Back to results
US 7,053,022 B2Granted
Hydrothermally synthesized MO-V-M-NB-X oxide catalysts for the selective oxidation of hydrocarbons
AssigneeRohm and Haas Company
InventorsAnne Mae Gaffney, Ruozhi Song
Life of this patent
Estimating the term…
Abstract
Hydrothermally synthesized catalysts comprising a mixed metal oxide are utilized to produce unsaturated carboxylic acids by the vapor phase oxidation of an alkane, or a mixture of an alkane and an alkene, in the presence thereof; or to produce unsaturated nitriles by the vapor phase oxidation of an alkane, or a mixture of an alkane and an alkene, and ammonia in the presence thereof.
Claims3
A process for producing a catalyst comprising a mixed metal oxide having the empirical formula
- MoaVbMcNbdXeOf
- wherein
- M is an element selected from the group consisting of Te and Sb;
- X is an element selected from the group consisting of Li, Na, K, Rb, Cs, Mg, Ca, Sr, Ba, Sc, Y, La, Ti, Zr, Hf, Ta, Cr, W, Mn, Re, Fe, Ru, Co, Rh, Ir, Ni, Pd, Pt, Cu, Ag, Au, Zn, B, Ga, In, Pb, P, As, Sb, Bi, Se, F, Cl, Br, I, Pr, Nd, Sm and Tb, with the proviso that, when M is Sb, X cannot be Sb;
- a, b, c, d, e and f are the relative atomic amounts of the elements Mo, V, M, Nb, X and O, respectively;
- and
- when a=1, b=0.01 to 1.0, c=0.01 to 1.0, d=0.01 to 1.0, 0<e≦1.0 and f is dependent on the oxidation state of the other elements;
- the process comprising:
- (i) admixing compounds of elements Mo, V, M, Nb and X, as needed, and a solvent comprising water to form a first admixture containing at least 2 but less than all of said elements Mo, V, M, Nb and X;
- (ii) heating said first admixture at a temperature of from 25° C. to 200° C. for from 5 minutes to 48 hours;
- (iii) then, admixing compounds of elements Mo, V, M, Nb and X, as needed, with said first admixture to form a second admixture containing elements Mo, V, M, Nb and X, in the respective relative atomic proportions a, b, c, d, and e wherein, when a=1, b=0.01 to 1.0, c=0.01 to 1.0, d=0.01 to 1.0 and 0<e≦1.0;
- (iv) heating said second admixture at a temperature of from 50° C. to 300° C. for from 1 hour to 7 days, in a closed vessel under pressure;
- (v) recovering insoluble material from said closed vessel to obtain a catalyst.
10 more elements
A process for producing a catalyst comprising a mixed metal oxide having the empirical formula
- MoaVbMcNbdXeOf
- wherein
- M is an element selected from the group consisting of Te and Sb;
- X is an element selected from the group consisting of Li, Na, K, Rb, Cs, Mg, Ca, Sr, Ba, Sc, Y, La, Ti, Zr, Hf, Ta, Cr, W, Mn, Re, Fe, Ru, Co, Rh, Ir, Ni, Pd, Pt, Cu, Ag, Au, Zn, B, Ga, In, Pb, P, As, Sb, Bi, Se, F, Cl, Br, I, Pr, Nd, Sm and Tb, with the proviso that, when M is Sb, X cannot be Sb;
- a, b, c, d, e and f are the relative atomic amounts of the elements Mo, V, M, Nb, X and O, respectively;
- and
- when a=1, b=0.01 to 1.0, c=0.01 to 1.0, d=0.01 to 1.0, 0<e≦1.0 and f is dependent on the oxidation state of the other elements;
- said mixed metal oxide having an x-ray diffraction pattern with peaks at the following diffraction angles (2θ):
- 22.1±0.3, 26.2±0.3, 27.3±0.3, 29.9±0.3, 45.2±0.3, 48.6±0.3, and no peaks at the diffraction angles (2θ):
- 28.2±0.3, 36.2±0.3, 36.2±0.3, 50.0±0.3 the process comprising:
- (i) admixing compounds of elements Mo, V, M, Nb and X, as needed, and a solvent comprising water to form a first admixture containing at least 2 but less than all of said elements Mo, V, M, Nb and X;
- (ii) heating said first admixture at a temperature of from 250° C. to 200° C. for from 5 minutes to 48 hours;
- (iii) then, admixing compounds of elements Mo, V, M, Nb and X, as needed, with said first admixture to form a second admixture containing elements Mo, V, M, Nb and X, in the respective relative atomic proportions a, b, c, d and e wherein, when a=1, b=0.01 to 1.0, c=0.01 to 1.0, d=0.01 to 1.0 and 0<e≦1.0;
- (iv) heating said second admixture at a temperature of from 50° C. to 300° C. for from 1 hour to 7 days, in a closed vessel under pressure;
- (v) recovering insoluble material from said closed vessel;
- (vi) calcining said recovered insoluble material;
- (vii) contacting said calcined recovered insoluble material with a liquid contact member selected from the group consisting of organic acids, alcohols, inorganic acid and hydrogen peroxide to form a contact mixture;
- (viii) recovering insoluble material from said contact mixture to obtain a catalyst.
15 more elements
Dependencies are inferred from the claim text.