# US 8,277,537 B2 · Method of manufacturing ultra low carbon ferritic stainless steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,537 B2
- Document ID: US8277537B2
- Status: Granted
- Kind: B2
- Application number: 12/747,451
- Filed: 2008-09-30
- Published: 2011-02-24
- Granted: 2012-10-02
- Earliest claimed: 2007-12-12
- Assignees: Posco
- Inventors: Joo Hyun Park; Sun Min Byun; Sang Beom Lee; Min Oh Suk; Hee Ho Lee
- Web page: https://patentgrep.com/patent/US8277537B2

## CPC

- C21C 7/10: Handling in a vacuum
- C21C 7/0075: {Treating in a ladle furnace, e.g. up-/reheating of molten steel within the ladle}
- C21C 7/0685: {of stainless steel}
- C21C 7/072: Treatment with gases (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C21C 7/076: Use of slags or fluxes as treating agents (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C22C 38/001: {containing N}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/28: with titanium or zirconium
- Y02P 10/20: Recycling
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of manufacturing a ferritic stainless steel containing an ultra low level of carbon concentration in molten steel within time shorter than existing technology by controlling content, appropriate composition, and liquid-state fraction, etc., of Cr2 O3 in slag to maximize vacuum decarburization refining efficiency, the method comprising: tapping molten steel to a ladle in a non-deoxidized state after pre-decarburization and denitrification in an ARGON OXYGEN DECARBURIZATION refining furnace and then removing non-deoxidized slag; placing the ladle in a vacuum furnace, reducing pressure and then blowing-in oxygen gas from the upper of the molten steel through a lance; creating Al2 O3 by injecting Al at point of time of beginning of oxygen blowing; forming CaO—Al2 O3 —Cr2 O3 —MgO-based slag by injecting calcium oxide at point of time of completion of the oxygen blowing; and supplying inert gas through a porous plug on a bottom of the ladle.

## Claims

### Claim 1

A method of manufacturing an ultra low carbon ferritic stainless steel comprising:
tapping molten steel to a ladle in a non-deoxidized state after pre-decarburization and denitrification in an argon oxygen decarburization refining furnace and then removing non-deoxidized slag;
placing the ladle in a vacuum furnace, reducing pressure and then blowing-in oxygen gas from the upper of the molten steel through a lance;
creating Al2O3 by injecting Al at point of time of beginning of oxygen blowing;
forming CaO—Al2O3—Cr2O3—MgO-based slag by injecting calcium oxide at point of time of completion of the oxygen blowing; and
supplying inert gas through a porous plug on a bottom of the ladle,
wherein the CaO—Al2O3—Cr2O3—MgO-based slag is indicated as (wt % CaO)/(wt % Al2O3): 0.5 to 1.0, Cr2O3: 15 to 60 wt %, and MgO<7 wt %.

### Claim 2 (depends on 1)

The method of manufacturing the ultra low carbon ferritic stainless steel according to claim 1, wherein Al of 1.2 to 3.8 kg/t-steel is injected at the point of time of the beginning of the oxygen blowing.

### Claim 3 (depends on 1)

The method of manufacturing the ultra low carbon ferritic stainless steel according to claim 1, wherein the calcium oxide of 2.5 to 5.0 kg/t-steel is injected at the point of time of the completion of the oxygen blowing.

### Claim 4

A method of manufacturing an ultra low carbon ferritic stainless steel comprising:
tapping molten steel to a ladle in a non-deoxidized state after pre-decarburization and denitrification in an argon oxygen decarburization refining furnace and then removing non-deoxidized slag;
placing the ladle a vacuum furnace, reducing pressure and then blowing-in oxygen gas from the upper of the molten steel through a lance;
forming CaO—Al2O3—Cr2O3—MgO-based slag by injecting CaO.Al2O3 flux at point of time of completion of the oxygen blowing; and
supplying inert gas through a porous plug on a bottom of the ladle,
wherein the CaO—Al2O3—Cr2O3—MgO-based slag is indicated as (wt % CaO)/(wt % Al2O3): 0.5 to 1.0, Cr2O3: 15 to 60 wt %, and MgO<7 wt %.

### Claim 5 (depends on 1, 4)

The method of manufacturing the ultra low carbon ferritic stainless steel according to claim 1 or claim 4, wherein concentrations of carbon and nitrogen in the molten steel after completion of the argon oxygen decarburization pre-decarburization are 0.2 to 0.4 wt % and 100 ppm or less, respectively.

### Claim 6 (depends on 1, 4)

The method of manufacturing the ultra low carbon ferritic stainless steel according to claim 1 or claim 4, wherein an oxygen blower is supplied with the oxygen gas at a flow of 1000 to 1600 Nm3/hr to blow-in oxygen gas.

### Claim 7 (depends on 4)

The method of manufacturing the ultra low carbon ferritic stainless steel according to claim 4, wherein the CaO.Al2O3 flux with a size of 10 to 50 mm is injected by 7 to 10 kg/t-steel.

### Claim 8 (depends on 4)