A transductor choke for a high frequency application comprising a magnetic core made from a nanocrystalline alloy, wherein the nanocrystalline alloy consists essentially of FeaCobCucM′dSixByM″z, wherein M′ signifies an element from the group V, Nb, Ta, Ti, Mo, W, Zr, Hf, or a combination thereof, and wherein M″ signifies an element from group C, P, Ge, As, Sb, In, O, N or a combination thereof, wherein the following conditions shall apply:
- a+b+c+d+x+y+z=100%, with a=100%−b−c−d−x−y−z;
- 0≦b≦15;
- 0.5≦c≦2;
- 0.1≦d≦6;
- 2≦x≦20;
- 2≦y≦18;
- 0≦z≦10 and
- x+y>18;
- and wherein the magnetic core has a hysteresis loop which is as rectangular as possible, a saturation magnetostriction |λs|<3 ppm, and an effective roughness Ra (eff) ranging from 3 to 9%.