Photocatalyst composition and photocatalyst containing layer
AssigneeDai Nippon Printing Co., Ltd.
InventorKiyoshi Itoh
Life of this patent
Estimating the term…
Abstract
The main object of the present invention is to provide a photocatalyst composition and a photocatalyst containing layer showing a high activity in a short period of time, and a pattern formed body using the photocatalyst containing layer. To attain the object, the invention provides a photocatalyst composition containing at least a photocatalyst, characterized by including a portion with the signal intensity of the electron spin resonance spectrum derived from the hydroxy radical increased to 1,000 times or more in 1 second within 600 seconds of the start of the ultraviolet ray irradiation at the time of measuring the electron spin resonance spectrum while irradiating the ultraviolet ray.
Claims6
A production method for a photocatalyst containing layer comprising an examination process for selecting only a photocatalyst containing layer including a portion which increases a signal intensity of an electron spin resonance spectrum derived from a hydroxy radical to 1,000 times or more in 1 second within 600 seconds of a start of an irradiation of an ultraviolet ray by measuring the electron spin resonance spectrum while irradiating the ultraviolet ray to the photocatalyst containing layer containing at least a photocatalyst.
A production method for a pattern formed body for producing a pattern formed body:
- by disposing a counter substrate and a photocatalyst containing layer side substrate which comprises a base body and a photocatalyst containing layer containing at least a photocatalyst formed on the base body, facing with each other;
- and by irradiating an energy in a pattern to form a property changeable pattern in which a property is changed on the counter substrate,
- wherein an examination process for selecting only the photocatalyst containing layer side substrate including a portion which increases a signal intensity of an electron spin resonance spectrum derived from a hydroxy radical to 1,000 times or more in 1 second within 600 seconds of a start of an irradiation of an ultraviolet ray by measuring the electron spin resonance spectrum while irradiating the ultraviolet ray to the photocatalyst containing layer is comprised.
Dependencies are inferred from the claim text.