Process for recycling waste acid
AssigneeVeolia ES Technical Solutions L.L.C.
InventorDanny Mislenkov
Life of this patent
Estimating the term…
Abstract
A recycling process is presented to treat spent waste acid solutions whereby useful products are produced. Spent waste acid containing inorganic and organic contaminants is mixed with a magnesium compound containing aluminum and iron compounds that form oxyhydroxide flocs that complex, react, sequester and/or co-precipate the contaminates from the admixture. The magnesium reacts with sulfate ions to form a high quality magnesium sulfate solution.
Claims13
A method of treating a spent acid solution contaminated with inorganic and organic impurities comprising, in combination,
- a) providing a spent waste acid containing compounds selected from the group consisting of sulfuric acid, copper sulfate, iron sulfate, acetic acid, phosphoric acid, methyl sulfonic acid and combinations thereof, and also containing contaminants selected from the group consisting of arsenic, antimony, chromium, germanium, gallium, copper, at least one organic compound, and mixtures thereof;
- b) forming an admixture initially having a pH of less than 5 by contacting the spent waste acid with a Mg compound containing aluminum and iron;
- c) measuring and monitoring the pH of the admixture;
- d) agitating and maintaining the admixture at a temperature in the range from about ambient to about 97° C.;
- e) complexing the contaminants contained in the spent waste acid through flocculation by forming flocs selected from the group consisting of iron oxyhydroxide, aluminum oxyhydroxide, copper oxyhydroxide and mixtures thereof;
- f) increasing the pH of the admixture by continued addition of the Mg compound to the admixture until a pH of 5 or higher is obtained;
- and
- g) isolating a solution containing magnesium sulfate by separating the flocs containing the contaminants from the admixture using a filtration process.
A method of treating a spent acid solution contaminated with inorganic and organic contaminants comprising, in combination,
- a) providing a spent waste acid containing compounds selected from the group consisting of sulfuric acid, acetic acid, phosphoric acid, methyl sulfonic acid and combinations thereof, and also containing contaminants selected from the group consisting of calcium, iron, arsenic, antimony, copper, chromium, germanium, gallium, at least one organic compound and mixtures thereof;
- b) forming an admixture initially having a pH of less than 5 by contacting the spent waste acid with a Mg compound and compounds containing aluminum and iron;
- c) measuring and monitoring the pH of the admixture;
- d) agitating and maintaining the admixture at a temperature in the range from about ambient to about 97° C.;
- e) complexing the contaminants contained in the spent waste acid through flocculation by forming flocs selected from the group consisting of iron oxyhydroxide, aluminum oxyhydroxide, copper oxyhydroxide and mixtures thereof;
- f) increasing the pH of the admixture by continued addition of the Mg compound to the admixture until a pH of 5 or higher is obtained;
- g) isolating a solution containing magnesium sulfate by separating the flocs containing the contaminants from the admixture using a filtration process;
- and
- h) forming a filter cake in the filtration process comprising the flocs and drying the filter cake to form a solid product containing metal oxides suitable for recycling in a smelting process.
A method of treating a spent acid solution contaminated with inorganic and organic contaminants comprising, in combination,
- a) providing a spent waste acid containing compounds selected from the group consisting of sulfuric acid, acetic acid, phosphoric acid, methyl sulfonic acid and combinations thereof, and also containing contaminants selected from the group consisting of calcium, iron, arsenic, antimony, copper, chromium, germanium, gallium, at least one organic compound and mixtures thereof;
- b) forming an admixture initially having a pH of less than 5 by contacting the waste stream with a Mg compound containing iron and aluminum;
- c) measuring and monitoring the pH of the admixture;
- d) agitating the admixture and maintaining the admixture at a temperature in the range from about ambient to about 97° C.;
- e) adding the Mg compound until the pH of the admixture is greater than 2;
- f) forming iron oxyhydroxide flocs;
- g) complexing the spent waste acid contaminants using the iron oxyhydroxide flocs while maintaining the pH of the admixture greater than 2;
- h) increasing the pH of the admixture to above 3.5;
- i) forming aluminum oxyhydroxide flocs;
- j) complexing the spent waste acid contaminants with the aluminum oxyhydroxide flocs;
- k) increasing the pH of the admixture by continued addition of the Mg compound to the admixture until a pH of 5 or higher is obtained;
- l) analyzing the admixture to determine copper content;
- m) measuring the specific gravity of the admixture;
- and
- n) filtering the admixture to remove the complexed contaminants and flocs to form a magnesium sulfate solution.