Methods for preparing slurries of coated particulates
AssigneeHalliburton Energy Services, Inc.
InventorsBilly Slabaugh, Jimmie D. Weaver, Philip D. Nguyen
Life of this patent
Estimating the term…
Loading patent…
AssigneeHalliburton Energy Services, Inc.
InventorsBilly Slabaugh, Jimmie D. Weaver, Philip D. Nguyen
Estimating the term…
Methods are provided that include a method of creating a stable slurry of coated particulates wherein the slurry is capable of being stored for at least 2 hours before use comprising the steps of: providing resin coated particulates wherein the resin comprises a resin that does not completely cure unless it is at least one of exposed to a temperature above about 175° F. or exposed to an external catalyst; and, substantially suspending the resin coated particulates in a servicing fluid to create a stable resin coated particulate slurry. Methods are provided that include a method of creating a stable slurry of coated particulates wherein the slurry is capable of being stored for at least 2 hours before use comprising the steps of: providing tackifier coated particulates; and, substantially suspending the tackifier coated particulates in a servicing fluid to create a tackifier coated particulate slurry.
A method of propping a fracture in a subterranean formation comprising the steps of:
A method of propping a fracture in a subterranean formation comprising the steps of:
Dependencies are inferred from the claim text.