# US 7,648,748 B2 · Liquid crystalline resin composition for blow molding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,648,748 B2
- Document ID: US7648748B2
- Status: Granted
- Kind: B2
- Application number: 11/580,091
- Filed: 2006-10-13
- Published: 2007-04-19
- Granted: 2010-01-19
- Earliest claimed: 2005-10-13
- Assignees: Polyplastics Co., Ltd.
- Inventors: Toshio Nakane; Mineo Ohtake; Toshio Shiwaku; Masato Suzuki
- Web page: https://patentgrep.com/patent/US7648748B2

## CPC

- C09K 19/3809: {Polyesters; Polyester derivatives, e.g. polyamides}
- C08L 67/00: Compositions of polyesters obtained by reactions forming a carboxylic ester link in the main chain (of polyester-amides C08L77/12; of polyester-imides C08L79/08); Compositions of derivatives of such polymers
- C08L 77/12: Polyester-amides
- C08L 25/08: Copolymers of styrene (C08L29/08, C08L35/06, C08L55/02 take precedence)
- C08L 33/14: of esters containing halogen, nitrogen, sulfur, or oxygen atoms in addition to the carboxy oxygen
- C08L 51/06: grafted on to homopolymers or copolymers of aliphatic hydrocarbons containing only one carbon-to-carbon double bond
- Y10T 428/13: Hollow or container type article [e.g., tube, vase, etc.]
- Y10T 428/1352: Polymer or resin containing [i.e., natural or synthetic]
- Y10T 428/1386: Natural or synthetic rubber or rubber-like compound containing
- Y10T 428/139: Open-ended, self-supporting conduit, cylinder, or tube-type article
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a liquid crystalline resin composition capable of readily blow-molding a molded article having uniform thickness, with the addition of good blow-moldability owing to the improved drawdown-resistant property, the improved melt-tension increase rate, and other properties without deteriorating the low gas-permeability which is a characteristic of liquid crystalline resin. Specifically, it provides a liquid crystalline resin composition for blow molding, obtainable by melt-kneading: (A) 100 parts by weight of a melt-processable aromatic polyester and/or polyester amide, which can form an anisotropic molten phase; (B) 10 to 25 parts by weight of a styrene-based copolymer composed of 40 to 97% by weight of a styrene group, 60 to 3% by weight of a specific glycidyl ester of α,β-unsaturated acid and 0 to 50% by weight of other vinyl-based monomer, wherein the styrene-based copolymer has epoxy equivalents ranging from 300 to 3000 g/eq, and weight average molecular weights of 30000 or more; and (C) 0 to 100 parts by weight of one or more of fibrous filler, powdery or granular filler, and plate-like filler.

## Claims

### Claim 1

A liquid crystalline resin composition for blow molding, said composition obtained by melt-kneading:
(A) 100 parts by weight of a melt-processable aromatic polyester and/or polyester amide, which can form an anisotropic molten phase;
(B) 10 to 25 parts by weight of a styrene-based copolymer comprising: 40 to 97% by weight of a styrene group; 60 to 3% by weight of a glycidyl ester of α,β-unsaturated acid, expressed by the following formula (1); and 0 to 50% by weight of other vinyl-based monomer, wherein the styrene-based copolymer has epoxy equivalents ranging from 300 to 3000 g/eq, and weight-average molecular weights of 30000 or more,
(wherein, —R′ is a hydrogen atom or an alkyl group; and
(C) 0 to 100 parts by weight of one or more of fibrous filler, powdery or granular filler, and plate-like filler.

### Claim 2 (depends on 1)

The liquid crystalline resin composition for blow molding according to claim 1, wherein the (A) melt-processable aromatic polyester and/or polyester amide which can form an anisotropic molten phase contains constitutional units expressed by the following formulae (2), (3), (4) and (5):
(wherein, —Ar1— is a divalent phenylene group and/or a divalent naphthalene group; —Ar2— is one or more selected from a divalent aromatic group and an aliphatic group containing 2 to 8 carbon atoms; —R— is one or more selected from a divalent aromatic group and an aliphatic group containing 2 to 8 carbon atoms; and —Ar3 is one or more selected from a divalent aromatic group and an aliphatic group containing 2 to 8 carbon atoms).

