# US 8,137,490 B2 · Process of manufacturing cement based armor panels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,137,490 B2
- Document ID: US8137490B2
- Status: Granted
- Kind: B2
- Application number: 12/394,506
- Filed: 2009-02-27
- Published: 2010-09-16
- Granted: 2012-03-20
- Earliest claimed: 2008-03-03
- Assignees: United States Gypsum Company
- Inventors: William A. Frank; Ashish Dubey
- Web page: https://patentgrep.com/patent/US8137490B2

## CPC

- C04B 28/02: containing hydraulic cements other than calcium sulfates
- B28B 5/027: {the moulding surfaces being of the indefinite length type, e.g. belts, and being continuously fed (feeding B28B13/02)}
- B28B 7/364: {of plastic material or rubber}
- B28B 13/022: {Feeding several successive layers, optionally of different materials}
- B28B 19/0015: {on multilayered articles}
- B28C 5/365: {Mixing with driven mixing elements while transporting the mixture on an endless belt}
- B28C 5/404: {Pre-treatment of fibres}
- E04H 9/10: Independent shelters; Arrangement of independent splinter-proof walls
- F41H 5/0414: {Layered armour containing ceramic material}
- F41H 5/0428: {Ceramic layers in combination with additional layers made of fibres, fabrics or plastics}
- C04B 2111/00612: {as one or more layers of a layered structure}
- C04B 2111/00974: {for pyrotechnic applications, e.g. blasting}
- C04B 2111/1056: {Silica-free or very low silica-content materials}
- C04B 2111/2046: {Shock-absorbing materials}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- B28C: PREPARING CLAY; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL, e.g. PLASTER (preparing material for foundry moulds B22C5/00)
- E04H: BUILDINGS OR LIKE STRUCTURES FOR PARTICULAR PURPOSES; SWIMMING OR SPLASH BATHS OR POOLS; MASTS; FENCING; TENTS OR CANOPIES, IN GENERAL (foundations E02D)
- F41H: ARMOUR; ARMOURED TURRETS; ARMOURED OR ARMED VEHICLES; MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A process for making a fiber reinforced cementitious product such as a panel which hardens to an ultra-high compressive strength composite for use in making panels with ballistic and blast resistant properties. The panel has a continuous phase resulting from curing an aqueous mixture, in the absence of silica flour, of inorganic cement binder, inorganic mineral filler having a particle size of about 150-450 microns, pozzolanic mineral filler, and polycarboxylate based superplasticizer self-leveling agent, and water. The mixture may also include alkanolamine and acid or acid salt. The continuous phase may be reinforced with fiber distributed in the continuous phase before curing to form a panel. The panel may be reinforced with a fiber reinforced skin attached to at least one surface of the core, e.g., by lamination with an adhesive, e.g., epoxy, to form a ballistic and blast resistant cementitious armor panel.

## Claims

### Claim 1

A method of making a blast resistant panel comprising:
preparing a self leveling cementitious aqueous mixture of
25-45 weight % inorganic cement binder,
an absence of silica flour,
35-65 weight % sand having a particle size of about 150-450 microns,
5-15 weight % pozzolanic filler having a median particle size of less than or equal to 50 microns,
0.25-5.0 weight % polycarboxylate based self-leveling agent, and
6-12 weight % water,
forming the uniform mixture into a fiber reinforced cementitious panel;
curing the fiber reinforced cementitious panel to produced a partially hardened cementitious panel,
sanding the surfaces of the partially hardened cementitious panel,
cutting the partially hardened cementitious panel to a desired size,
curing the partially hardened cementitious panel to a final hardened cementitious panel.

### Claim 2 (depends on 1)

The method of claim 1, adding to the aqueous mixture reinforcing fiber in an amount of about 0.5-6.0% by volume of the aqueous mixture.

### Claim 3 (depends on 1)

The method of claim 1, wherein the cementitious panel has a compressive strength of more than about 10,000 psi when cured.

### Claim 4 (depends on 1)

The method of claim 1, wherein a cementitious panel resulting from the curing of the aqueous mixture has a compressive strength of about 15,000 psi when cured.

### Claim 5 (depends on 2)

The method of claim 2, wherein the cementitious panel has a compressive strength of more than about 25,000 psi when cured.

### Claim 6 (depends on 1)

The method of claim 1, wherein the aqueous mixture comprises an alkanolamine in an amount of about 0.005 wt. % to about 0.500 wt. % by weight of the cement binder, and an acid or acid salt in an amount of about 0.10 wt. % to about 1.80 wt. % by weight of the combined weight of the cement binder and pozzolanic filler.

