# US 7,682,780 B2 · Industrial X-ray photosensitive material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,682,780 B2
- Document ID: US7682780B2
- Status: Granted
- Kind: B2
- Application number: 12/486,770
- Filed: 2009-06-18
- Published: 2010-01-14
- Granted: 2010-03-23
- Earliest claimed: 2008-07-08
- Assignees: FUJIFILM Corporation
- Inventors: Masayoshi Fujita; Yoshihisa Hashi
- Web page: https://patentgrep.com/patent/US7682780B2

## CPC

- G03C 5/16: X-ray, infrared, or ultraviolet ray processes
- G03C 1/0051: {Tabular grain emulsions}
- G03C 1/09: Noble metals or mercury; Salts or compounds thereof; Sulfur, selenium or tellurium, or compounds thereof, e.g. for chemical sensitising (G03C1/34, G03C1/35 take precedence)
- G03C 5/17: using screens to intensify X-ray images (X-ray conversion screens G21K4/00)
- Y10S 430/167: X-ray
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

An industrial X-ray photosensitive material including at least one silver halide emulsion layer on both sides of a transparent support, wherein the silver halide emulsion layer contains tabular silver halide particles having an average particle thickness of less than 0.2 μm and an aspect ratio of more than 8, a core of the particles which is a core having a volume of 1% or more and less than 3% of a particle volume does not contain Ir or Rh, and a shell of the particles which is a shell having a volume of 97% or more and less than 99% of a particle volume contains at least Ir or Rh. An industrial X-ray photosensitive material having rapid processing suitability, as well as high sensitivity and high contrast is provided.

## Claims

### Claim 1

An industrial X-ray photosensitive material comprising at least one silver halide emulsion layer on both sides of a transparent support, wherein the silver halide emulsion layer contains tabular silver halide particles having an average particle thickness of from 0.03 μm to 0.15 μm and an aspect ratio of more than 8, a core of the particles which is a core having a volume of 1% or more and less than 3% of a particle volume does not contain Ir or Rh, and a shell of the particles which is a shell having a volume of 97% or more and less than 99% of a particle volume contains at least Ir or Rh.

### Claim 2 (depends on 1)

The industrial X-ray photosensitive material according to claim 1, wherein the shell contains Ir or Rh in an amount of from 1×10−9 mol % to 1×10−2 mol % per 1 mole of silver.

### Claim 3 (depends on 1)

The industrial X-ray photosensitive material according to claim 1, wherein a water swelling value per one side of the industrial X-ray photosensitive material is less than 20 μm.

### Claim 4 (depends on 1)

The industrial X-ray photosensitive material according to claim 1, wherein an amount of coated silver per one side of the industrial X-ray photosensitive material is less than 5.5 g/m2.

### Claim 5 (depends on 1)

The industrial X-ray photosensitive material according to claim 1, wherein a ratio by weight of a total amount of coated gelatin to an amount of coated silver per one side of the industrial X-ray photosensitive material (total amount of coated gelatin/amount of coated silver) is from 1.4 to 1.8.

### Claim 6 (depends on 2)

The industrial X-ray photosensitive material according to claim 2, wherein a water swelling value per one side of the industrial X-ray photosensitive material is less than 20 μm.

### Claim 7 (depends on 2)

The industrial X-ray photosensitive material according to claim 2, wherein an amount of coated silver per one side of the industrial X-ray photosensitive material is less than 5.5 g/m2.

### Claim 8 (depends on 2)

The industrial X-ray photosensitive material according to claim 2, wherein a ratio by weight of a total amount of coated gelatin to an amount of coated silver per one side of the industrial X-ray photosensitive material (total amount of coated gelatin/amount of coated silver) is from 1.4 to 1.8.

### Claim 9 (depends on 1)

The industrial X-ray photosensitive material according to claim 1, wherein a total processing time (Dry to Dry) is 3 minutes and 30 seconds or shorter.

### Claim 10 (depends on 1)

The industrial X-ray photosensitive material according to claim 1, wherein the aspect ratio of tabular silver halide particles is from 9 to 16.