Battery recycling
AssigneeUmicore AG & Co. KG
InventorsDaniel Cheret, Sven Santen
Life of this patent
Estimating the term…
Abstract
Process for the recovery of Co or Ni, comprising the steps of: preparing a metallurgical charge comprising Fe, slag formers, and a useful load containing either one or both of Co and Ni; feeding the charge to a shaft furnace; and smelting the charge so as to form a Co or Ni-bearing alloy, an Fe-bearing slag and a gaseous phase, characterised in that the useful load comprises at least 30 wt. % electrochemical batteries or their scrap, and in that the redox potential in the furnace is chosen so as to slag at least 20 wt. % of the Fe, and at most 20 wt. % of the Co or 20 wt. % of the Ni present in the charge.
Claims11
Process for the recovery of Co and Ni, comprising the steps of:
- preparing a metallurgical charge comprising Fe, slag formers, and a useful load containing either one or both of Co and Ni;
- feeding the charge to a shaft furnace;
- and
- smelting the charge so as to form a Co or Ni-bearing alloy, an Fe-bearing slag and a gaseous phase,
- wherein the useful load comprises at least 30 wt. % electrochemical batteries or their scrap, and wherein the redox potential in the furnace is chosen so as to slag at least 20 wt. % of the Fe, and at most 20 wt. % of the Co or 20 wt. % of the Ni present in the charge.
Dependencies are inferred from the claim text.