# US 7,553,701 B2 · Semiconductor packaging method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,553,701 B2
- Document ID: US7553701B2
- Status: Granted
- Kind: B2
- Application number: 12/195,991
- Filed: 2008-08-21
- Published: 2009-02-26
- Granted: 2009-06-30
- Earliest claimed: 2007-08-23
- Assignees: LS Mitron Ltd.
- Inventors: Joon-Mo Seo; Byoung-Un Kang; Jae-Hoon Kim; Soon-Young Hyun; Ji-Eun Kim; Jun-Woo Lee; Ju-Hyuk Kim
- Web page: https://patentgrep.com/patent/US7553701B2

## CPC

- H10W 70/417: {Bonding materials between chips and die pads}
- H10W 72/073: {of die-attach connectors}
- H10W 72/07338: {hardening the adhesive by curing, e.g. thermosetting}
- H10W 72/07341: {Controlling the bonding environment, e.g. atmosphere composition or temperature}
- H10W 72/07352: {changes in structures or sizes}
- H10W 72/075: {of bond wires}
- H10W 72/321: {Structures or relative sizes of die-attach connectors}
- H10W 72/354: {comprising polymers}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 90/756: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a semiconductor packaging method. The method comprises (S1) applying a die adhesive to an upper surface of a member through screen-printing; (S2) B-stage curing the member having the die adhesive; (S3) attaching a die on the B-stage cured die adhesive; (S4) wire-bonding the die to the member; and (S5) encapsulating the outside of the resultant, after the B-stage curing process of the step S2, a degree of cure of the die adhesive shows a decrease in heat capacity by 80 to 100%, and the step S3 is performed such that the die adhesive maintains an adhesive strength of 10 kgf/cm2 or more at normal temperature after the die attaching.

## Claims

### Claim 1

A semiconductor packaging method, comprising:
(S1) applying a die adhesive to an upper surface of a member through screen-printing;
(S2) B-stage curing the member having the die adhesive;
(S3) attaching a die on the B-stage cured die adhesive;
(S4) wire-bonding the die to the member; and
(S5) encapsulating the outside of the resultant,
wherein after the B-stage curing process of the step S2, a degree of cure of the die adhesive shows a decrease in heat capacity by 80 to 100%, and
wherein the step S3 is performed such that the die adhesive maintains an adhesive strength of 10 kgf/cm2 or more at normal temperature after the die attaching.

### Claim 2 (depends on 1)

The semiconductor packaging method according to claim 1,
wherein in the case that the die adhesive after the step S2 is left for 1 day or more under conditions of 85° C. temperature and 85% humidity, the die adhesive has a moisture absorption rate of 0.5% or less.

### Claim 3 (depends on 1, 2)

The semiconductor packaging method according to claim 1 or 2,
wherein the die attaching process of the step S3 is performed such that an attached area of the die to the die adhesive is 50 to 100% based on the entire area of the applied die adhesive.

### Claim 4 (depends on 1, 2)

The semiconductor packaging method according to claim 1 or 2,
wherein the die adhesive has a glass transition temperature (Tg) of 50 to 100° C.