# US 7,776,472 B2 · Anode material for secondary battery, method for producing the same and secondary batteries using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,776,472 B2
- Document ID: US7776472B2
- Status: Granted
- Kind: B2
- Application number: 11/653,330
- Filed: 2007-01-12
- Published: 2007-07-19
- Granted: 2010-08-17
- Earliest claimed: 2006-01-16
- Assignees: LS Mitron Ltd.
- Inventors: Ho-Gun Kim; Jong-Sung Kim; Dong-Hun Shin; Chul Youm; Jeong-Hun Oh
- Web page: https://patentgrep.com/patent/US7776472B2

## CPC

- H01M 4/587: for inserting or intercalating light metals
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are an anode material for a secondary battery, a method for producing the same and a secondary battery using the same. The present invention provides the anode material for a secondary battery produced by coating a high-crystallinity core carbonaceous material with a coating carbonaceous material and calcinating the high-crystallinity core carbonaceous material, wherein the anode material has a specific volume of 0.002 cc/g or less. The anode material for a secondary battery of the present invention may be produced by coating a high-crystallinity core carbonaceous material with a coating carbonaceous material and undergoing a predetermined calcination process, and the anode material can have an increased volume ratio of the micropores. Accordingly, the secondary battery of the present invention may be useful to improve charging/discharging capacity and efficiency since sorption of lithium ion in the anode material is improved.

## Claims

### Claim 1

An anode material for a secondary battery produced by coating a high-crystallinity core carbonaceous material with a coating carbonaceous material and calcinating the high-crystallinity core carbonaceous material,
wherein total pores of the anode material for a secondary battery have a specific volume of 0.002 cc/g or less, and a volume of pores (micropores) having a diameter of less than 40 nm is 10% or more of the total pore volume and a volume of pores (micropores) having a diameter of 40 to 180 nm is 90% or less of the total pore volume.

### Claim 2 (depends on 1)

The anode material for a secondary battery according to claim 1,
wherein the coating carbonaceous material, used for coating the core carbonaceous material, accounts for 5% by weight or more before the calcination.

### Claim 3 (depends on 1)

The anode material for a secondary battery according to claim 1,
wherein the anode material for a secondary battery has a tap density of 1.0 g/cm3 or more.

### Claim 4 (depends on 1)

The anode material for a secondary battery according to claim 1,
wherein the anode material for a secondary battery has a BET specific surface area of 4 m2/g or less.

### Claim 5 (depends on 1)

The anode material for a secondary battery according to claim 1,
wherein the high-crystallinity core carbonaceous material is natural graphite.

### Claim 6 (depends on 5)

The anode material for a secondary battery according to claim 5,
wherein the natural graphite is spheroidized natural graphite, and has a tap density of 0.8 g/cm3 or above.

### Claim 7 (depends on 1)

The anode material for a secondary battery according to claim 1,
wherein the coating carbonaceous material has a softening temperature of 100° C. or more.

### Claim 8

A secondary battery produced by using, as a battery anode, an anode material for a secondary battery produced by coating a high-crystallinity core carbonaceous material with a coating carbonaceous material and calcinating the high-crystallinity core carbonaceous material,
wherein total pores of the anode material for a secondary battery have a specific volume of 0.002 cc/g or less, and a volume of pores (micropores) having a diameter of less than 40 nm is 10% or more of the total pore volume and a volume of pores (micropores) having a diameter of 40 to 180 nm is 90% or less of the total pore volume.

### Claim 9 (depends on 8)

The secondary battery according to claim 8,
wherein the coating carbonaceous material, used for coating the core carbonaceous material, accounts for 5% by weight or more before the calcination.

### Claim 10 (depends on 8)

The secondary battery according to claim 8,
wherein the anode material for a secondary battery has a tap density of 1.0 g/cm3 or more.

### Claim 11 (depends on 8)

The secondary battery according to claim 8,
wherein the anode material for a secondary battery has a BET specific surface area of 4 m2/g or less.

### Claim 12 (depends on 8)

The secondary battery according to claim 8,
wherein the high-crystallinity core carbonaceous material is natural graphite.

### Claim 13 (depends on 12)

The secondary battery according to claim 12,
wherein the natural graphite is spheroidized natural graphite, and has a tap density of 0.8 g/cm3 or above.

### Claim 14 (depends on 8)

The secondary battery according to claim 8,
wherein the coating carbonaceous material has a softening temperature of 100° C. or more.

### Claim 15 (depends on 8)

The secondary battery according to claim 8,
wherein the anode material for a secondary battery has a discharging capacity of 340 mAh/g or more and a charging/discharging efficiency of 90% or more.

### Claim 16

A method for producing an anode material for a secondary battery, comprising:
(S1) preparing a core carbonaceous material having a tap density of 0.8 g/cm3 or more and a content of 95% by weight or less, and a coating carbonaceous material having a softening temperature of 100° C. or above and a content of 5% by weight or more;
(S2) mixing the materials by means of wet stirring to obtain a mixture in which the core carbonaceous material is coated with the coating carbonaceous material; and
(S3) calcinating the mixture to obtain an anode material in which the core carbonaceous material is coated with the coating carbonaceous material,
wherein total pores in the anode material for a secondary battery have a specific volume of 0.002 cc/g or less, and a volume of pores (micropores) having a diameter of less than 40 nm is 10% or more of the total pore volume and a volume of pores (micropores) having a diameter of 40 to 180 nm is 90% or less of the total pore volume.

### Claim 17 (depends on 16)

The method for producing an anode material for a secondary battery according to claim 16,
wherein the core carbonaceous material of the step (S1) is natural graphite.

### Claim 18 (depends on 16)

The method for producing an anode material for a secondary battery according to claim 16,
wherein the calcination of the step (S3) is carried out at a temperature of 1,000 to 2,500° C.

### Claim 19 (depends on 16)

The method for producing an anode material for a secondary battery according to claim 16,
wherein the calcination of the step (S3) is sequentially carried out under different temperature conditions.

### Claim 20 (depends on 19)

The method for producing an anode material for a secondary battery according to claim 19,
wherein the calcination, sequentially carried out under the different temperature conditions, is carried out at a relatively higher calcination temperature in the latter step than in the former step.