# US 7,528,199 B2 · Conjugated-diolefin (co)polymer rubber and process for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,528,199 B2
- Document ID: US7528199B2
- Status: Granted
- Kind: B2
- Application number: 10/567,905
- Filed: 2005-03-14
- Published: 2007-04-19
- Granted: 2009-05-05
- Earliest claimed: 2004-03-15
- Assignees: Jsr Corporation
- Inventors: Kouta Taniguchi; Keisuke Tsukimawashi; Naokazu Kobayashi; Toshihiro Tadaki
- Web page: https://patentgrep.com/patent/US7528199B2

## CPC

- C08C 2/06: Winning of rubber from solutions
- C08C 19/25: Incorporating silicon atoms into the molecule
- C08C 19/44: of polymers containing metal atoms exclusively at one or both ends of the skeleton
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS

## Abstract

A method for producing an alkoxysilyl group-containing conjugated diolefin (co)polymer rubber by polymerizing a conjugated diolefin or a conjugated diolefin and an aromatic vinyl compound in a hydrocarbon solvent by anionic polymerization using as an initiator at least one metal compound selected from an organic alkali metal compound and an organic alkali earth metal compound, and then allowing an alkoxysilane-based compound to react, wherein after the alkoxysilane-based compound has been allowed to react, an alkaline compound is added at the time of desolvation, and treatment is conducted at a pH of 8 to 12.

## Claims

### Claim 1

A method for producing an alkoxysilyl group containing conjugated diolefin (co)polymer rubber from a conjugated diolefin or a conjugated diolefin and an aromatic vinyl compound, wherein said (co)polymer rubber has an alkoxysilyl group and has been desolvated under alkaline conditions, comprising polymerizing a conjugated diolefin or a conjugated diolefin and an aromatic vinyl compound in a hydrocarbon solvent by anionic polymerization using as an initiator at least one metal compound selected from the group consisting of an organic alkali metal compound and an organic alkali earth metal compound, and then allowing an alkoxysilane-based compound to react, wherein after said alkoxysilane-based compound has been allowed to react, an alkaline compound is added at the time of desolvation, and treatment is conducted at a pH of 8 to 12.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the (co)polymer rubber further comprises an amino group.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the amino group is a primary amino group.

### Claim 4 (depends on 2)

The method according to claim 2, wherein an amino group-containing alkoxysilane-based compound is used as a compound for allowing the amino group and the alkoxysilyl group to be bonded to a (co)polymer chain.

### Claim 5 (depends on 3)

The method according to claim 3, wherein an amino group-containing alkoxysilane-based compound is used as a compound for allowing the amino group and the alkoxysilyl group to be bonded to a (co)polymer chain.

### Claim 6 (depends on 1)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 1, wherein the alkaline compound is at least one selected from the group consisting of ammonia, sodium hydroxide, potassium hydroxide and lithium hydroxide.

### Claim 7 (depends on 1)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 1, wherein the hydrocarbon solvent is selected from the group consisting of pentane, hexane, heptane, octane, methylcyclopentane, cyclohexane, benzene, toluene, and xylene and is present in such an amount as to give a total monomer concentration of 5 to 30% by weight.

### Claim 8 (depends on 1)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 1, wherein the conjugated diolefin is selected from the group consisting of 1,3-butadiene, isoprene, 2,3-dimethyl-1,3-butadiene, 2-chloro-1,3-butadiene, 1,3-pentadiene, and mixtures thereof.

### Claim 9 (depends on 8)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 8, comprising polymerizing a conjugated diolefin and an aromatic vinyl compound wherein the aromatic vinyl compound is selected from the group consisting of styrene, 2-methylstyrene, 3-methylstyrene, 4-methylstyrene, .alpha.-methylstyrene, 2,4-dimethylstyrene, 2,4-diisopropylstyrene, 4-tert-butylstyrene, divinylbenzene, tert-butoxystyrene, vinylbenzyldimethylamine, (4-vinyl-benzyl)dimethylaminoethyl ether, N,N-dimethylaminoethyl-styrene, 2-t-butylstyrene, 3-t-butylstyrene, 4-t-butyl-styrene, vinylpyridine, and mixtures thereof.

### Claim 10 (depends on 1)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 1, wherein the organic alkali metals and organic alkali earth metals are selected from the group consisting of n-butyllithium, sec-butyllithium and t-butyllithium, 1,4-dilithiobutane, phenyllithium, stilbenelithium, lithiumnaphthalene, sodiumnaphthalene, potassiumnaphthalene, n-butylmagnesium, n-hexylmagnesium, ethoxycalcium, calcium stearate, t-butoxystrontium, ethoxybarium, isopropoxybarium, ethylmercaptobarium, t-butoxybarium, phenoxybarium, di-ethylaminobarium and barium stearate.

### Claim 11 (depends on 1)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 1, wherein the alkoxysilane-based compound is selected from the group consisting of tetramethoxysilane, tetraethoxysilane, tetrapropoxysilane, tetrabutoxysilane, tetraphenoxysilane, tetratoluyloxysilane, methyltrimethoxysilane, methyltriethoxysilane, methyltripropoxysilane, methyltributoxysilane, methyltriphenoxysilane, ethyltrimethoxysilane, ethyltriethoxysilane, ethyltripropoxysilane, ethyltributoxysilane, ethyltriphenoxysilane, dimethyldimethoxysilane, dimethyldiethoxysilane, dimethyldipropoxysilane, dimethyldibutoxysilane, dimethyldiphenoxysilane, diethyldimethoxysilane, diethyldiethoxysilane, diethyldipropoxysilane, diethyldibutoxysilane, diethyldiphenoxysilane, vinyltrimethoxysilane, vinyltriethoxysilane, vinyltripropoxysilane, vinyltri-butoxysilane, vinyltriphenoxysilane, allyltriphenoxysilane, octenyltrimethoxysilane, phenyltrimethoxysilane, phenyltriethoxysilane, phenyltripropoxysilane, phenyltributoxysilane, phenyltriphenoxysilane, trimethoxychlorosilane, triethoxychlorosilane, tripropoxychlorosilane, tributoxychlorosilane, triphenoxychlorosilane, dimethoxydichlorosilane, dipropoxydichlorosilane and diphenoxydichlorosilane.

### Claim 12 (depends on 4)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 4, wherein the amino group-containing alkoxysilane-based compound is selected from the group consisting of N,N-bis (trimethylsilyl)amino-propylmethyldimethoxysilane, N,N-bis(trimethylsilyl)amino-propylmethyldiethoxysilane, N,N-bis(trimethylsilyl)amino-propyltrimethoxysilane, N,N-bis(trimethylsilyl)aminopropyltriethoxysilane, N,N-bis(trimethylsilyl)aminoethyltrimethoxysilane, N,N-bis(trimethylsilyl)aminoethyltriethoxysilane, N,N-bis(trimethylsilyl)aminoethylmethyldimethoxysilane, N,N-bis(trimethylsilyl)aminoethylmethyldiethoxysilane, 1-trimethylsilyl-2,2-dimethoxy-1-aza-2-sila-cyclopentane, N,N-diethyl-3-aminopropyltrimethoxysilane, N,N-diethyl-3-aminopropyltriethoxysilane, 2-(triethoxy-silylethyl)pyridine, and γ-isocyanatepropyltriethoxysilane.

### Claim 13 (depends on 1)

A method for producing the alkoxysilyl group-containing conjugated diolefin (co)polymer rubber according to claim 1, wherein the weight average molecular weight of the (co)polymer rubber is 150,000 to 1,700,000 and the Mooney viscosity of the (co)polymer rubber is 20 to 200.