Production method of an electroacoustic transducer diaphragm, electroacoustic transducer diaphragm, and an electroacoustic transducer
AssigneeVictor Company of Japan, Ltd.
InventorsYoshiaki Suzuki, Tomoaki Ogata, Yoshiaki Tanaka
Life of this patent
Estimating the term…
Abstract
A production method for an electroacoustic transducer diaphragm includes producing an adhered sheet by adhering a sheet member on a surface of a wooden sheet having a thickness of from 0.01 mm to 3 mm, and the sheet member being made of a material different from the wooden sheet, immersing the adhered sheet into one of a solution including 0.01-1 wt % of a penetrating agent and a solution including 0.01-1 wt % of penetrating agent and 0.01-20 wt % of a wetting agent, and molding the adhered sheet obtained by the immersing step so that the immersed adhered sheet has a predetermined shape of the electroacoustic transducer diaphragm.
Claims5
A production method for an electroacoustic transducer diaphragm, comprising:
- a producing step of producing an adhered sheet by adhering a sheet member on a surface of a wooden sheet having a thickness of from 0.01 mm to 3 mm, and the sheet member being made of a material different from the wooden sheet;
- an immersing step of immersing the adhered sheet into one of a solution including 0.01-1 wt % of a penetrating agent and a solution including 0.01-1 wt % of the penetrating agent and 0.01-20 wt % of a wetting agent;
- and
- a first hot press molding step of molding an adhered sheet obtained by the immersing step so that the immersed adhered sheet has a predetermined shape of the electroacoustic transducer diaphragm, wherein
- the penetrating agent is one of sodium butyl naphthalene sulfonate, sodium di(2-ethylhexyl) sulfosuccinate, sodium lauryl sulfate, and a combination thereof;
- the wetting agent is one of a of monovalent alcohol, dihydric alcohol, triatomic alcohol, ethylene glycol, butyl glycol, propyl glycol, sugars, mucopolysaccharides, sugar alcohols, water-soluble proteins and a combination thereof;
- and
- the solution contains 0.05-0.1 wt % of sodium di(2-ethylhexyl) sulfosuccinate.
A production method for an electroacoustic transducer diaphragm, comprising:
- a producing step of producing an adhered sheet by adhering a sheet member on a surface of a wooden sheet having a thickness of from 0.01 mm to 3 mm, and the sheet member being made of a material different from the wooden sheet;
- an immersing step of immersing the adhered sheet into one of a solution including 0.01-1 wt % of a penetrating agent and a solution including 0.01-1 wt % of the penetrating agent and 0.01-20 wt % of a wetting agent;
- and
- a first hot press molding step of molding an adhered sheet obtained by the immersing step so that the immersed adhered sheet has a predetermined shape of the electroacoustic transducer diaphragm, wherein
- the penetrating agent is one of sodium butyl naphthalene sulfonate, sodium di(2-ethylhexyl) sulfosuccinate, sodium lauryl sulfate, and a combination thereof;
- the wetting agent is one of a of monovalent alcohol, dihydric alcohol, triatomic alcohol, ethylene glycol, butyl glycol, propyl glycol, sugars, mucopolysaccharides, sugar alcohols, water-soluble proteins and a combination thereof;
- and
- the solution contains 0.02 wt % of sodium lauryl sulfate and 5 wt % of glucose.
Dependencies are inferred from the claim text.