# US 7,422,675 B2 · Process for changing anodes in an electrolytic aluminum production cell including adjustment of the position of the anode and device for implementing the process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,422,675 B2
- Document ID: US7422675B2
- Status: Granted
- Kind: B2
- Application number: 11/212,118
- Filed: 2005-08-26
- Published: 2006-03-09
- Granted: 2008-09-09
- Earliest claimed: 2004-09-08
- Assignees: E.C.L.
- Inventors: Alain Van Acker; Patrick Marchand
- Web page: https://patentgrep.com/patent/US7422675B2

## CPC

- C25C 3/06: of aluminium
- C25C 7/06: Operating or servicing
- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- Y10T 29/53039: with control means energized in response to activator stimulated by condition sensor
- Y10T 29/53087: with signal, scale, illuminator, or optical viewer
- Y10T 29/53091: for work-holder for assembly or disassembly
- Y10T 29/5313: Means to assemble electrical device
- Y10T 29/53204: Electrode
- Y10T 29/53217: Means to simultaneously assemble multiple, independent conductors to terminal
- Y10T 29/53252: Means to simultaneously fasten three or more parts
- Y10T 29/53261: Means to align and advance work part
- Y10T 29/53274: Means to disassemble electrical device
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A process for changing an anode of a cell for the production of aluminum by fused bath electrolysis including a plurality of anodes. According to the invention, an anode handling tool is used including a positioning device, a gripping device and a sensor detecting the vertical position of the gripping device, and the position sensor is used to measure the vertical distances traveled by the gripping device with respect to a reference level N. At least one sound or electromagnetic waves beam is then produced in a determined reference line or plane and the passage of the anode in the beam is used to measure the distances. The vertical position of the replacement anode in the cell is determined starting from the values obtained for the traveled distances and the replacement anode is put into this position in the place initially occupied by the spent anode.

## Claims

### Claim 1

Process for changing an anode of a cell for the production of aluminum by fused bath electrolysis, the cell comprising a plurality of anodes, at least one cathode block, and containing an electrolytic bath, each of said anodes comprising at least one anode block and a metal rod and being fixed removably by mechanical attachment means to a mobile metal frame, each said anode block having a reference surface, comprising the steps of:
establishing a reference line or plane using a beam of sound waves or electromagnetic waves;
selecting a spent anode for replacement by a replacement anode;
using at least one anode handling tool comprising a positioning device, a position sensor and a gripping device to grip the metal rod of the spent anode, and measuring with the position sensor a vertical distance A traveled by the gripping device in reaching a position in which the metal rod is gripped;
withdrawing the spent anode from the electrolytic cell, passing the anode block of the spent anode vertically through the beam and measuring with the position sensor a vertical distance B traveled by the gripping device at a moment when a reference surface of the spent anode passes through the beam;
gripping the metal rod of a replacement anode using a gripping device, passing the anode block of the replacement anode vertically through the beam and measuring with the position sensor a vertical distance C traveled by the gripping device at a moment when a reference surface of the replacement anode corresponding to the reference surface of the spent anode passes through the beam; and
determining a desired vertical position of the replacement anode corresponding to the vertical position of the spent anode in the cell, from values obtained for the traveled distances A, B and C, and placing the replacement anode in the desired vertical position.

### Claim 2 (depends on 1)

Process according to claim 1, wherein a single gripping device is used to handle both the spent anode and the replacement anode.

### Claim 3 (depends on 1)

Process according to claim 1, wherein the anode reference surface is a lower surface of the anode block that will be immersed in the electrolytic bath contained in the electrolytic cell and that will be parallel to an upper surface of the cathode block.

### Claim 4 (depends on 1)

Process according to claim 1, wherein the vertical distance B is measured during a downwards movement of the spent anode.

### Claim 5 (depends on 1)

Process according to claim 1, wherein the vertical distance C is measured during an upwards movement of the replacement anode.

### Claim 6 (depends on 1)

Process according to claim 1, wherein the vertical position of the replacement anode corresponds to a vertical distance A′ traveled by the gripping device during said placing of the replacement anode.

### Claim 7 (depends on 6)

Process according to claim 6, wherein the vertical distance A′=A−B+C+D, where D is a correction term to take account of the replacement anode reaching its normal operating rate in the cell.

### Claim 8 (depends on 1)

Process according to claim 1, wherein the position sensor is integrated into the anode handling tool.

### Claim 9 (depends on 1)

Process according to claim 1, wherein the anode handling tool is provided with a means for measuring the tension in the tool.

### Claim 10 (depends on 9)

Process according to claim 9, wherein the means for measuring tension comprises an axial dynamometer.

### Claim 11 (depends on 1)

Process according to claim 1, wherein the electromagnetic waves are selected from the group consisting of visible light, infrared radiation and radio waves.

### Claim 12 (depends on 1)

Process according to claim 1, wherein the beam is generated using a laser.

### Claim 13 (depends on 1)

Process according to claim 1, wherein the sound waves are ultrasound waves.

### Claim 14 (depends on 1)

Process according to claim 1, wherein at least two beams of sound or electromagnetic waves are generated so as to form a reference plane.

### Claim 15 (depends on 14)

Process according to claim 14, wherein each of said beams is generated by a distinct wave source.

### Claim 16 (depends on 1)

Process according to claim 1, additionally comprising placing a sound or electromagnetic wave detector facing a sound or electromagnetic wave beam generator, such that the detector detects the beam produced by the generator and detects the moment when the reference surface of an anode passes through and interrupts the beam.

### Claim 17 (depends on 1)

Process according to claim 1, additionally comprising placing a sound or electromagnetic wave detector and a sound or electromagnetic waves beam generator facing a reflecting surface, such that the detector detects the beam produced by the generator and reflected by the reflecting surface and detects the moment when the reference surface of an anode passes through the beam and interrupts the beam.

### Claim 18 (depends on 1)

Process according to claim 1, additionally comprising placing a sound or electromagnetic wave detector and a sound or electromagnetic wave beam generator such that the detector can detect the beam produced by the generator and reflected by an anode block and detects the, moment when the reference surface of an anode passes through the beam, the anode block reflecting all or part of the beam towards the detector.

### Claim 19 (depends on 1)

Process according to claim 1, wherein the reference line or plane is substantially horizontal.

### Claim 20 (depends on 1)

Process according to claim 1, wherein the spent anodes are replaced sequentially by replacement anodes.

### Claim 21 (depends on 1)

Process according to claim 1, wherein at least two spent anodes are replaced at the same time by replacement anodes.