# US 7,220,536 B2 · Silver salt photothermographic dry imaging material, thermal development method of the same, and thermal development apparatus for the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,220,536 B2
- Document ID: US7220536B2
- Status: Granted
- Kind: B2
- Application number: 11/251,701
- Filed: 2005-10-17
- Published: 2006-04-27
- Granted: 2007-05-22
- Earliest claimed: 2004-10-22
- Assignees: Konica Minolta Medical & Graphic, Inc.
- Inventors: Koji Kuwano; Takayuki Sasaki; Kazuhiro Kido
- Web page: https://patentgrep.com/patent/US7220536B2

## CPC

- G03C 1/49818: {Silver halides}
- G03C 1/498: Photothermographic systems, e.g. dry silver
- G03C 1/49881: {characterised by the process or the apparatus}
- G03C 1/04: with macromolecular additives; with layer-forming substances
- G03C 1/061: {Hydrazine compounds}
- G03C 1/08: Sensitivity-increasing substances
- G03C 1/485: Direct positive emulsions
- G03C 1/49845: {Active additives, e.g. toners, stabilisers, sensitisers}
- G03C 1/49863: {Inert additives, e.g. surfactants, binders}
- G03C 2001/03564: {Mixed grains or mixture of emulsions}
- G03C 2001/03594: {Size of the grains}
- G03C 2200/09: Apparatus
- G03C 2200/43: Process
- G03C 2200/52: Rapid processing
- G03C 2200/58: Sensitometric characteristics
- G03C 2200/60: Temperature
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A photothermographic imaging material comprising a support having thereon, (a) a photosensitive layer containing an organic silver salt, photosensitive silver halide grains, a reducing agent and a binder, (b) a light-insensitive layer, and (c) a protective layer, wherein a weight reducing value from 25° C. to 100° C. by a heat drying weight measurement of the photographic imaging material is not more than 0.4% based on a weight value at 25° C.

## Claims

### Claim 1

A photothermographic imaging material comprising a support having thereon:
(a) a photosensitive layer containing an organic silver salt, photosensitive silver halide grains, a reducing agent and a binder,
(b) a light-insensitive layer, and
(c) a protective layer,
wherein a weight reducing value from 25° C. to 100° C. by a heat drying weight measurement of the photographic imaging material is not more than 0.4% based on a weight value at 25° C.

### Claim 2 (depends on 1)

The photothermographic imaging material of claim 1, wherein the weight reducing value from 100° C. to 120° C. by
the heat drying weight measurement of the photographic imaging material is not more than 0.04% based on the weight value at 25° C.

### Claim 3 (depends on 1)

The photothermographic imaging material of claim 1,
wherein the light-insensitive layer comprises a cross-linking agent.

### Claim 4 (depends on 1)

The photothermographic imaging material of claim 1,
wherein the protective layer comprises tabular grains.

### Claim 5 (depends on 1)

The photothermographic imaging material of claim 1,
wherein the photosensitive silver halide grains are silver halide grains convertible from internal latent-image type grains to surface latent-image type grains after the thermal development process.

### Claim 6 (depends on 1)

The photothermographic imaging material of claim 1, exhibiting a total dry thickness of the photosensitive layer and the light-insensitive layer of not less than 10 μm and not more than 20 μm.

### Claim 7 (depends on 1)

The photothermographic imaging material of claim 1 exhibiting the total dry thickness of the photosensitive layer of not less than 9 μm and not more than 16 μm.

### Claim 8 (depends on 1)

The photothermographic imaging material of claim 1,
wherein as silver halide grains, the photosensitive layer contains thermally convertible interior latent-image type silver halide grains surface sensitivity of which is reduced from that of before thermal development by conversion from the surface latent-image type to the interior latent-image type after the thermal development process.

### Claim 9 (depends on 1)

The photothermographic imaging material of claim 1, exhibits a relative ratio (S2/S1) of not more than 1/10,
wherein sensitivity S1 is determined from characteristic curves which are obtained by thermal development with common thermal development conditions after exposure of the photothermographic material, exposure being conducted by white light or light of a specific spectral sensitized region through an optical wedge, or by laser light changing illumination intensity on the surface of the photosensitive layer in incremental steps; and
sensitivity S2 is determined from characteristic curves which are obtained by thermal development under the same conditions as above thermal development after exposure under the same exposure conditions as above exposure, except that exposure is conducted after heating of the photothermographic material under the same conditions as above thermal development.

### Claim 10 (depends on 1)

The photothermographic imaging material of claim 1,
wherein in the interior of the silver halide grains, contained are dopants which function as electron traps after thermal development.

### Claim 11 (depends on 1)

The photothermographic imaging material of claim 1,
wherein a compound represented by Formula (SE1) or Formula (SE2) is incorporated as a silver saving agent:
Q1-NHNH-Q2 Formula (SE1)
wherein Q1 is an aromatic group bonding with —NHNH-Q2 at a carbon atom site or a heterocycle group; Q2 is a carbamoyl group, an acyl group, an alkoxycarbonyl group, an aryloxycarbonyl group, a sulfonyl group or a sulfamoyl group;
Formula (SE2)
wherein R1 is an alkyl group, an acyl group, an acylamino group, a sufonamide group, an alkoxycarbonyl group, or a carbamoyl group; R2 is a hydrogen atom, a halogen atom, an alkyl group, an alkoxy group, an aryloxy group, an alkylthio group, an arylthio group, an acyloxy group, or ester carbonate; and R3 and R4 are each a substituent group capable of substituting to a benzene ring and may form a condensed ring combining each other.

