Dynamic process for enhancing the wear resistance of ferrous articles
AssigneeThe United States of America as represented by the Secretary of the Army
InventorsPaul J. Conroy, Charles S. Leveritt, John D. Demaree, James Hirvonen
Life of this patent
Estimating the term…
Abstract
A dynamic process for increasing the wear life of ferrous articles subjected to a high-temperature environment created by combustion of a propellant or fuel comprises selecting the propellant or fuel so that its combustion products include relatively large amounts of nitrogen, which nitrogen forms a protective nitride layer on the surface of the ferrous article. Disclosed is a specific embodiment of the invention for prolonging the wear life of gun barrels.
Claims19
A method for enhancing the wear life of a steel surface of a bore or a barrel of a gun, the method comprising the steps of:
- providing a nitrogen content propellant, the propellant generating, upon combustion, a propellant gas which includes at least 20% by mole fraction of nitrogen, wherein the mole fraction ratio of CO to CO2 in the propellant gas is greater than 3.0, and the mole fraction ratio of nitrogen to CO in the propellant gas is at least 0.65;
- igniting the propellant in the gun to cause the propellant to combust and generate the propellant gas;
- and
- directing the propellant gas into the bore of the gun barrel and the nitrogen in the propellant gas reacts with the steel surface to form an iron nitride, wherein the atomic percentage of nitrogen in the iron nitride is greater than 0 but less than or equal to 20% of the iron nitride and the melting point of the iron nitride is greater than 1600° K.
A method for enhancing the wear life ferrous surfaces of a bore of a barrel of a gun having a layer of a metal disposed upon at least a portion of the ferrous surface where the metal is selected from the group consisting of:
- tantalum, tungsten, molybdenum, iridium, chromium, and combinations thereof, and where the metal layer includes a plurality of cracks which extend through the metal layer to expose portions of the underlying ferrous surface of the bore, the method comprising the steps of:
- providing a nitrogen content propellant, the propellant generating, upon combustion, a propellant gas which includes at least 20 mole percent of nitrogen, wherein the mole fraction ratio of CO to CO2 in the propellant gas is greater than 3.0, and the mole fraction ratio of nitrogen to CO in the propellant gas is at least 0.65;
- igniting the propellant in the gun to cause the propellant to combust and generate the propellant gas;
- and
- directing the propellant gas into the bore of the barrel and the nitrogen in the propellant gas reacts with the exposed ferrous surfaces to form an iron nitride, wherein the iron nitride is characterized in that the atomic percentage of nitrogen in the iron nitride is greater than 0 but less than or equal to 20% of the iron nitride.
A method for repairing and extending the wear life of ferrous surfaces of a bore of a barrel of a gun, the method comprising the steps of:
- providing a nitrogen content propellant, the propellant generating, upon combustion, a propellant gas which includes at least 20 mole percent of nitrogen;
- igniting the propellant in the gun to cause the propellant to combust and generate the propellant gas;
- and
- directing the propellant gas into the bore of the barrel and the nitrogen in the propellant gas reacts with the steel surface to form an iron nitride, wherein the atomic percentage of nitrogen in the iron nitride is greater than 0 but less than or equal to 20% of the iron nitride.
Dependencies are inferred from the claim text.