Pyrogenically prepared, surface modified aluminum oxide
AssigneeDegussa AG
InventorsJuergen Meyer, Manfred Ettlinger
Life of this patent
Estimating the term…
Abstract
Pyrogenically prepared, surface modified aluminum oxide, having the following physical chemical properties: Surface area [m2/g] 50 to 150 Tamped density [g/L] 25 to 130 Drying loss [%] less than 5 Loss on ignition [%] 0.1 to 15 C content [%] 0.1 to 15 pH value 3 to 9 is prepared by treating pyrogenically prepared aluminum oxide with a surface modifying agent.
Claims6
A product consisting of a pyrogenically prepared, surface modified aluminum oxide modified by a surface modifying agent selected from the group consisting of octyltrimethoxysilane and octyltriethoxysilane, and having the following physical chemical properties:
- Surface area [m2/g]
- 50 to 150
- Tamped density [g/L]
- 25 to 130
- Drying loss [%]
- less than 5
- Loss on ignition [%]
- 0.1 to 15
- C content [%]
- 0.1 to 15
- pH value
- 3 to 9.