# US 7,857,904 B2 · Process of producing roofing shingle coating asphalt

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,857,904 B2
- Document ID: US7857904B2
- Status: Granted
- Kind: B2
- Application number: 12/002,648
- Filed: 2007-12-18
- Published: 2009-01-01
- Granted: 2010-12-28
- Earliest claimed: 2007-06-28
- Assignees: Owens Corning Intellectual Capital, LLC
- Inventors: David C. Trumbore; David R. Jones, IV; Edward R. Harrington; Donn R. Vermilion; Jason D. Guerra
- Web page: https://patentgrep.com/patent/US7857904B2

## CPC

- C08L 91/06: Waxes
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C10C 3/04: by blowing or oxidising {, e.g. air, ozone}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C10C: WORKING-UP PITCH, ASPHALT, BITUMEN, TAR; PYROLIGNEOUS ACID (compositions of bituminous materials C08L95/00; carbon filaments by decomposition of organic filaments D01F9/14)

## Abstract

A process of producing a roofing shingle coating asphalt from an asphalt feedstock includes the following steps. Wax and blowing catalyst are added to the asphalt feedstock. Then the asphalt feedstock is blown to produce the coating asphalt. The coating asphalt has a softening point within a range of from about 190° F. (88° C.) to about 235° F. (113° C.) and has a penetration of at least about 15 dmm at 77° F. (25° C.).

## Claims

### Claim 1

A process of producing a roofing shingle coating asphalt from an asphalt feedstock comprising the following steps:
adding wax and a blowing catalyst to the asphalt feedstock; and then
blowing the asphalt feedstock to produce the coating asphalt;
the coating asphalt having a softening point within a range of from about 190° F. (88° C.) to about 235° F. (113° C.) and having a penetration of at least about 15 dmm at 77° F. (25° C.),
wherein said wax has a melt point of at least about 90° C.

### Claim 2 (depends on 1)

The process of claim 1 wherein the blowing catalyst comprises phosphoric acid added in an amount within a range of from about 0.1% to about 5% by total weight of the phosphoric acid and the asphalt.

### Claim 3 (depends on 1)

The process of claim 1 wherein the wax has a melt point of at least about 100° C.

### Claim 4 (depends on 1)

The process of claim 1 wherein the feedstock asphalt comprises paving asphalt.

### Claim 5 (depends on 1)

The process of claim 1 wherein the feedstock asphalt comprises polymer modified asphalt.

### Claim 6 (depends on 1)

The process of claim 1 wherein the coating asphalt has a melt viscosity within a range of from about 130 cps to about 420 cps at 400° F. (204° C.).

### Claim 7 (depends on 1)

The process of claim 1 wherein the coating asphalt has a durability of greater than about 60 cycles in a weatherometer.

### Claim 8 (depends on 1)

The process of claim 1 wherein the coating asphalt has a stain index less than about 10.

### Claim 9 (depends on 1)

The process of claim 1 further comprising adding a polymer to the asphalt at any time during the process.

### Claim 10 (depends on 1)

The process of claim 1 further comprising blending a polymer modified asphalt with the coating asphalt produced by the process.

### Claim 11

A process of producing a roofing shingle coating asphalt from an asphalt feedstock comprising:
partially blowing the asphalt feedstock to raise its softening point to a first softening point that is lower than a target range;
adding wax to the partially blown asphalt, said wax having a melt point of at least about 90° C.; and
further blowing the asphalt to further raise its softening point to a second softening point that is within the target range; and
adding a blowing catalyst to the asphalt before or during the blowing;
the process producing a coating asphalt having a softening point within the target range of from about 190° F. (88° C.) to about 235° F. (113° C.) and having a penetration of at least about 15 dmm at 77° F. (25° C.).

### Claim 12 (depends on 11)

The process of claim 11 wherein the blowing catalyst comprises phosphoric acid added in an amount within a range of from about 0.1% to about 5% by total weight of the phosphoric acid and the asphalt.

### Claim 13 (depends on 11)

The process of claim 11 wherein the feedstock asphalt comprises paving asphalt.

### Claim 14 (depends on 11)

The process of claim 11 wherein the feedstock asphalt comprises polymer modified asphalt.

### Claim 15 (depends on 11)

The process of claim 11 wherein the coating asphalt has a melt viscosity within a range of from about 130 cps to about 420 cps at 400° F. (204° C.).

### Claim 16 (depends on 11)

The process of claim 11 wherein the coating asphalt has a durability of greater than about 60 cycles in a weatherometer.

### Claim 17 (depends on 11)

The process of claim 11 wherein the coating asphalt has a stain index less than about 10.

### Claim 18 (depends on 11)

The process of claim 11 further comprising adding a polymer to the asphalt at any time during the process.

### Claim 19 (depends on 11)

The process of claim 11 further comprising blending a polymer modified asphalt with the coating asphalt produced by the process.

### Claim 20 (depends on 11)

The process of claim 11, wherein said wax has a melt point of at least about 100° C.

### Claim 21

A process of producing a roofing shingle coating asphalt from an asphalt feedstock comprising the following steps:
blowing the asphalt feedstock with a high level of blowing catalyst such that the blowing step is effective to raise the softening point of the asphalt to within a target range of from about 190° F. (88° C.) to about 235° F. (113° C.) and to lower the penetration of the asphalt to within a target range of from about 15 dmm to about 28 dmm at 77° F. (25° C.), the blowing step raising the melt viscosity of the asphalt to higher than a target range; and
adding wax to the blown asphalt after said blowing step to lower its melt viscosity to within the target range of from about 130 cps to about 420 cps at 400° F. (204° C.); and
blending a polymer modified asphalt with the blown asphalt.

### Claim 22 (depends on 21)

The process of claim 21 wherein the blowing catalyst comprises phosphoric acid.

### Claim 23 (depends on 22)

The process of claim 22 wherein the phosphoric acid is added in an amount within a range of from about 2% to about 7% active by total weight of the phosphoric acid and the asphalt.

### Claim 24 (depends on 21)

The process of claim 21 wherein the feedstock asphalt comprises paving asphalt.

### Claim 25 (depends on 21)

The process of claim 21 wherein the wax is added in an amount within a range of from about 0.5% to about 8% by total weight of the wax and the asphalt.

### Claim 26 (depends on 21)

The process of claim 21, wherein said blowing catalyst is added in an amount from about 2 to about 7% by weight of said blowing catalyst and said asphalt.

### Claim 27 (depends on 21)

The process of claim 21, wherein said wax has a melt point of at least about 90° C.

### Claim 28 (depends on 21)

The process of claim 21, wherein said wax has a melt point of at least about 100° C.