Textured yarn with different shrinkage and excellent suede effect and method for preparing the same
AssigneeKolon Industries, Inc.
InventorsJeong-Gi Lee, Chang-Bae Lee, Yang-Soo Park
Life of this patent
Estimating the term…
Abstract
The present invention relates to a textured yarn (ATY) with different shrinkage and excellent suede effect, wherein at least one or two kinds of two-component composite yarn (effect) yarn having a monofilament fineness are twined around a thermoplastic multifilament yarn (core yarn), forming loops on the surface of the textured yarn.
Claims28
A textured yarn(ATY) with different shrinkage and excellent suede effect, wherein at least one or two kinds of two-component composite yarn(effect yarn) having a monofilament fineness of 0.001 to 0.3 denier after dividing or extracting an extraction component are twined around a thermoplastic multifilament yarn(core yarn), 2 to 350 loops per meter of the two-component composite yarn of at least 1.0 mm in length are formed on the surface of the textured yarn, and more than 95% of the two-component composite yarn loops of at least 1.0 mm in length has a length of 1.0 to 2.5 mm.
A method for preparing a textured yarn(ATY) with different shrinkage and excellent suede effect by air-texturing an effect yarn and core yarn, wherein at least one or two kinds of two-component composite yarn(A) is fed as the effect yarn into an air texturing nozzle(3) at an over feed rate of 10 to 60% through the first feed roller(1), the two-component composite yarn(A) consisting of a fiber forming component and an extraction component or consisting of at least two kinds of fiber forming components and having a monofilament fineness of 0.001 to 0.3 denier after dividing or extracting the extraction component, at the same time, a thermoplastic multifilament yarn(B) is fed as the core yarn into the air texturing nozzle(3) at an overfed rate of 5 to 55% through the second feed roller(2) while supplying water to a water supply device(4) disposed between the second feed roller(2) and the air texturing nozzle(3), and then the effect and core yarns are air-textured by an air pressure of 6 to 16 kgf/cm2 in the air texturing nozzle(3), heat-treated at a temperature of 130 to 210° C. in a hollow heater(6) in a state that the overfeed rate is 0 to −8% and wound in a state that the overfeed rate is −2 to −12%.