### Claim 3 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the —Ar1— group in the formula (2) in the (A) component is 1,4-phenylene group, 2,6-(or 2,7-)naphthalene group, or a combination thereof.

### Claim 4 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the —Ar2— group in the formula (3) and the —Ar3— group in the formula (5) in the (A) component are each one or more selected from 1,4-(or 1,3-)phenylene group and 2,6-(or 2,7-)naphthalene group; and the —R— in the formula (4) is one or more selected from 1,4-phenylene group, 4,4′-biphenyl group, 2,6-(or 2,7-)naphthalene group and ethylene group.

### Claim 5 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the (B) styrene-based copolymer is a copolymer containing, in addition to styrene and a glycidyl ester of α,β-unsaturated acid, at least one of acrylonitrile, acrylic acid ester, maleic anhydride and phenyl maleimide.

### Claim 6 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the melt viscosity of the resin composition is in a range from 15 to 400 Pa·s at a shear rate of 1000 sec−1 at a temperature (T1) higher by 20° C. than the melting point of the (A) component.

### Claim 7 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the melt tension of the resin composition is in a range from 50 to 200 mN at a drawing speed of 15 m/min at a temperature (T1) higher by 20° C. than the melting point of the (A) component.

### Claim 8 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the increase ratio in the melt tension (the melt tension increase rate) at double drawing speed to the melt tension of the resin composition at a drawing speed of 15 m/min at temperature T1 is 1.05 fold or more.

### Claim 9 (depends on 2)

A blow-molded article obtained by applying blow molding to the liquid crystalline resin composition according to claim 2.

### Claim 10 (depends on 2)

The liquid crystalline resin composition for blow molding according to claim 2, wherein the (B) styrene-based copolymer has epoxy equivalents ranging from 500 to 3000 g/eq.

### Claim 11 (depends on 10)

A blow-molded article obtained by applying blow molding to the liquid crystalline resin composition according to claim 10.

### Claim 12 (depends on 1)

The liquid crystalline resin composition for blow molding according to claim 1, wherein the (B) styrene-based copolymer is a copolymer containing, in addition to styrene and a glycidyl ester of α,β-unsaturated acid, at least one of acrylonitrile, acrylic acid ester, maleic anhydride and phenyl maleimide.

### Claim 13 (depends on 1)

The liquid crystalline resin composition for blow molding according to claim 1, wherein the melt viscosity of the resin composition is in a range from 15 to 400 Pa·s at a shear rate of 1000 sec−1 at a temperature (T1) higher by 20° C. than the melting point of the (A) component.

### Claim 14 (depends on 1)

The liquid crystalline resin composition for blow molding according to claim 1, wherein the melt tension of the resin composition is in a range from 50 to 200 mN at a drawing speed of 15 m/min at a temperature (T1) higher by 20° C. than the melting point of the (A) component.

### Claim 15 (depends on 1)

The liquid crystalline resin composition for blow molding according to claim 1, wherein the increase ratio in the melt tension (the melt tension increase rate) at double drawing speed to the melt tension of the resin composition at a drawing speed of 15 m/min at temperature T1 is 1.05 fold or more.

### Claim 16 (depends on 1)

A blow-molded article obtained by applying blow molding to the liquid crystalline resin composition according to claim 1.

### Claim 17 (depends on 1)

The liquid crystalline resin composition for blow molding according to claim 1, wherein the (B) styrene-based copolymer has epoxy equivalents ranging from 500 to 3000 g/eq.

### Claim 18 (depends on 17)

A blow-molded article obtained by applying blow molding to the liquid crystalline resin composition according to claim 17.