# US 7,531,020 B2 · Heat sink made from diamond-copper composite material containing boron, and method of producing a heat sink

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,531,020 B2
- Document ID: US7531020B2
- Status: Granted
- Kind: B2
- Application number: 11/590,613
- Filed: 2006-10-30
- Published: 2007-02-22
- Granted: 2009-05-12
- Earliest claimed: 2004-04-29
- Assignees: Plansee SE; Ecole Polytechnique Federale de Lausanne
- Inventors: Ludger Weber
- Web page: https://patentgrep.com/patent/US7531020B2

## CPC

- H10W 40/254: {Diamond}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A heat sink that is particularly suitable for semiconductor components is made from a diamond-containing composite material. In addition to a diamond fraction amounting to 40-90% by volume, the composite material also contains 7 to 59% by volume copper or a copper-rich phase (with Cu>80 at. %) and 0.01 to 20% by volume boron or a boron-rich phase (with B>50 at. %). The bonding of copper to the diamond grains can be considerably improved by the addition of boron, with the result that a high thermal conductivity can be achieved. The heat sink component is preferably produced with an unpressurized and pressure-assisted infiltration technique.

## Claims

### Claim 1

A heat sink component formed of a composite material, the composite material comprising:
40 to 90% by volume diamond grains;
7 to 59% by volume copper or a copper-rich solid solution with Cu>80 at. %; and
0.01 to 20% by volume boron or a boron-rich phase with B>50 at. %.

### Claim 2 (depends on 1)

The component according to claim 1, wherein the copper-rich solid solution contains 0.005 to 0.3 at. % boron.

### Claim 3 (depends on 1)

The component according to claim 1, wherein the composite material contains 0.001 to 5% by volume of a boron-carbon compound.

### Claim 4 (depends on 3)

The component according to claim 3, wherein said boron-carbon compound is formed predominantly or exclusively by reacting boron with carbon of said diamond grains.

### Claim 5 (depends on 3)

The component according to claim 3, wherein said boron-carbon compound is disposed as a layer covering at least 60% of a surface of said diamond grains.

### Claim 6 (depends on 5)

The component according to claim 5, wherein a thickness of said boron-carbon layer is 1 to 50 nm.

### Claim 7 (depends on 1)

The component according to claim 1, wherein said copper solid solution contains 0.01 to 5 at. % silver.

### Claim 8 (depends on 1)

The component according to claim 1, which further comprises 0.01 to 10% by volume of a silver-rich phase.

### Claim 9 (depends on 1)

The component according to claim 1, which comprises 0.01 to 5% by volume of unbonded, amorphous carbon.

### Claim 10 (depends on 1)

The component according to claim 1, wherein a mean diamond grain size of said diamond grains is 50 to 300 μm.

### Claim 11 (depends on 10)

The component according to claim 10, wherein the mean diamond grain size is 100 to 200 μm.

### Claim 12 (depends on 1)

The component according to claim 1, wherein said diamond grains have a defined grain size with a bimodal distribution, including a first distribution maximum at 20-40 μm and a second distribution maximum at 130-250 μm.

### Claim 13 (depends on 1)

The component according to claim 1, which comprises 0.005 to 1% by volume of a boron-carbon compound.

### Claim 14 (depends on 1)

The component according to claim 1, which comprises 15 to 40% by volume copper or a copper-rich solid solution with Cu>90 at. %.

### Claim 15 (depends on 1)

The component according to claim 1, which comprises 0.2 to 10% by volume boron or a boron-rich phase with B>90 at. %.

### Claim 16 (depends on 1)

A heat sink component formed of the material according to claim 1 and having a metallic coating applied thereto, said metallic coating comprising a material selected from the group consisting of Ni, Cu, Au, Ag, and an alloy thereof.

### Claim 17 (depends on 1)

A heat sink component formed of the material according to claim 1 and having a ceramic frame soldered thereonto.

### Claim 18

A method of producing a heat sink component, the method which comprises:
providing an intermediate material containing diamond grains with a mean grain size of 50 to 300 μm and an optional component of a Cu—B alloy and/or a binder;
shaping the intermediate material in an unpressurized or pressure-assisted shaping process, wherein a diamond fraction, based on a total volume of the intermediate material, amounts to 40 to 90% following the shaping step;
heating, with an unpressurized or pressure-assisted heating process, the intermediate material and an infiltrate alloy containing Cu and B to a temperature above a liquidus temperature of the infiltrate alloy but below 1100° C., and causing the infiltrate alloy to infiltrate the intermediate material, and filling at least 97% of pore spaces in the intermediate material.

### Claim 19 (depends on 18)

The method according to claim 18, which comprises providing a eutectic or near-eutectic Cu—B alloy for the infiltration, wherein near-eutectic alloys comprise alloys with a liquidus temperature of <1050° C.

### Claim 20

A method of producing a heat sink component, the method which comprises:
providing an intermediate material with diamond grains and an infiltrate alloy containing Cu and B, and mixing or milling the intermediate material;
filling a die of a hot press with the intermediate material, heating to a temperature T, where 500° C.<T<1100° C., and hot-pressing the intermediate material.

### Claim 21 (depends on 20)

The method according to claim 20, which comprises providing a eutectic or near-eutectic Cu—B alloy for the infiltration, wherein near-eutectic alloys comprise alloys with a liquidus temperature of <1050° C.

### Claim 22 (depends on 1)

The heat sink component according to claim 1 configured as a heat sink for one or more semiconductor components.