# US 8,276,764 B2 · Process for producing a polymer membrane, and polymer membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,276,764 B2
- Document ID: US8276764B2
- Status: Granted
- Kind: B2
- Application number: 11/899,877
- Filed: 2007-09-06
- Published: 2008-01-03
- Granted: 2012-10-02
- Earliest claimed: 2005-03-10
- Assignees: Helmholtz-Zentrum Geesthacht Zentrum für Material-und Küstenforschung GmbH
- Inventors: Detlev Fritsch; Gisela Bengtson; Katrin Ebert; Joachim Koll; Petra Merten
- Web page: https://patentgrep.com/patent/US8276764B2

## CPC

- C11C 3/126: {using catalysts based principally on other metals or derivates}
- B01D 67/00111: {Polymer pretreatment in the casting solutions}
- B01D 69/02: characterised by their properties
- B01D 69/141: {Heterogeneous membranes, e.g. containing dispersed material; Mixed matrix membranes}
- B01J 10/007: {in the presence of catalytically active bodies, e.g. porous plates}
- B01J 19/2475: {Membrane reactors}
- B01J 23/42: Platinum
- B01J 23/44: Palladium
- B01J 35/59: Membranes
- B01D 67/0016: {Coagulation}
- B01D 2323/08: Specific temperatures applied
- B01D 2325/10: Catalysts being present on the surface of the membrane or in the pores
- B01J 37/0201: {Impregnation}
- B01J 37/16: Reducing
- B01J 2219/00074: by indirect heating or cooling employing heat exchange fluids
- B01J 2219/00162: controlling the pressure
- C11C: FATTY ACIDS FROM FATS, OILS OR WAXES; CANDLES; FATS, OILS OR FATTY ACIDS BY CHEMICAL MODIFICATION OF FATS, OILS, OR FATTY ACIDS OBTAINED THEREFROM
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The invention relates to a process for producing a polymer membrane, the polymer membrane being produced from a solution, in particular a casting solution, comprising at least one first polymer. The invention further relates to a polymer membrane. The process of the invention is distinguished by the fact that a water-soluble second polymer and/or oligomer that forms phases in the solution is part of the solution. The polymer membrane of the invention, preferably produced by the process of the invention, has an oil flow rate, in particular of a refined edible oil, of greater than 200 l/m2 h bar at 60° C.

## Claims

### Claim 1

A method for the making of a microporous polymer membrane comprising the following steps:
preparation of a casting solution with a first polymer, a water soluble and phase forming second polymer and/or oligomer and with a filling material including porous particles, wherein the second polymer and/or oligomer is a block-copolymer of propylene oxide and ethylene oxide,
formation of at least one additional phase or microphase of the second polymer and/or oligomer in a temperature range between 0° C. and 40° C., wherein the second polymer and/or oligomer undergoes a thermal transition in the solution, taking place at a temperature which corresponds to a melting temperature or a glass transition temperature of the polymers and/or oligomers in the solution,
casting a membrane by drawing of the solution in a temperature range between 5° C. and 12° C.,
drying and precipitation of the drawn solution, and
washing out of the second polymer and/or oligomer from the polymer membrane;
wherein the filling material is supplemented with at least one catalyst, particularly palladium and/or platinum.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the block-copolymer is a polyethylene glycol-b-polypropylene glycol-b-polyethylene glycol block-copolymer.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the porous particles contain Al2O3, TiO2, ZrO2 and/or SiO2.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the first polymer includes polyamideimide, polysulfone, polyethersulfone, polyacrylonitrile, polyetherimide, poly(vinylidene fluoride), polyaramide, polyetheramide, polyimide and/or polyamide.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the solution is supplemented by poly(vinylpyrrolidone) (PVP) and/or wetting and dispersion material.

### Claim 6 (depends on 1)

The method according to claim 1, wherein as the solvent N-methylpyrrolidone (NMP) and/or dimethylacetamide/γ-butyrolactone (DMAc/GBL) is used.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the membrane is subsequently activated by impregnation with at least one catalyzer.

### Claim 8

A method for the making of a microporous polymer membrane comprising the following steps:
preparation of a casting solution with a first polymer, a water soluble and phase forming second polymer and/or oligomer and with a filling material including porous particles, wherein the second polymer and/or oligomer is a block-copolymer of propylene oxide and ethylene oxide,
formation of at least one additional phase or microphase of the second polymer and/or oligomer in a temperature range between 0° C. and 40° C., wherein the second polymer and/or oligomer undergoes a thermal transition in the solution, taking place at a temperature which corresponds to a melting temperature or a glass transition temperature of the polymers and/or oligomers in the solution,
casting a membrane by drawing of the solution in a temperature range between 5° C. and 12° C.,
drying and precipitation of the drawn solution,
washing out of the second polymer and/or oligomer from the polymer membrane, and subsequently activating the manufactured membrane by impregnation with at least one catalyzer.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the block-copolymer is a polyethylene glycol-b-polypropylene glycol-b-polyethylene glycol block-copolymer.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the porous particles contain Al2O3, TiO2, ZrO2 and/or SiO2.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the first polymer includes polyamideimide, polysulfone, polyethersulfone, polyacrylonitrile, polyetherimide, poly(vinylidene fluoride), polyaramide, polyetheramide, polyimide and/or polyamide.

### Claim 12 (depends on 8)

The method according to claim 8, wherein the solution is supplemented by poly(vinylpyrrolidone) (PVP) and/or wetting and dispersion material.

### Claim 13 (depends on 8)

The method according to claim 8, wherein as the solvent N-methylpyrrolidone (NMP) and/or dimethylacetamide/γ-butyrolactone (DMAc/GBL) is used.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the propylene oxide block is arranged between two ethylene oxide blocks of the second polymer and/or oligomer.

### Claim 15 (depends on 8)

The method according to claim 8, wherein the propylene oxide block is arranged between two ethylene oxide blocks of the second polymer and/or oligomer.