Surfactants and polymerizable surfactants based on room-temperature ionic liquids that form lyotropic liquid crystal phases with water and room-temperature ionic liquids
AssigneeThe Regents of the University of Colorado
InventorsDouglas L. Gin, Jason E. Bara, Richard D. Noble, Xiaohui Zeng
Life of this patent
Estimating the term…
Abstract
A modular surfactant architecture based on room temperature ionic liquids (RTILs) has been developed that affords non-polymerizable and polymerizable amphiphiles that form lamellar (L), hexagonal (H) or bicontinuous cubic (Q) LLC phases when mixed with water or RTILs serving as the polar solvent. The amphiphiles are imidazolium salts having two or more imidazolium head groups joined by one or more spacers. Polymerization of the LLC assembly can produce polymeric materials having ordered nanopores, with the ordering of the pores determined by the LLC phase.
Claims24
A polymerizable surfactant composition having the general formula:
- wherein X is an anion;
- Y1 and Y2 each are a hydrophobic tail group consisting of a linear alkylene group attached to a polymerizable group P, with the tail group as a whole having at least 10 carbon atoms;
- Z1, Z2, Z3, Z4, Z5 and Z6 each are hydrogen or a hydrophobic tail group comprising from 1 to 12 carbon atoms;
- and
- L is a spacer group which comprises an alkylene group having from 1 to 12 carbon atoms, comprises 1 to 6 ether groups or is —(CH2CH2—(O—CH2—CH2)p—, where p is 1 to 3.
A lyotropic liquid crystal system comprising
- a surfactant having the composition given by
- Wherein X is an anion;
- Y1 and Y2 each are a hydrophobic tail group comprising at least 10 carbon atoms and optionally comprising a polymerizable group;
- Z1, Z2, Z3, Z4, Z5 and Z6 each are hydrogen or a hydrophobic tail group comprising from 1 to 12 carbon atoms;
- and
- L is a spacer group which comprises an alkylene group having from 1 to 12 carbon atoms, comprises 1 to 6 ether groups, or is —(CH2CH2—(O—CH2—CH2)p—, where p is 1 to 3;
- and
- a polar solvent,
- wherein the concentration of the surfactant is between 10 wt % and 100 wt % and the surfactant forms a lyotropic liquid crystal phase in combination with the solvent.
A cross-linked lyotropic liquid crystal (LLC) polymer comprising polymerizable surfactants which have been crosslinked, wherein the cross-linked polymerizable surfactants form a LLC phase and the polymerizable surfactants have the general formula:
- wherein X is an anion;
- Y1 and Y2 each are a hydrophobic tail group comprising a polymerizable group P, and at least 10 carbon atoms;
- Z1, Z2, Z3, Z4, Z5 and Z6 each are hydrogen or a hydrophobic tail group comprising from 1 to 12 carbon atoms;
- and
- L is a spacer group which comprises an alkylene group having from 1 to 12 carbon atoms, comprises 1 to 6 ether groups or is —(CH2CH2—(O—CH2—CH2)p—, where p is 1 to 3.
A method of making a cross-linked lyotropic liquid crystal (LLC) polymer, the method comprising the steps of:
- a. preparing an LLC polymerization mixture comprising a plurality of a polymerizable surfactant, a polymerization initiator and a polar solvent selected from the group consisting of water, imidazolium based room temperature ionic liquids, and mixtures thereof, wherein the surfactant forms a lyotropic liquid crystal phase in combination with the solvent and the polymerizable surfactants has the general formula:
- wherein X is an anion;
- Y1 and Y2 each are a hydrophobic tail group comprising a polmerizable group P, and at least 10 carbon atoms;
- Z1, Z2, Z3, Z4, Z5 and Z6 each are hydrogen or a hydrophobic tail group comprising from 1 to 12 carbon atoms;
- and
- L is a spacer group which comprises an alkylene group having from 1 to 12 carbon atoms, comprises 1 to 6 ether groups or is —(CH2CH2—(O—CH2—CH2)p—, where p is 1 to 3;
- b. cross-linking at least some of the surfactants.
Dependencies are inferred from the claim text.