# US 7,034,260 B2 · Method of making a heating element of molybdenum silicide type

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,034,260 B2
- Document ID: US7034260B2
- Status: Granted
- Kind: B2
- Application number: 10/510,144
- Filed: 2003-04-04
- Published: 2005-08-25
- Granted: 2006-04-25
- Earliest claimed: 2002-04-05
- Assignees: Sandvik AB
- Inventors: Mats Sundberg; Anders Magnusson
- Web page: https://patentgrep.com/patent/US7034260B2

## CPC

- C04B 35/58092: {based on refractory metal silicides}
- H01C 17/0656: {composed of silicides (H01C17/0652 takes precedence)}
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/402: Aluminium
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/72: Products characterised by the absence or the low content of specific components, e.g. alkali metal free alumina ceramics
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01C: RESISTORS

## Abstract

A method of producing a heating element made from molybdenum silicide and alloys thereof, and which includes aluminum oxide on its surface. A material is produced that contains substantially Mo(Si1-xAlx)2 and Al2O3 by mixing a mixture of a silicon and molybdenum compound with an aluminum compound. Either of the silicon and molybdenum compounds include Mo(Si1-yAly)2 and are mixed with one or both of an aluminum compound in the form of Al2O3 or Al(OH)3 and optionally the compounds SiO2, Si, and MoO3, or by virtue of the mixture of the silicon and molybdenum compound containing MoO3 and Al and Si and/or SiO2. The input components together have a degree of purity corresponding to at least 98%. The mixture reacts exothermically and/or by being sintered, so that exchange reactions take place to form the compounds Mo(Si1-xAlx)2 and Al2O3, where x lies in the range of 0.4–0.6.

## Claims

### Claim 1

A method of producing a heating element containing essentially molybdenum silicide and alloys thereof, which forms aluminum oxide on its surface, said method comprising the steps of: producing a material that contains substantially Mo(Si1-xAlx)2 and Al2O3 by mixing a mixture of a silicon and a molybdenum compound with an aluminum compound, wherein the silicon and molybdenum compound mixture is mixed with an aluminum compound including at least one of Al2O3 or Al(OH)3, wherein the mixture of a silicon and a molybdenum compound with an aluminum compound includes components that together have a degree of purity corresponding to at least 98%; and reacting the mixture components by at least one of exothermic reaction and sintering so that exchange reactions take place to form the compounds Mo(Si1-x Alx)2 and Al2O3, where x lies in the range of 0.4–0.6.

### Claim 2 (depends on 1)

A method according to claim 1, wherein SiO2 is included in the mixture is a silicate and does not affect symmetry of molybdenum suicide crystal lattice.

### Claim 3 (depends on 1)

A method according to claim 1, wherein x lies in the range of 0.45–0.55.

### Claim 4 (depends on 1)

A method according to claim 1, including the step of adding at least one of sintering auxiliaries MgO, CaO, SiO2 and Y2O3 to said mixture.

### Claim 5 (depends on 1)

A method according to claim 1, including the step of partially substituting for molybdenum at least one of Re or W or Nb in the material Mo(Si1-xAlx)2.

### Claim 6 (depends on 5)

A method according to claim 5, including the step of replacing molybdenum with W in an amount corresponding to approximately one third.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the mixture components together have a degree of purity of at least 99%.

### Claim 8 (depends on 1)

A method according to claim 1, including the step of adding to the mixture at least one of the compounds SiO2, Si, and MoO3.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the mixture of the silicon and the molybdenum compound contains MoO3 and Al, and at least one of Si and SiO2.

### Claim 10 (depends on 2)

A method according to claim 2, wherein the silicate is mullite.

### Claim 11 (depends on 2)

A method according to claim 2, wherein the silicate is sillimanite.

### Claim 12 (depends on 1)

A method according to claim 1, wherein the heating element includes a surface layer of aluminum oxide that is retained after cyclic operation of the heating element between room temperature and 1500° C.