# US 7,501,293 B2 · Semiconductor device in which zinc oxide is used as a semiconductor material and method for manufacturing the semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,501,293 B2
- Document ID: US7501293B2
- Status: Granted
- Kind: B2
- Application number: 10/518,945
- Filed: 2003-06-04
- Published: 2006-03-16
- Granted: 2009-03-10
- Earliest claimed: 2002-06-13
- Assignees: Murata Manufacturing Co., Ltd.
- Inventors: Yoshihiro Ito; Michio Kadota
- Web page: https://patentgrep.com/patent/US7501293B2

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H01S 5/327: in AIIBVI compounds, e.g. ZnCdSe-laser
- H10H 20/823: comprising only Group II-VI materials, e.g. ZnO
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/2914: {Oxides}
- H10P 14/3226: {Oxides}
- H10P 14/3234: {being oxide semiconducting materials (Group IIB-VIA semiconductors H10P14/3224)}
- H10P 14/3252: {Alternating layers, e.g. superlattice}
- H10P 14/3426: {Oxides}
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10P 14/3446: {Transition metal elements; Rare earth elements}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device having excellent crystallinity and excellent electric characteristics includes a ZnO thin film having excellent surface smoothness. ZnO-based thin films (an n-type contact layer, an n-type clad layer, an active layer, a p-type clad layer, and a p-type contact layer) primarily including ZnO are formed sequentially by an ECR sputtering method or other suitable method on a zinc-polar surface of a ZnO substrate. A transparent electrode and a p-side electrode are formed by an evaporation method or other suitable method on a surface of the p-type contact layer, and an n-side electrode is formed on an oxygen-polar surface of the ZnO substrate.

## Claims

### Claim 1

A semiconductor device comprising:
a single crystal substrate primarily including zinc oxide and having a zinc-polar surface and an oxygen-polar surface; and
at least one layer of thin film primarily including zinc oxide disposed on the zinc-polar surface; wherein
the at least one layer of thin film includes a multilayer film and the multilayer film defines a light-emitting layer;
the multilayer film includes an n-type contact layer, an n-type clad layer, an active layer, a p-type clad layer and a p-type contact layer; and
the n-type contact layer is a zinc oxide layer that is in contact with the zinc-polar surface of the single crystal substrate.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein the at least one layer of thin film has zinc-polarity.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, further comprising a transparent electrode disposed on the multilayer film.

### Claim 4 (depends on 3)

The semiconductor device according to claim 3, wherein the transparent electrode is made of Indium Tin Oxide.

### Claim 5

A method for manufacturing a semiconductor device, comprising the steps of:
determining whether a surface of a single crystal substrate primarily including zinc oxide is a zinc-polar surface or an oxygen-polar surface; and
forming at least one layer of thin film primarily including zinc oxide on the zinc-polar surface; wherein
the at least one layer of thin film includes a multilayer film and the multilayer film defines a light-emitting layer;
the multilayer film includes an n-type contact layer, an n-type clad layer, an active layer, a p-type clad layer and a p-type contact layer; and
the n-type contact layer is a zinc oxide layer that is in contact with the zinc-polar surface of the single crystal substrate.

### Claim 6 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the thin film has zinc-polarity.

### Claim 7 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, further comprising the steps of:
providing a sputtering apparatus provided with a plasma generation chamber and a separate film formation chamber; and
performing sputtering treatment using the sputtering apparatus so as to form the thin film.

### Claim 8 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the sputtering treatment is performed by a method selected from the group consisting of an electron cyclotron resonance plasma sputtering method, an inductively coupled plasma sputtering method, a helicon wave excited plasma sputtering method, an ion beam sputtering method, and a cluster beam sputtering method.

### Claim 9 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the thin film is formed by a method selected from the group consisting of a molecular-beam epitaxy method, a metal organic chemical vapor deposition method, a laser molecular-beam epitaxy method, and a laser abrasion method.