Anti-microbial carpet underlay and method of making
AssigneeL&P Property Management Company
InventorsStephen D. Gilder, Martin J. Lovato, William A. Griggs
Life of this patent
Estimating the term…
Abstract
A method for making antimicrobial rebonded carpet pad includes mixing zinc pyrithione with a polyol to form an antimicrobial polyol mixture concentrate, blending the antimicrobial polyol mixture concentrate with a binder stream, mixing the binder with foam particles and curing the binder. The percentage of zinc pyrithione mixed with the polyol and the addition ratio of the antimicrobial polyol mixture concentrate with the binder stream are selected to provide an overall concentration of zinc pyrithione in the binder of at least about 7500 ppm. The particles and binder are cured into a block and sliced to form carpet pad.
Claims11
A method, for making rebonded carpet pad, comprising:
- mixing zinc pyrithione with a polyol to form an antimicrobial polyol mixture concentrate;
- blending the antimicrobial polyol mixture concentrate with a binder stream to form a binder;
- selecting a percentage of zinc pyrithione mixed with the polyol and an addition ratio of the antimicrobial polyol mixture concentrate with the binder stream to provide an overall concentration of zinc pyrithione in the binder of at least about 7500 ppm;
- mixing the binder with foam particles;
- shaping the mixture of binder and foam particles into a block, curing the binder and slicing the block to a thickness to form carpet pad;
- and
- laminating a 0.45 to 0.5 mil monolayer blown film to at least one side of the carpet pad;
- wherein laminating a film to at least one side of the carpet pad comprises:
- forming an 0.45 to 0.5 mil monolayer blown film;
- and
- thermally laminating the film to at least one side of the carpet pad;
- wherein the film comprises an effective amount of an antimicrobial compound, and wherein the antimicrobial compound comprises zinc pyrithione;
- and
- wherein the net effective concentration of zinc pyrithione in the film is from about 500 ppm to 850 ppm.
Dependencies are inferred from the claim text.