# US 8,276,805 B2 · Method and system for brazing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,276,805 B2
- Document ID: US8276805B2
- Status: Granted
- Kind: B2
- Application number: 12/328,406
- Filed: 2008-12-04
- Published: 2010-06-10
- Granted: 2012-10-02
- Earliest claimed: 2008-12-04
- Assignees: Schlumberger Technology Corporation
- Inventors: Kjell Haugvaldstad
- Web page: https://patentgrep.com/patent/US8276805B2

## CPC

- B23K 1/0008: {specially adapted for particular articles or work}
- B23K 1/008: Soldering within a furnace (B23K1/012 takes precedence)
- B23K 3/087: {Soldering or brazing jigs, fixtures or clamping means}
- B23K 2101/002: {Drill-bits}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

This invention provides methods and systems for brazing. One aspect of the invention provides a method of brazing cutter teeth. The method includes providing a bit body, pressing at least one cutter against the bit body with a spring device, placing the bit body and the at least one cutter in an inert gas filled chamber with about 10% H2, and heating the chamber to a temperature above the melting point of the filler metal thereby melting the filler metal. A quantity of filler metal is held between each of the at least one cutters and the bit body.

## Claims

### Claim 1

A method of brazing cutter teeth, the method comprising:
providing a bit body having a longitudinal axis along a length of the bit body;
pressing at least one cutter against the bit body with an external spring device having a frame, external to the at least one cutter and positioned radially outward of the bit body, and at least one spring positioned radially between the frame and the at least one cutter, wherein the spring has a longitudinal axis along a length of the coil, and the longitudinal axis of the spring is non-parallel to the longitudinal axis of the bit body, wherein a quantity of filler metal is held between each of the at least one cutters and the bit body;
placing the bit body and the at least one cutter in an inert gas filled chamber with about 10% H2; and
heating the chamber to a temperature above the melting point of the filler metal thereby melting the filler metal.

### Claim 2 (depends on 1)

The method of claim 1, wherein the bit body has a interior cavity, the method further comprising:
introducing a heating element into the interior cavity of the bit body; and
heating the bit body with the heating element.

### Claim 3 (depends on 2)

The method of claim 2, wherein the heating element is an induction coil.

### Claim 4 (depends on 2)

The method of claim 2, wherein the bit body is heated in a controlled manner.

### Claim 5 (depends on 1)

The method of claim 1, wherein the method results in a brazing thickness of about 0.06 mm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the chamber is heated in a controlled manner.

### Claim 7 (depends on 1)

The method of claim 1, wherein the cutter teeth comprise polycrystalline diamond.

### Claim 8 (depends on 1)

The method of claim 1, wherein the filler metal is silver.

### Claim 9 (depends on 1)

The method of claim 1, wherein the filler metal is pretinned to the cutter teeth.

### Claim 10 (depends on 1)

The method of claim 1, wherein the cutter teeth are brazed in the absence of flux.

### Claim 11 (depends on 1)

The method of claim 1, wherein the inert gas is N2.

### Claim 12 (depends on 1)

The method of claim 1, wherein the chamber is heated to about 700° C.

### Claim 13

A method of brazing cutter teeth, the method comprising:
providing a bit body having a longitudinal axis along a length of the bit body, the bit body having an interior cavity;
pressing at least one cutter against the bit body with an external spring device having a frame, external to the at least one cutter and positioned radially outward of the bit body, and at least one spring positioned radially between the frame and the at least one cutter, wherein the spring has a longitudinal axis along a length of the coil, and the longitudinal axis of the spring is non-parallel to the longitudinal axis of the bit body, wherein a quantity of silver is held between each of the at least one cutters and the bit body;
placing the bit body and the at least one cutter in an inert gas filled chamber with about 10% H2; and
placing an induction element in the interior cavity of the bit body to heat the bit body in a controlled manner;
heating the chamber to a temperature above the melting point of silver thereby melting the silver.

### Claim 14 (depends on 13)

The method of claim 13 wherein the method results in a brazing thickness of about 0.06 mm.

### Claim 15 (depends on 13)

The method of claim 13 wherein the cutter teeth comprise polycrystalline diamond.

### Claim 16 (depends on 13)

The method of claim 13 wherein the silver is pretinned to the cutter teeth.

### Claim 17 (depends on 13)

The method of claim 13, wherein the cutter teeth are brazed in the absence of flux.