# US 7,003,965 B2 · Method for directly cooling fine-particle solid substances

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 7,003,965 B2
- Document ID: US7003965B2
- Status: Granted
- Kind: B2
- Application number: 10/482,909
- Filed: 2002-07-04
- Published: 2004-12-02
- Granted: 2006-02-28
- Earliest claimed: 2001-07-05
- Assignees: Kerr-McGee Pigments International GmbH
- Inventors: Gerhard Auer; Dirk Weber; Werner Schuy; Frank Wittekopf
- Web page: https://patentgrep.com/patent/US7003965B2

## CPC

- F28C 3/12: the heat-exchange medium being a particulate material and a gas, vapour, or liquid
- B02C 19/06: Jet mills
- B02C 23/20: after crushing or disintegrating
- C09C 1/24: Oxides of iron
- C09C 1/3018: {Grinding}
- C09C 1/3623: {Grinding}
- C09C 3/041: {Grinding}
- F25B 19/005: {the refrigerant being a liquefied gas}
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- F28C: HEAT-EXCHANGE APPARATUS, NOT PROVIDED FOR IN ANOTHER SUBCLASS, IN WHICH THE HEAT-EXCHANGE MEDIA COME INTO DIRECT CONTACT WITHOUT CHEMICAL INTERACTION (safety devices in general F16P; fluid heaters having heat generating means F24H; with an intermediate heat-transfer medium coming into direct contact with heat-exchange media F28D15/00 - F28D19/00; details of heat-exchange apparatus of general application F28F)
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- F25B: REFRIGERATION MACHINES, PLANTS OR SYSTEMS; COMBINED HEATING AND REFRIGERATION SYSTEMS; HEAT PUMP SYSTEMS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The invention relates to a method for directly cooling fine-particle, powdery solid substances by using a cooling medium provided in the form of low-boiling condensed gases or of cold gases obtained therefrom, whereupon bulk material packings are subsequently filled with these solid substances. The invention also relates to a device for directly cooling the fine-particle, powdery solid substances and to fine-particle, powdery solid substances, which are located inside bulk material packings and which, compared to air, have a lower oxygen content in the gas phase between the solid substance particles.

## Claims

### Claim 1

Method for directly cooling a fine-particle, powder-form solid substance of elevated temperature by means of introducing a cooling medium consisting of
a) one or more different condensed gases having a low boiling point, or
b) a cold gas or gas mixture, which was produced using one or more different condensed gases having a low boiling point, or
c) a cold gas or gas mixture that was pre-cooled using one or more different condensed gases having a low boiling point, into the solid substance having an average particle size of less than 50 μm of an inorganic or organic pigment or of cement or of a solid coated with a temperature-sensitive compound, and subsequently filling the cooled solid substance into bulk material packaging or mobile bulk material containers.

### Claim 2 (depends on 1)

Method according to claim 1, wherein the particle size is less than 20 μm.

### Claim 3 (depends on 2)

Method according to claim 2, wherein the fine-particle, powder-form solid substances has an average particle size of less than 5 ∞m.

### Claim 4 (depends on 1)

Method according to claim 1, wherein the fine-particle, powder-form solid substances is ground before the process step of direct cooling.

### Claim 5 (depends on 4)

Method according to claim 4, wherein the fine-particle, powder-form solid substance is a pigment directly cooled between a process step of steam jet grinding and the process step of filling into bulk material packaging or mobile bulk material containers, by the addition of the cooling medium.

### Claim 6 (depends on 5)

Method according to claim 5, wherein a mixture of ground pigment and gas phase that contains steam, is present immediately after the steam jet grinding, part of the gas phase that contains steam is first removed from the ground pigment, using a dust separator or a dust filter, and subsequently the ground pigments are cooled by means of direct cooling, using the cooling medium.

### Claim 7 (depends on 1)

Method according to claim 1, wherein the cooling medium used for direct cooling has a temperature of less than 0° C.

### Claim 8 (depends on 1)

Method according to claim 1, wherein the fine-particle, powder-form solid substances are transported pneumatically for filling into bulk material packaging or mobile bulk material containers, and that the gas used for the pneumatic transport is used as the cooling medium for direct cooling, the gas being cooled either indirectly in a heat exchanger, by means of condensed gases having a low boiling point, or directly, by injection of one or more different condensed gases having a low boiling point, before contact with the fine-particle, powder-form solid substances.

### Claim 9 (depends on 8)

Method according to claim 8, wherein the cooling medium is metered into the transport line in the pneumatic transport of the fine-particle, powder-form solid substances.

### Claim 10 (depends on 1)

Method according to claim 1, wherein gaseous nitrogen or gaseous carbon dioxide is used as the cooling medium.

### Claim 11 (depends on 1)

Method according to claim 1, wherein liquid nitrogen or liquid or solid carbon dioxide is used as the cooling medium.

### Claim 12 (depends on 1)

Method according to claim 1, wherein the fine-particle, powder-form solid substance is cooled within the short period of time that is required for mixing with the cooling medium, by at least 20° C.

### Claim 13 (depends on 1)

Method according to claim 1, wherein the fine-particle, powder-form solid substance is cooled to a maximum of 100° C.

### Claim 14 (depends on 8)

Method according to claim 8, wherein the cooling medium is introduced into the transport gas for the pneumatic transport of the fine-particle, powder-form solid substance before the transport gas makes contact with the solid substance.

### Claim 15 (depends on 1)

Method according to claim 1, wherein the cooling medium used for direct cooling contains less than 0.0001 parts by mass water, and that the dew point of the gas phase that contains solid substance is lowered in this manner.

### Claim 16 (depends on 1)

Method according to claim 1, wherein the fine-particle, powder-form solid substance is filled into bulk material packaging, after cooling has taken place, or filled into a silo vehicle.

### Claim 17 (depends on 1)

Method according to claim 1, wherein the solid substance has the cooling medium applied to it, and is filled into bulk material packaging, in such a manner that in the bulk material packaging, the gas phase between the pigment particles contains less than 20 wt.-% oxygen.

### Claim 18 (depends on 1)

Method according to claim 1, wherein the solid substance has the cooling medium applied to it, and is filled into bulk material packaging, in such a manner that in the bulk material packaging, the gas phase between the pigment particles contains a mass ratio of nitrogen to oxygen of more than 4.

### Claim 19 (depends on 1)

Device for implementing the method according to claim 1, wherein the direct cooling of the fine-particle, powder-form solid substance takes place after steam-jet grinding, comprising a supply container for a condensed gas having a low boiling point, an insulated connecting line between the supply container and the transport line for pneumatic transport of the solid substance, a nozzle for introduction of the condensed gas having a low boiling point into the transport line, and a control and regulation device, wherein
a steam jet mill and a separation device arranged after the steam jet mill and ahead of a packaging device, in the transport direction, which separates the solid and the steam, are assigned to the feed line.

### Claim 20 (depends on 1)

Method according to claim 1, wherein the pigment is selected from the group consisting of titanium dioxide, iron oxide, chromium oxide, a photo-resistant pigment, a colored pigment, a metal pigment, a magnetic pigment, and carbon black.

### Claim 21 (depends on 7)

Method according to claim 7, wherein the temperature is less than −40° C.

### Claim 22 (depends on 12)

Method according to claim 12, wherein the solid substance is cooled by at least 50° C.

### Claim 23 (depends on 13)

Method according to claim 13, wherein the solid substance is cooled to less than 60° C.