Compositionally graded sintered alloy and method of producing the same
AssigneeToshiba Tungaloy Co., Ltd.
InventorMasaki Kobayashi
Life of this patent
Estimating the term…
Loading patent…
AssigneeToshiba Tungaloy Co., Ltd.
InventorMasaki Kobayashi
Estimating the term…
There is disclosed a compositionally graded sintered alloy which comprises: 1 to 40% by weight of a iron group metal; 0.1 to 10% by weight of at least one type of a specific metal element selected from the group consisting of Cr, Au, Ge, Cu; Sn, Al, Ga, Ag, In, Mn and Pb; a hard phase containing, as a main component, at least one compound selected from the group consisting of a carbide, a nitride and a mutual solid solution of a metal(s) which belongs to Group 4 (Ti, Zr, Hf), 5 (V, Nb, Ta) or 6 (Cr, Mo, W) of the Periodic Table; and inevitable impurities, wherein the content of the specific metal element gradually increases from a surface of the sintered alloy toward an inner portion thereof, and a ratio of the average concentration of the specific metal element in a region which is at least 1 mm inside from the surface of the sintered alloy, to the average concentration of the specific metal element in a region between the surface and the position which is 0.1 mm inside the surface, of the sintered alloy, is 1.3 or more.
A compositionally graded sintered alloy which comprises:
Dependencies are inferred from the claim text.