Back to results
US 7,446,139 B2Granted
Modified asphalt binder material using crumb rubber and methods of manufacturing a modified asphalt binder
AssigneeInnophos, Inc.
InventorJean-Valery Martin
Life of this patent
Estimating the term…
Abstract
In a first aspect, bituminous asphalt binder materials which are modified by the addition of crumb rubber or ground tire rubber are described. In a second aspect, the present invention is directed to methods of producing a modified asphalt binder containing crumb rubber or ground tire rubber. The modified asphalt binders comprise neat asphalt, crumb rubber, one or more synthetic polymers, and one or more acids. The crumb rubber may be obtained from recycled truck and/or automobile tires.
Claims11
A method for making a modified asphalt binder composition, comprising the steps of:
- a. providing neat asphalt in an appropriate vessel;
- b. heating the neat asphalt to a temperature of between about 120° C. and about 200° C.;
- c. adding to the neat asphalt a first modifying ingredient selected from the group consisting of at least one acid, at least one synthetic polymer and crumb rubber;
- d. mixing the asphalt and the first modifying ingredient with one of a high shear mixer or a low shear mixer for a period of between about 5 minutes and about 10 hours
- e. adding to the modified asphalt binder a second modifying ingredient selected from the group consisting of at least one acid, at least one synthetic polymer and crumb rubber, wherein the second modifying ingredient is a different type of ingredient than the first modifying ingredient;
- f. mixing the second modifying ingredient and the modified asphalt binder in one of a high shear mixer or a low shear mixer for a period of between about 5 minutes and about 10 hours
- g. adding to the modified asphalt binder a third modifying ingredient selected from the group consisting of at least one acid, at least one synthetic polymer and crumb rubber, wherein the third modifying ingredient is a different type of ingredient than the first modifying ingredient and the second modifying ingredient;
- and
- h. agitating the third modifying ingredient and the modified binder material in one of a low shear mixer or a high shear mixer for a period of between about 5 minutes and about 48 hours.
6 more elements
Dependencies are inferred from the claim text.