Polyimide copolymer and metal laminate using the same
AssigneeNippon Mektron, Ltd.
InventorsMin Zuo, Jenq-Tain Lin
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Mektron, Ltd.
InventorsMin Zuo, Jenq-Tain Lin
Estimating the term…
A novel polyimide copolymer, which is a copolymer comprising two kinds of tetracarboxylic acid dianhydrides consisting of (A) isopropylidene-bis(4-phenyleneoxy-4-phthalic acid) dianhydride and (B) 3,3′,4,4′-biphenyltetracarboxylic acid dianhydride, and one kind of a diamine consisting of (C) 6-amino-2-(p-aminophenyl)benzimidazole, or two or three kinds of diamines consisting of component (C) and (D) at least one kind of diamines consisting of bis(4-amino-phenyl)ether (D1) and phenylenediamine (D2), and a metal laminate manufactured by laminating said polyimide copolymer to a metallic foil. The metal laminate comprising the novel polyimide copolymer as a layer on the metallic foil has a low curling susceptibility to cause curling, twisting, warping, etc. against temperature changes due to a low coefficient of linear thermal expansion of the polyimide copolymer, and also has satisfactory adhesiveness and thermal dimensional stability and a low water absorbability, and thus can be used as a suitable for a flexible, finely printed circuit board requiring a high dimensional stability.
A metal laminate manufactured by laminating a single layer of a polyimide copolymer to a metallic foil which metal laminate is subjected to an etching process to remove a portion of the metallic foil said etching process being conducted after the single layer of the polyimide copolymer is laminated to the metallic foil, said polyimide copolymer comprising two kinds of tetracarboxylic acid dianhydrides consisting of (A) isopropylidenebis (4- phenyleneoxy-4-phthalic acid) dianhydride and (B) 3,3′,4,4′-biphenyltetracarboxylic acid dianbydride, and two or three kinds of diamines consisting of (C) 6-amino-2-(p-aminophenyl) benzimidazole and (D) at least one kind of diamines consisting of bis(4-amninophenyl) ether (D1) and phenylenedianhifle (D2) and said polyimide copolymer being resistant to curling resulting from the metal laminate etching process so that the resulting etched metal laminate is substantially curl-free.
Dependencies are inferred from the claim text.