# US 8,017,306 B2 · Method for producing conductive film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,017,306 B2
- Document ID: US8017306B2
- Status: Granted
- Kind: B2
- Application number: 12/696,683
- Filed: 2010-01-29
- Published: 2010-08-12
- Granted: 2011-09-13
- Earliest claimed: 2009-02-02
- Assignees: FUJIFILM Corporation
- Inventors: Tsukasa Tokunaga; Hiroshi Sakuyama
- Web page: https://patentgrep.com/patent/US8017306B2

## CPC

- G03C 5/58: Processes for obtaining metallic images by vapour deposition or physical development (images obtained by photomechanical means, e.g. by etching G03F)
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A conductive film producing method includes a metallic silver forming step of exposing and developing a photosensitive material having a 95-μm-thick long support and thereon a silver salt-containing emulsion layer, thereby forming a metallic silver portion to prepare a conductive film precursor, and a smoothing treatment step of subjecting the conductive film precursor to a smoothing treatment to produce a conductive film. In the smoothing treatment, the conductive film precursor is pressed by first and second calender rolls facing each other, and the first calender roll is a resin roll to be brought into contact with the support. The method satisfies the condition of 1/2≦P1/P2≦1, wherein P1 represents a conveying force applied when the conductive film precursor is introduced to an area where the smoothing treatment step is conducted, and P2 represents a conveying force applied when the smoothing-treated conductive film is discharged from the area.

## Claims

### Claim 1

A method for producing a conductive film, comprising
a metallic silver forming step of exposing and developing a photosensitive material comprising a long support and thereon an emulsion layer containing a silver salt, thereby forming a metallic silver portion to prepare a conductive film precursor, and
a smoothing treatment step of subjecting the conductive film precursor to a smoothing treatment to produce a conductive film, wherein
the support has a thickness of 95 μm or more,
the conductive film precursor is pressed by a first calender roll and a second calender roll facing each other in the smoothing treatment,
the first calender roll is a resin roll and is brought into contact with the support, and
the method satisfies the condition of
1/2≦P1/P2≦1
wherein P1 represents a conveying force applied when the conductive film precursor is introduced to an area where the smoothing treatment step is conducted, and P2 represents a conveying force applied when the smoothing-treated conductive film is discharged from the area where the smoothing treatment step is conducted.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the method satisfies the condition of
0.58≦R2/R1≦0.77
wherein R1 represents the surface resistance of the conductive film precursor, and R2 represents the surface resistance of the conductive film.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the support has a thickness of 95 μm or more and 150 μm or less.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the photosensitive material has a thickness of 100 μm or more and 200 μm or less.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the conductive film has a length of 2 m or more.

### Claim 6 (depends on 1)

A method according to claim 1, wherein the second calender roll is a metal roll and is brought into contact with the metallic silver portion.

### Claim 7 (depends on 6)

A method according to claim 6, wherein the metal roll has an embossed surface.

### Claim 8 (depends on 6)

A method according to claim 6, wherein the metal roll has a surface roughness of 0.05 to 0.8 s in maximum height Rmax.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the emulsion layer has a silver/binder volume ratio of 1/1 or more.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the smoothing treatment is carried out while applying a load (line pressure) of 200 to 600 kgf/cm (1960 to 5880 N/cm) to the conductive film precursor.

### Claim 11 (depends on 1)

A method according to claim 1, wherein the smoothing treatment is carried out while conveying the conductive film precursor at a conveying rate of 10 to 50 m/minute.