### Claim 12 (depends on 1)

The photothermographic imaging material of claim 1,
wherein the photosensitive layer contains a binder exhibiting a glass-transition temperature (Tg) of 70 to 150° C.

### Claim 13 (depends on 1)

The photothermographic imaging material of claim 1,
wherein a compound represented by Formula (SF) is incorporated:
(Rf-(L1)n1-)p-(Y)m1-(A)q Formula (SF)
wherein Rf is a substituent group containing a fluorine atom, L1 is a divalent linking group not containing a fluorine atom, Y is a (p+Q) valent linking group containing no fluorine atom, A is an anion group or its salt, n1 and m1 are each an integer of 0 or 1, p and q are each an integer of 1 to 3, but when q is 1, n1 and m1 are not zero at the same time.

### Claim 14 (depends on 1)

The photothermographic imaging material of claim 1,
wherein an average grain diameter of the silver halide grains contained in the photosensitive layer is 10 to 50 nm.

### Claim 15 (depends on 14)

The photothermographic imaging material of claim 14,
wherein the photosensitive layer further contains silver halide grains exhibiting an average grain diameter of 55 to 100 nm.

### Claim 16 (depends on 1)

The photothermographic imaging material of claim 1,
wherein a portion of the silver halide grains contained in the photosensitive layer is provided with chemical sensitization employing a chalcogen compound.

### Claim 17 (depends on 1)

A method of development of the photothermographic imaging material of claim 1 comprising the steps of:
(a) exposing the photothermographic imaging material, and
(b) developing the exposed photothermographic material using a thermal development apparatus having a distance from an exposure section to a development section of 0 to 20 cm.

### Claim 18 (depends on 1)

A method of thermal development of a photothermographic imaging material of claim 1, further exhibiting a weight reducing value from 25° C. to 100° C. by a heat drying weight measurement of not more than 0.4% based on a weight value at 25° C., comprising the steps of:
(a) exposing the photothermographic material,
(b) heating the exposed photothermographic material within a heating time of 0.5 to 10 seconds, and
(c) cooling the heated material,
wherein a side of the photothermographic material coated with the photosensitive layer is open to the air, and heating is conducted from the opposite side of the photosensitive layer.

### Claim 19 (depends on 1)

The method of thermal development of the photothermographic imaging material of claim 1, further exhibiting a weight reducing value from 100 to 120° C. by the heat drying weight measurement of not more than 0.04% based on a weight value at 25° C., comprising the steps of:
(a) exposing the photothermographic material,
(b) heating the exposed photothermographic material within a heating time of 0.5 to 10 seconds, and
(c) cooling the heated material,
wherein a side of the photothermographic material coated with the photosensitive layer is open to the air, and heating is conducted from the side opposite the photosensitive layer.

### Claim 20 (depends on 19)

The method of thermal development of the photothermographic imaging material of claim 19,
wherein the heated photothermographic material is transferred to a cooling process while the photosensitive layer coated side of the photothermographic material is open to the air.

### Claim 21 (depends on 19)

The method of thermal development of the photothermographic imaging material of claim 19,
wherein the side opposite the photosensitive layer of the photothermographic material is cooled while the photosensitive layer coated side of the photothermographic material is open to the air.

### Claim 22 (depends on 19)

The method of thermal development of the photothermographic imaging material of claim 19,
wherein at least an entering portion of a thermal development apparatus, the photosensitive later coated side of the material is open to the air.

### Claim 23 (depends on 18)

A thermal development apparatus for the method of thermal development of claim 18 comprising a temperature raising section which heats the photothermographic material to a thermal development temperature and a temperature maintaining section to prevent heat loss of the material, wherein different heating methods are employed in each of the temperature raising section and the temperature maintaining section.

### Claim 24 (depends on 23)

The thermal development apparatus of claim 23,
wherein the temperature raising section heats the photothermographic material while in contact with a plate heater while pressed by opposed rollers, and the temperature maintaining section keeps the material warm in a slit formed by guides, at least one of which guides has a heater.

### Claim 25 (depends on 23)

The thermal development apparatus of claim 23,
wherein a slit distance in the temperature maintaining section is 0.5 to 3.0 mm.

### Claim 26 (depends on 23)

The thermal development apparatus of claim 23,
wherein a slit distance in the temperature maintaining section is 1 to 3 mm.

### Claim 27 (depends on 18)

The method of thermal development of the photothermographic imaging material of claim 18,
wherein the heated photothermographic material is transferred to a cooling process while the photosensitive layer coated side of the photothermographic material is open to the air.

### Claim 28 (depends on 18)

The method of thermal development of the photothermographic imaging material of claim 18,
wherein the side opposite the photosensitive layer of the photothermographic material is cooled while the photosensitive layer coated side of the photothermographic material is open to the air.

### Claim 29 (depends on 18)

The method of thermal development of the photothermographic imaging material of claim 18,
wherein at least an entering portion of a thermal development apparatus, the photosensitive later coated side of the material is open to the air.