# US 8,277,538 B2 · Method of leaching copper sulfide ore

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,538 B2
- Document ID: US8277538B2
- Status: Granted
- Kind: B2
- Application number: 12/625,678
- Filed: 2009-11-25
- Published: 2010-12-16
- Granted: 2012-10-02
- Earliest claimed: 2009-06-16
- Assignees: JX Nippon Mining & Metals Corporation
- Inventors: Takenari Kuwazawa; Akira Miura
- Web page: https://patentgrep.com/patent/US8277538B2

## CPC

- C22B 3/18: with the aid of microorganisms or enzymes, e.g. bacteria or algae
- C22B 15/0071: {containing sulfur}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method of copper leaching without reducing the growth of iron-oxidizing bacterium and the iron-oxidizing capacity when leaching copper from a copper sulfide ore with the use of a sulfuric acid solution to which iron-oxidizing bacteria and silver have been added. Also disclosed is a method of leaching copper from a copper sulfide ore, including adding a naturally occurring nitrogen-containing organic component to a leaching solution upon copper leaching from a copper sulfide ore with the use of, as the leaching solution, a sulfuric acid solution to which iron-oxidizing bacteria and silver have been added is provided.

## Claims

### Claim 1

A method of leaching copper from a copper sulfide ore, comprising
adding a corn steep liquor to a leaching solution upon copper leaching from a copper sulfide ore,
wherein the concentration of the corn steep liquor in the leaching solution is 0.05 to 0.1 g/L and the leaching solution comprises a sulfuric acid solution to which iron-oxidizing bacteria and silver have been added.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the copper sulfide ore is a copper sulfide ore or concentrate containing chalcopyrite as a main constituent.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the silver concentration in the leaching solution is 10 to 50 mg/L.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the silver concentration in the leaching solution is 10 to 50 mg/L.