# US 7,718,509 B2 · Method for producing bonded wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,718,509 B2
- Document ID: US7718509B2
- Status: Granted
- Kind: B2
- Application number: 12/473,122
- Filed: 2009-05-27
- Published: 2009-12-03
- Granted: 2010-05-18
- Earliest claimed: 2008-06-03
- Assignees: Sumco Corporation
- Inventors: Akihiko Endo; Tatsumi Kusaba
- Web page: https://patentgrep.com/patent/US7718509B2

## CPC

- H10P 10/128: {by direct semiconductor to semiconductor bonding}
- H10P 90/1922: {using silicon etch back techniques, e.g. BESOI or ELTRAN}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A bonded wafer is produced by comprising a step of implanting oxygen ions from a surface of a wafer for active layer to form an oxygen ion implanted layer at a given position inside the wafer for active layer; a step of bonding the wafer of active layer to a wafer for support substrate directly or through an insulating film; a step of subjecting the resulting bonded wafer to a heat treatment for increasing a bonding strength; a step of removing a portion of the wafer for active layer in the bonded wafer to a given position not exposing the oxygen ion implanted layer by a given method; a step of exposing the entire surface of the oxygen ion implanted layer; and a step of removing the exposed oxygen ion implanted layer to obtain an active layer of a given thickness, wherein the step of exposing the entire surface of the oxygen ion implanted layer is carried out by a dry etching under given conditions.

## Claims

### Claim 1

A method for producing a bonded wafer, comprising a step of implanting oxygen ions from a surface of a wafer for active layer to form an oxygen ion implanted layer at a given position inside the wafer for active layer; a step of bonding the wafer of active layer to a wafer for support substrate directly or through an insulating film so as to form a bonded wasfer; a step of subjecting the resulting bonded wafer to a heat treatment for increasing a bonding strength; a step of removing a portion of the wafer for active layer in the bonded wafer to a given position not exposing the oxygen ion implanted layer by a given method; a step of exposing the entire surface of the oxygen ion implanted layer; and a step of removing the exposed oxygen ion implanted layer to obtain an active layer of a given thickness, wherein the step of exposing the entire surface of the oxygen ion implanted layer is carried out by a dry etching under given conditions
wherein the oxygen ion implanted layer has an oxygen concentration peak of not less than 1×1022 atoms/cm3 and satisfies a relationship of Re>2×{(ts)/(to)}×{(De+Dt)/(100−De)} when a thickness and a variation in an in-plane thickness of a silicon layer in the wafer for active layer on the oxygen ion implanted layer before the dry etching are ts and ±Dt %, respectively, and a thickness of the oxygen ion implanted layer is to and an etching rate ratio of Si to silicon oxide film (Si/SiOx) is Re and a variation in an in-plane etching is ±De %.

### Claim 2 (depends on 1)

A method for producing a bonded wafer according to claim 1, wherein the dry etching is a reactive ion etching using a mixed gas of sulfur hexafluoride, carbon tetrafluoride, trifluoromethane or xenon difluoride, and oxygen or hydrogen chloride as a dry etching gas.

### Claim 3 (depends on 1)

A method for producing a bonded wafer according to claim 1, wherein a crystal orientation of a bonding face between the wafer for active layer and the wafer for support substrate is <100>, <110>or <111>.