### Claim 7 (depends on 2)

The method of claim 2, wherein the reinforcing fiber is fiber glass.

### Claim 8 (depends on 2)

The method of claim 2, wherein the pozzolanic mineral filler is silica fume.

### Claim 9 (depends on 1)

The method of claim 1, wherein the polycarboxylate self leveling agent is a polyether and is present in an amount of about 0.75 to about 2.5% by wt. of the cementitious mixture on a dry basis.

### Claim 10 (depends on 1)

The method of claim 1, wherein the weight ratio of pozzolanic filler to inorganic cement binder is about 0.05 to 0.30:1.0.

### Claim 11 (depends on 1)

The method of claim 1, wherein the weight ratio of sand to the combined weight of inorganic cement binder and pozzolanic filler is about 0.75 to about 1.50:1.0.

### Claim 12 (depends on 1)

The method of claim 1, wherein the weight ratio of water to the combined weight of the inorganic cement binder and pozzolanic filler dry reactive powders is less than or equal to about 0.35:1.0.

### Claim 13 (depends on 1)

The method of claim 1, wherein the weight ratio of pozzolanic filler to inorganic cement binder is about 0.15 to about 0.20:1.0; the weight ratio of sand to the combined weight of inorganic cement binder and pozzolanic filler is about 0.90 to 1.10:1.0; and the weight ratio of water to the combined weight of the inorganic cement binder and pozzolanic filler dry reactive powders in the continuous phase is less than or equal to about 0.20:1.0.

### Claim 14 (depends on 1)

The method of claim 1, wherein the particle size of the sand is about 250 to about 350 microns.

### Claim 15 (depends on 1)

The method of claim 1, wherein the median particle size of the pozzolanic filler is less than about 0.1 microns.

### Claim 16 (depends on 1)

The method of claim 1, wherein the aqueous cementitious mixture is deposited on a layer of chopped glass fiber on a carrier on a continuous conveyor to form a first layer of cementitious slurry and glass fibers, a second layer of chopped glass fibers is then deposited over the top surface of the formed panel and the formed panel is passed through embedment rollers to embed the fibers into the panel,
a second layer of slurry is deposited over the second layer of chopped glass fiber, and
the panel is leveled to a smooth surface with a screed bar before the panel is cured to a cementitious panel.

### Claim 17 (depends on 16)

The method of claim 16, wherein the embedment of the reinforcing fibers is performed by passing the layer of slurry and fibers through embedment rollers having disks that are spaced from about 0.1 in. to about 0.25 in. (0.25 to 0.63 cm) apart to allow for embedment of the fibers in the cementitious material.

### Claim 18 (depends on 16)

The method of claim 16, wherein the composition cures after 2 days to a compressive strength of less than about 2000 psi to about 4000 psi and develops a compressive strength of over 20,000 psi after curing for 28 days.

### Claim 19

A method of making a blast resistant panel comprising:
preparing a cementitious mixture into a cementitious core comprising:
a continuous phase resulting from the curing of a self leveling cementitious aqueous mixture of:
5-45 weight % inorganic cement binder,
in the absence of silica flour,
35-65 weight % sand having a particle size of about 250-350 microns,
5-15 weight % pozzolanic filler having a median particle size of less than or equal to 0.1 microns,
1.0-1.2 weight % polycarboxylate based self-leveling agent,
triethanolamine an in an amount of about 0.025 to about 0.075 wt. % by weight of the cement binder,
tartaric acid an acid in an amount of about 0.40 to about 0.60 wt. % by weight of the combined weight of the cement binder and pozzolanic filler, and
6-12 weight % water,
adding fiber glass reinforcing fiber in an amount of about 3.0-3.5% by volume to the mixture to form a uniform mixture,
forming the uniform mixture into a fiber reinforced cementitious panel;
curing the fiber reinforced cementitious panel to produced a partially hardened cementitious panel,
sanding the surfaces of the partially hardened cementitious panel,
cutting the partially hardened cementitious panel to a desired size,
curing the partially hardened cementitious panel to a final hardened cementitious panel, and
attaching a fiber glass reinforced polyester laminate skin layer to at least one surface of the cementitious panel.

### Claim 20 (depends on 19)

The method of claim 19, wherein the pozzolanic filler is silica fume, wherein the composition cures after 2 days to a compressive strength of less than about 2000 psi to about 4000 psi and develops a compressive strength of over 20,000 psi after curing for 28 days.