Base metal recovery from a tailings dump by bacterial oxidation
AssigneeBilliton SA Limited
InventorsPeter Michael Craven, Trevor Hugh Tunley
Life of this patent
Estimating the term…
Abstract
A method of recovering base metal from a tailings dump which includes the steps of: aerating a surface layer of the dump; adjusting the pH and the moisture content of the surface layer to provide conditions favourable for bacterial oxidation of sulphide minerals; allowing bacterial oxidation to take place for a controlled period, after the controlled period removing the oxidized surface layer and adding water thereto for form a slurry; separating the slurry into solids and a solution; and recovering base metal from the solution.
Claims26
A method of recovering base metal from a tailings dump which contains bacteria which are capable of oxidizing sulphide minerals in the dump, the method including the steps of:
- (a) aerating a surface layer of the dump by agitating or mechanically loosening the surface layer;
- (b) providing conditions favourable for oxidation of sulphide minerals by the bacteria:
- (1) adjusting the pH of the surface layer to a level in the range of from 1.3 to 2.0, and
- (2) adjusting the moisture content of the surface layer to a value of from 16% to 20%;
- (c) allowing oxidation of the sulphide minerals by the bacteria to take place for a controlled period resulting in an oxidised surface layer;
- (d) removing the oxidised surface layer after the controlled period and adding water thereto to form a slurry wherein the slurry is directed to at least one tank in which agitation of the slurry takes place;
- (e) separating the slurry into solids and a solution;
- and
- (f) recovering base metal from the solution using solvent extraction or ion exchange techniques.
A method of recovering base metal from a tailings dump which contains bacteria which are capable of oxidizing sulphide minerals in the dump, the method including the steps of:
- (a) aerating a surface layer of the dump by agitating or mechanically loosening the surface layer;
- (b) providing conditions favourable for oxidation of sulphide minerals by the bacteria:
- (1) adjusting the pH of the surface layer to a level in the range of from 1.3 to 2.0, and
- (2) adjusting the moisture content of the surface layer to a value of from 16% to 20%;
- (c) allowing oxidation of the sulphide minerals by the bacteria to take place for a controlled period resulting in an oxidised surface layer;
- (d) removing the oxidised surface layer after the controlled period and adding water thereto to form a slurry;
- (e) separating the slurry into solids and a solution;
- and
- (f) recovering base metal from the solution using solvent extraction or ion exchange techniques wherein base metal in sulphate form in solution is separated from the slurry.
A method of recovering base metal from a tailings dump which contains bacteria which are capable of oxidizing sulphide minerals in the dump, the method including the steps of:
- (a) aerating a surface layer of the dump by agitating or mechanically loosening the surface layer;
- (b) providing conditions favourable for oxidation of sulphide minerals by the bacteria:
- (1) adjusting the pH of the surface layer to a level in the range of from 1.3 to 2.0, and
- (2) adjusting the moisture content of the surface layer to a value of from 16% to 20%;
- (c) allowing oxidation of the sulphide minerals by the bacteria to take place for a controlled period resulting in an oxidised surface, layer;
- (d) removing the oxidised surface layer after the controlled period and adding water thereto to form a slurry;
- (e) separating the slurry into solids and a solution;
- and
- (f) recovering base metal from the solution using solvent extraction or ion exchange techniques wherein said base metal is copper.
A copper recovery process wherein copper ore is ground and then subjected to a flotation process which results in tailings which are transferred to a tailings pile, and wherein the tailings pile contains bacteria which are capable of oxidising sulphide minerals in the tailings pile, the process including the steps of subjecting the tailings pile to the following:
- a) loosening and aerating of a surface layer of the pile;
- b) adjusting the pH of the surface layer to a value in the range of from 1.3 to 2.0;
- c) adjusting the moisture content of the pile to lie in a range of from 16% to 20%;
- d) allowing oxidation by the bacteria of at least sulphide minerals in the surface layer for a controlled period;
- e) removing the surface layer thereafter;
- f) mixing the surface layer with water to form a slurry which is conveyed to at least one agitation tank;
- g) separating the slurry in the tank into solids and a solution from which copper is extracted using solvent extraction or ion exchange techniques.
Dependencies are inferred from the claim text.