Propylene polymer resin with improved properties
AssigneeBorealis Technology Oy
InventorsPirjo Jääskeläinen, Marijke Verpoest, Bert Broeders, Helge Grande
Life of this patent
Estimating the term…
Loading patent…
AssigneeBorealis Technology Oy
InventorsPirjo Jääskeläinen, Marijke Verpoest, Bert Broeders, Helge Grande
Estimating the term…
The present invention relates to a process for the production of a propylene polymer in a multistage polymerization process comprising the polymerisation of propylene in the presence of a catalyst in a first reaction zone comprising at least one slurry reactor to give a first polymerisation product, transferring said first product to a second reaction zone comprising at least one gas phase reactor and continuing polymerisation of propylene in the gas phase in the presence of said first polymerisation product which is characterised in that the temperature in both the slurry and the gas phase reactor is at least 75° C. and the product of at least one reactor is having an ethylene content in the range of 0.05 to 0.5 wt %. Furthermore, the invention relates to a propylene polymer obtainable by the inventive process, to a propylene polymer which is characterised in that it comprises ethylene comonomer in an amount of 0.05 to 0.5 wt. %, is having a xylene solubles contents of 3.0 wt. % or less and is having a maximum in its temperature rising elution fractionation (TREF)-function at 120° C. or less, and to articles such as fibres, non-wovens, films and sheets comprising the inventive polymer.
A process for the production of a propylene polymer in a multistage polymerisation process comprising the polymerisation of propylene in the presence of a catalyst in a first reaction zone comprising at least one slurry reactor to give a first polymerisation product, transferring said first product to a second reaction zone comprising at least one gas phase reactor and continuing polymerisation of propylene in the gas phase in the presence of said first polymerisation product characterised in that the temperature in both the slurry and the gas phase reactor is at least 75° C. and the product of at least one reactor has an ethylene content in the range of 0.05 to 0.5 wt % and the polypropylene polymer has a xylene solubles content of 3.0 wt. % or less and a maximum in its temperature rising elution fractionation (TREF)-function at 120° C. or less.
Dependencies are inferred from the claim text.