Quantum-splitting fluoride-based phosphors, method of producing, and radiation sources incorporating same
AssigneeGeneral Electric Company
InventorsVenkatesan Manivannan, Alok Mani Srivastava, Holly Ann Comanzo
Life of this patent
Estimating the term…
Abstract
A quantum-splitting fluoride-based phosphor comprises gadolinium, at least a first alkali metal, and a rare-earth metal activator. The phosphor is made in a solid-state method without using HF gas. The phosphor can be used alone or in conjunction with other phosphors in light sources and displays wherein it can be excited by VUV radiation, and increases the efficiency of these devices.
Claims17
A phosphor comprising a material having a formula of AGdF4:RE, wherein A is a first alkali metal and is selected from the group consisting of K, Rb, Cs, and combinations thereof;
- RE is at least a rare-earth metal activator other than gadolinium;
- and an additional metal selected from the group consisting of V, Nb, W, Zr, Hf, and combinations thereof.
A phosphor blend comprising:
- (a) a first phosphor having a formula of AGdF4:RE, wherein A is a first alkali metal and is selected from the group consisting of K, Rb, Cs, and combinations thereof;
- and RE is at least a rare-earth metal activator other than gadolinium;
- and an additional metal selected from the group consisting of V, Nb, W, Zr, Hf, and combinations thereof;
- (b) at least a second phosphor selected from the group consisting of LaPO4:Ce3+,Tb3+;
- GdMgB5O10:Ce3+,Tb3+;
- CeMgAl11O19:Ce3+,Tb3+;
- Ca5(PO4)3(Cl,F,OH):Sb3+,Mn2+, Eu2+;
- Sr4Al14O25:Eu2+;
- (Ba,Sr,Ca)5(PO4)3(Cl,F,OH):Eu2+;
- (Ba,Sr,Ca)MgAl10O17:Eu2+;
- (Ba,Sr,Ca)BPO5:Eu2+;
- BaAl8O13:Eu2+2SrO0.84P2O50.16B2O3:Eu2+;
- MgWO4;
- BaTiP2O8;
- (Ba,Sr,Ca)MgAl10O17:Eu2+,Mn2+;
- (Ba,Sr,Ca)5(PO4)3(Cl,F,OH):Sb3+;
- (Y,Gd,La,Lu,Sc)2O3:Eu3+;
- (Y,Gd,La,In,Lu,Sc)BO3:Eu3+;
- (Y,Gd,La)(Al,Ga)O3:Eu3+;
- (Ba,Sr,Ca)(Y,Gd,La,Lu)2O4:(Y,Gd)Al3B4O12:Eu3+;
- monoclinic Gd2O3:Eu3+;
- (Gd,Y)4(Al,Ga)2O9:Eu3+;
- (Ca,Sr)(Gd,Y)3(Ge,Si)AlO9:Eu3+;
- (Sr,Mg)3(PO4)2:Sn2+;
- GdMgB5O10:Ce3+,Mn2+;
- and 3.5MgO0.5MgF2. GeO2:Mn4+.
A phosphor blend comprising;
- (a) a first phosphor having a formula of (A1-yDy)(Gd1-xREx)F4;
- wherein A is a first alkali metal selected from the group consisting of K, Rb, Cs, and combinations thereof;
- D is a second alkali metal selected from the group consisting of Li, Na, K, Rb, Cs, and combinations thereof;
- RE is a rare-earth metal activator, and an additional metal selected from the group consisting of V, Nb, W, Zr, Hf, and combinations thereof;
- and x and y are independently in a range from about 0.0001 to about 0.1;
- (b) at least a second phosphor selected from the group consisting of LaPO4:Ce3+,Tb3+;
- GdMgB5O10:Ce3+,Tb3+;
- CeMgAl11O19:Ce3+,Tb3+;
- Ca5(PO4)3(Cl,F,OH):Sb3+,Mn2+,Eu2+;
- Sr4Al14O25:Eu2+;
- (Ba,Sr,Ca)5(PO4)3(Cl,F,OH):Eu2+;
- (Ba,Sr,Ca)MgAl10O17:Eu2+;
- (Ba,Sr,Ca)BPO5:Eu2+;
- BaAl8O13:Eu2+;2SrO0.84P2O5.0.16B2O3:Eu2+;
- MgWO4;
- BaTiP2O8;
- (Ba,Sr,Ca)MgAl10O17:Eu2+,Mn2+;
- (Ba,Sr,Ca)5(PO4)3(Cl,F,OH):Sb3;
- (Y,Gd,La,Lu,Sc)2O3:Eu3+;
- (Y,Gd,La,Lu,Sc)BO3:Eu 3+;
- (Y,Gd,La)(Al,Ga)O3:Eu3+;
- (Ba,Sr,Ca)(Y,Gd,La,Lu)2O4:Eu3+;
- (Y,Gd)al3B4O12:Eu3+;
- monoclinic Gd2O3:Eu3+;
- (Gd,Y)4(Al,Ga)2O9:Eu3+;
- (Ca,Sr)(Gd,Y)3Ge,Si)AlO9:Eu3+;
- (Sr,Mg)3(PO4) 2:Sn2+;
- 9:Eu3+(Sr,Mg)3(PO4)2GdMgB5O10:CE3+,Mn2+;
- and 3.5MgO0.5MgF2. GeO2:Mn4+.
A light source comprising:
- (a) a source of UV radiation that is located in a sealed housing, said UV radiation including a portion in a VUV range;
- and
- (b) a phosphor material disposed within the sealed housing and adapted to be excited by the UV radiation and to emit visible light, wherein the phosphor material comprises a first phosphor having a formula of AGdF4:RE, wherein A is a first alkali metal and is selected from the group consisting of K, Rb, Cs, and combinations thereof;
- and RE is at least a rare-earth metal activator other than gadolinium;
- and an additional metal selected from the group consisting of V, Nb, W, Zr, Hf, and combinations thereof.
A display comprising:
- (a) a source of electrons;
- and
- (b) a phosphor material disposed within the sealed housing and adapted to be excited by the electrons and to emit visible light, wherein the phosphor material comprises a first phosphor having a formula of AGdF4:RE, wherein A is a first alkali metal and is selected from the group consisting of K, Rb, Cs, and combinations thereof;
- and RE is at least a rare-earth metal activator other than gadolinium;
- and an additional metal selected from the group consisting of V, Nb, W, Zr, Hf, and combinations thereof.