# US 7,462,444 B2 · Image forming method for the photothermographic material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,462,444 B2
- Document ID: US7462444B2
- Status: Granted
- Kind: B2
- Application number: 11/267,199
- Filed: 2005-11-07
- Published: 2006-05-25
- Granted: 2008-12-09
- Earliest claimed: 2002-10-18
- Assignees: FUJIFILM Corporation
- Inventors: Yutaka Oka; Tomoyuki Ohzeki
- Web page: https://patentgrep.com/patent/US7462444B2

## CPC

- G03C 1/49881: {characterised by the process or the apparatus}
- G03C 1/49818: {Silver halides}
- G03C 1/08: Sensitivity-increasing substances
- G03C 1/49827: {Reducing agents}
- G03C 1/49845: {Active additives, e.g. toners, stabilisers, sensitisers}
- G03C 1/49863: {Inert additives, e.g. surfactants, binders}
- G03C 5/02: Sensitometric processes, e.g. determining sensitivity, colour sensitivity, gradation, graininess, density; Making sensitometric wedges
- G03C 7/3041: {Materials with specific sensitometric characteristics, e.g. gamma, density}
- G03C 7/30541: {characterised by the released group}
- G03C 2001/03558: {Iodide content}
- G03C 2001/03564: {Mixed grains or mixture of emulsions}
- G03C 2200/36: Latex
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

An image forming method comprising: imagewise exposing and thermal developing a photothermographic material using an image recording apparatus, wherein a part of the sheet is exposed and, in parallel with the exposure, development is started on a part of the sheet having been already exposed: wherein the photothermographic material comprises a reducing agent represented by formula (R), and wherein the photosensitive silver halide contains at least two preformed photosensitive silver halides having respective sensitivities different from each other for a light with the same exposure wavelength and a silver iodide content of the photosensitive silver halide is 40% by mole or more.

## Claims

### Claim 1

An image forming method comprising: imagewise exposing and thermal developing a sheet of photothermographic material using an image recording apparatus,
wherein the image recording apparatus has at least the following portions (A) to (D):
(A) a laser irradiation portion that scans the photothermographic material with a laser beam based on image data to expose the photothermographic material;
(B) a transport portion that transports the photothermographic material in the laser irradiation portion;
(C) a thermal developing portion, disposed on the side downstream from the transport portion, and in which a part of one sheet of the photothermographic material is imagewise exposed by the laser irradiation portion and simultaneously a part of the sheet having been already imagewise exposed is developed by heating; and
(D) a guide portion, provided between the transport portion and the thermal developing portion, and allowing a flexion of the photothermographic material generated by a difference between a transport speed in the transport portion and a transport speed in the thermal developing portion:
wherein the photothermographic material comprises at least a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent represented by following formula (R) and a binder on at least one surface of a support;
wherein R11 and R11′ each independently represents an alkyl group having 1 to 20 carbon atoms, R12 and R12′ each independently represents a hydrogen atom or a group capable of substituting for a hydrogen atom on a benzene ring, L represents a —S— group or a —CHR13 — group, R13 represents a hydrogen atom or an alkyl group having 1 to 20 carbon atoms, and X and X1 each independently represents a hydrogen atom or a group capable of substituting for a hydrogen atom on a benzene ring; and
wherein the photosensitive silver halide contains at least two preformed photosensitive silver halides having respective sensitivities different from each other for a light with the same exposure wavelength and a silver iodide content of the photosensitive silver halide is 40% by mole or more.

### Claim 2 (depends on 1)

The image forming method according to claim 1, wherein the thermal development is started on the sheet within 60 sec after the imagewise exposure.

### Claim 3 (depends on 1)

The image forming method according to claim 1, wherein the thermal development is started on the sheet within 15 sec after the imagewise exposure.

### Claim 4 (depends on 1)

The image forming method according to claim 1, wherein V1 is a transport speed in the transport portion and V2 is a transport speed in the thermal developing portion, and V1 and V2 satisfy the following relationship: 0.7<V2/V1 ≦1.0.

### Claim 5 (depends on 1)

The image forming method according to claim 1, wherein a difference in sensitivity between the at least two preformed photosensitive silver halides is 0.3 to 1.0 in terms of log E.

### Claim 6 (depends on 1)

The image forming method according to claim 1, wherein the maximum density of a photographic characteristic curve obtained by imagewise exposure and thermal development of the photothermographic material is 3.0 or more, and a y value at a density of 0.5 is 0.8 to 1.8 and a γ value at a density of 1.0 is 2.2 to 3.8.

### Claim 7 (depends on 1)

The image forming method according to claim 1, wherein the at least two preformed photosensitive silver halides have respective average grain sizes, which are different from each other.

### Claim 8 (depends on 7)

The image forming method according to claim 7, wherein the average grain sizes of the preformed photosensitivesilver halides are 5 nm to 100 nm.

### Claim 9 (depends on 7)

The image forming method according to claim 7, wherein a difference in average grain size between the at least two preformed photosensitive silver halides is 20 nm to 95 nm.

### Claim 10 (depends on 1)

The image forming method according to claim 1, wherein the photothermographic material further comprises a compound that can be one-electron-oxidized to provide a one-electron oxidation product, which releases one or more electrons.

### Claim 11 (depends on 1)

The image forming method according to claim 1, wherein at least one of the preformed photosensitive silver halide is chemically sensitized.

### Claim 12 (depends on 1)

The image forming method according to claim 1, wherein the photothermographic material further comprises a compound expressed by the following formula (PO):
Q—(Y)n—C(Z1)(Z2)X formula (PO)
wherein Q represents a heterocyclic group, Y represents a divalent linkage group, n represents 0 or 1, Z1 and Z2 each independently represents a halogen atom, and X represents a hydrogen atom or an electron-withdrawing group.

### Claim 13 (depends on 1)

The image forming method according to claim 1, wherein the binder is a polymer latex.

### Claim 14 (depends on 1)

The image forming method according to claim 1, wherein the photothermographic material further comprises a developing accelerator.

### Claim 15 (depends on 1)

The image forming method according to claim 1, wherein the photothermographic material further comprises a hydrogen bonding compound.