentrates containing arsenic and antimony compounds

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,539 B2
- Document ID: US8277539B2
- Status: Granted
- Kind: B2
- Application number: 12/991,304
- Filed: 2009-04-17
- Published: 2011-03-10
- Granted: 2012-10-02
- Earliest claimed: 2008-05-06
- Assignees: The University of British Columbia
- Inventors: David G. Dixon; Berny Rivera-Vasquez
- Web page: https://patentgrep.com/patent/US8277539B2

## CPC

- C25C 1/12: of copper
- C22B 3/26: by liquid-liquid extraction using organic compounds
- C22B 15/0063: {Hydrometallurgy}
- C22B 15/0071: {containing sulfur}
- C22B 15/0084: {Treating solutions (with organic compounds C22B3/20)}
- Y02P 10/20: Recycling
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of recovering copper from a copper sulfide concentrate comprising a copper arsenic sulfosalt or a copper antimony sulfosalt, using pyrite as a catalyst. The concentrate and pyrite are added to an acidic sulfate leach solution. The copper is leached from the concentrate, in the presence of an oxygen-containing gas, under conditions whereby the pyrite is substantially unoxidized. The pyrite:copper sulfide ratio of the pyrite being added to the copper sulfide present in the concentrate being added is at least 1:3. The pyrite may be maintained at a concentration in the leach solution of at least 9 grams per liter. The leached copper is recovered from the solution by conventional methods.

## Claims

### Claim 1

A method of recovering copper from a copper sulfide concentrate comprising a copper sulfide, wherein the copper sulfide includes one of a copper arsenic sulfosalt and a copper antimony sulfosalt, comprising the steps of:
(a) adding the concentrate and a pyrite to an acidic sulfate leach solution, the concentrate and the pyrite being in particulate form, wherein a pyrite:copper sulfide weight ratio of the pyrite and the copper sulfide added to the leach solution is at least 1:1;
(b) leaching the copper from the concentrate in the leach solution, in the presence of an oxygen-containing gas, under conditions whereby the pyrite is substantially unoxidized, to produce a solution containing copper ions; and
(c) recovering the leached copper from the solution.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the copper sulfide concentrate comprises a copper arsenic sulfosalt selected from one of a sulfarsenite and a sulfarsenate.

### Claim 3 (depends on 2)

A method according to claim 2, wherein the copper sulfide concentrate comprises enargite.

### Claim 4 (depends on 2)

A method according to claim 2, wherein the copper sulfide concentrate comprises tennantite.

### Claim 5 (depends on 2)

A method according to claim 2, wherein the pyrite is maintained at a concentration in the leach solution of at least 9 g/L.

### Claim 6 (depends on 2)

A method according to claim 2, wherein the pyrite is maintained at a concentration in the leach solution that is at least as high as one of 10, 16, 31, 40, 44, 47, 63 and 78 g/L.

### Claim 7 (depends on 2)

A method according to claim 2, wherein the pyrite:copper sulfide weight ratio is in the range of 1:1 to 20:1.

### Claim 8 (depends on 2)

A method according to claim 2, wherein the pyrite:copper sulfide weight ratio is in the range of 1:1 to 10:1.

### Claim 9 (depends on 2)

A method according to claim 2, wherein the pyrite:copper sulfide weight ratio is in the range of 3:1 to 5:1.

### Claim 10 (depends on 2)

A method according to claim 2, wherein the concentrate and the pyrite are added in the form of a mixture.

### Claim 11 (depends on 2)

A method according to claim 2, wherein at least some of the pyrite that is added is recycled pyrite obtained from the leach solution following a solid-liquid separation step.

### Claim 12 (depends on 2)

A method according to claim 2, wherein the conditions comprise maintaining an operating potential of the leach solution such that the pyrite is substantially unoxidized.

### Claim 13 (depends on 12)

A method according to claim 12, wherein the operating potential is 500 mV or less versus Ag/AgCl.

### Claim 14 (depends on 12)

A method according to claim 12, wherein the operating potential is between 400 and 550 mV versus Ag/AgCl.

### Claim 15 (depends on 12)

A method according to claim 12, wherein the operating potential is between 460 and 500 mV versus Ag/AgCl.

### Claim 16 (depends on 2)

A method according to claim 2, wherein the maintaining of the operating potential is carried out by means of selecting one or more of:
(i) the ratio of the concentrate to the pyrite;
(ii) the particle size of the concentrate and the pyrite;
(iii) an acid concentration of the leach solution; and
(iv) a temperature of the leach solution.

