Method of making a lariat
OwnerJoe Sayatovichinventor
Life of this patent
Estimating the term…
Abstract
A method of making a lariat includes twisting under tension a plurality of strands of a plastic material such as nylon to form a rope and then securing the ends of the rope to prevent the strands from untwisting. The rope is then dipped into a hot wax mixture, removed from the hot wax and dried and cooled. A powdery material such as talcum powder is then applied to a portion of the rope adjacent one end after loosely tying a hondo knot therein or prior to tying a hondo knot the powdery material is applied and a hondo knot is then tied and the hondo knot is snugged by stretching the rope.
Claims10
In a method of making a lariat comprising the steps of twisting together under tension a plurality of strands of plastic material to form a rope, securing the ends of the rope to prevent the strands from untwisting, dipping the rope into hot wax, removing the rope from the hot wax and letting the rope cool, and forming a hondo at one end of the rape, the improvement comprising
- loosely tying a hondo knot at one end the rope,
- applying a powdery material to said one end of the rope having the hondo knot therein in an amount sufficient to coat the hondo knot to lower the coefficient of friction on the surface thereof and
- snugging the hondo knot by stretching the rope until knot security is obtained. with the powdery material reducing the amount of stretching required to obtain knot security.
In a method of making a lariat comprising the steps of twisting together under tension a plurality of strands of plastic material to form a rope, securing the ends of the rope to prevent the strands from untwisting. dipping the rope into hot wax, removing the rope from the hot wax and letting the rope cool, and forming a hondo at one end of the rope, the improvement comprising
- applying a powdery material to a portion of the rope adjacent said one end, in an amount sufficient to coat said one end whereby the coefficient of friction on the surface thereof is lowered, prior to forming a hondo knot,
- loosely tying a hondo knot In said one end of the rope and
- snugging the hondo knot by stretching the rope until knot security is obtained. with the powdery material reducing the amount of stretching required to obtain knot security.
Dependencies are inferred from the claim text.