The present invention attempts to provide a hard coating which has excellent hardness and lubricity. Such attempt has been completed by providing a hard coating comprising (Al1-aVa) (C1-XNX) wherein 0.27≦a≦0.75, and 0.3≦X≦1, wherein a and X independently represent an atomic ratio.
Claims20
A hard coating consisting of
- (Al1-aVa)(C1-XNX), wherein
- 0.35≦a≦0.75;
- 0.3≦X≦1;
- a and X independently represent an atomic ratio;
- and
- the hard coating comprises a NaCl-type crystal structure.
3 more elements
A hard coating consisting of
- (Al1-a-b-cVaSibBc)(C1-XNX), wherein
- 0.35≦a≦0.75;
- 0<b+c≦0.20;
- 0.3≦X≦1;
- a, b, c, and X independently represent an atomic ratio with the proviso that b and c are not simultaneously 0 while one of b and c may be 0;
- and
- the hard coating comprises a NaCl-type crystal structure.
4 more elements
A hard coating consisting of
- (Al1-a-b-c-d-eVaSibBcModWe)(C1-XNX), wherein
- 0.2≦a≦0.75;
- 0<b+c≦0.20;
- 0<d+e≦0.30;
- 0.3≦X≦1;
- a, b, c, d, e, and X independently represent an atomic ratio with the proviso that b and c are not simultaneously 0 while one of b and c may be 0, and d and e are not simultaneously 0 while one of d and e may be 0;
- and
- the hard coating comprises a crystal structure including at least one of a cubic structure and a hexagonal structure.
5 more elements
A hard coating consisting of
- (Al1-a-f-gVaHffZrg)(C1-XNX), wherein
- 0.35≦a≦0.75;
- 0<f+g≦0.5;
- and
- 0.3≦X≦1;
- a, f, g and X independently represent an atomic ratio with the proviso that f and g are not simultaneously 0 while one of f and g may be 0;
- and
- the hard coating comprises a crystal structure including at least one of a cubic structure and a hexagonal structure.
5 more elements
A hard coating consisting of
- (Al1-a-b-c-f-gVaSibBcHffZrg)(C1-XNX), wherein
- 0.01≦a≦0.75;
- 0<b+c≦0.20;
- 0<f+g≦0.5;
- 0.3≦X≦1;
- a, b, c, f, g, and X independently represent an atomic ratio with the proviso that b and c are not simultaneously 0 while one of b and c may be 0, and f and g are not simultaneously 0 while one of f and g may be 0;
- and
- the hard coating comprises a crystal structure including at least one of a cubic structure and a hexagonal structure.
5 more elements
A hard coating deposited by arc ion plating in a gas containing 30 to 100% by atom of N in relation to the sum of N and C by using
- a target comprising (Al1-aVa), wherein 0.35≦a≦0.75 and a represents an atomic ratio, or
- a target comprising (Al1-a-b-cVaSibBc), wherein 0.1≦a≦0.75;
- 0<b+c≦0.20;
- and
- a, b, and c independently represent an atomic ratio with the proviso that b and c are not simultaneously 0 while one of b and c may be 0;
- wherein
- the hard coating comprises a NaCl-type crystal structure.