### Claim 17 (depends on 2)

A method according to claim 2, further comprising the step of selecting one or more of:
(i) pulp density level,
(ii) oxygen flow rate, and
(iii) intensity of agitation of the leach solution, to control the operating potential.

### Claim 18 (depends on 2)

A method according to claim 2, wherein step (b) is carried out at atmospheric pressure.

### Claim 19 (depends on 2)

A method according to claim 2, wherein step (b) is carried out above atmospheric pressure.

### Claim 20 (depends on 2)

A method according to claim 2, wherein step (b) is carried out at a pulp density of 9% solids or higher.

### Claim 21 (depends on 2)

A method according to claim 2, wherein step (c) comprises a solvent extraction step and electrowinning.

### Claim 22 (depends on 21)

A method according to claim 21, wherein ferrous ions in a raffinate stream from the solvent extraction step are oxidized to ferric ions by oxygen gas and precipitated as a stable ferric salt.

### Claim 23 (depends on 2)

A method according to claim 2, wherein the pyrite is present in an ore from which the concentrate is prepared.

### Claim 24 (depends on 1)

A method according to claim 1, wherein the copper sulfide concentrate comprises a copper antimony sulfosalt selected from one of a sulfantimonite and a sulfantimonate.

### Claim 25 (depends on 24)

A method according to claim 24, wherein the copper sulfide concentrate comprises famatinite.

### Claim 26 (depends on 24)

A method according to claim 24, wherein the copper sulfide concentrate comprises tetrahedrite.

### Claim 27 (depends on 24)

A method according to claim 24, wherein the pyrite is maintained at a concentration in the leach solution of at least 9 g/L.

### Claim 28 (depends on 24)

A method according to claim 24, wherein the pyrite is maintained at a concentration in the leach solution that is at least as high as one of 10, 16, 31, 40, 44, 47, 63 and 78 g/L.

### Claim 29 (depends on 24)

A method according to claim 24, wherein the pyrite:copper sulfide weight ratio is in the range of 1:1 to 20:1.

### Claim 30 (depends on 24)

A method according to claim 24, wherein the pyrite:copper sulfide weight ratio is in the range of 1:1 to 10:1.

### Claim 31 (depends on 24)

A method according to claim 24, wherein the pyrite:copper sulfide weight ratio is in the range of 3:1 to 5:1.

### Claim 32 (depends on 24)

A method according to claim 24, wherein the concentrate and the pyrite are added in the form of a mixture.

### Claim 33 (depends on 24)

A method according to claim 24, wherein at least some of the pyrite that is added is recycled pyrite obtained from the leach solution following a solid-liquid separation step.

### Claim 34 (depends on 24)

A method according to claim 24, wherein the conditions comprise maintaining an operating potential of the leach solution such that the pyrite is substantially unoxidized.

### Claim 35 (depends on 34)

A method according to claim 34, wherein the operating potential is 500 mV or less versus Ag/AgCl.

### Claim 36 (depends on 34)

A method according to claim 34, wherein the operating potential is between 400 and 550 mV versus Ag/AgCl.

### Claim 37 (depends on 34)

A method according to claim 34, wherein the operating potential is between 460 and 500 mV versus Ag/AgCl.

### Claim 38 (depends on 34)

A method according to claim 34, wherein the maintaining of the operating potential is carried out by means of selecting one or more of:
(i) a ratio of the concentrate to the pyrite;
(ii) the particle size of the concentrate and the pyrite;
(iii) an acid concentration in the leach solution; and
(iv) a temperature of the leach solution.

### Claim 39 (depends on 34)

A method according to claim 34, further comprising the step of selecting one or more of:
(i) pulp density level,
(ii) oxygen flow rate, and (iii) intensity of agitation of the leach solution, to control the operating potential.

### Claim 40 (depends on 24)

A method according to claim 24, wherein step (b) is carried out at atmospheric pressure.

### Claim 41 (depends on 24)

A method according to claim 24, wherein step (b) is carried out above atmospheric pressure.

### Claim 42 (depends on 24)

A method according to claim 24, wherein step (b) is carried out at a pulp density of 9% solids or higher.

### Claim 43 (depends on 24)

A method according to claim 24, wherein step (c) comprises a solvent extraction step and electrowinning.

### Claim 44 (depends on 43)

A method according to claim 43, wherein ferrous ions in a raffinate stream from the solvent extraction step are oxidized to ferric ions by oxygen gas and precipitated as a stable ferric salt.

### Claim 45 (depends on 24)

A method according to claim 24, wherein the pyrite is present in an ore from which the concentrate is prepared.