US 7,063,728 B2Granted
Process for making chrome tanned leathers
AssigneeCouncil of Scientific and Industrial Research
InventorsVictor John Sundar, Chellapp Muralidharan
Life of this patent
Estimating the term…
Abstract
The present invention provides an improved pickling and bating free process suitable for both hides and skins for making chrome tanned leathers by using a mixture of conventional chrome tanning salt and alkali metal salt is used at a pH in the range of 5–5.5.
Claims5
A tanning process for making chrome tanned leathers, said process comprising the steps of:
- a) conditioning delimed hides or skins to a pH in the range of 5–5.5,
- b) treating the delimed hides or skins with 6–8% w/w, of a mixture of basic chromium sulfate of basicity ranging 30–45% and alkali metal salt of organic acid up to three carbon chain, for a period of at least 2 Hrs, without addition of water,
- c) adjusting pH of the contents of step (b) in the range of 4–4.2 by alkalinizing agent, and
- d) washing the tanned leather with water to obtain chrome tanned leather;
- wherein the process does not include pickling or bating the delimed hides or skins.
2 more elements
Dependencies are inferred from the claim text.